论文

高低温熔体混合对Au-20Sn共晶合金凝固组织的影响

  • 郭德燕 宋佳佳 蔡亮 毛勇
展开
  • 云南大学物理科学技术学院材料科学与工程系, 昆明 650091
郭德燕, 男, 1986年生, 硕士生

收稿日期: 2012-06-20

  修回日期: 2012-07-20

  网络出版日期: 2012-11-11

基金资助

国家自然科学基金项目50964014和51161024资助

EFFECTS OF MELT MIXING WITH HIGH AND LOW TEMPERATURE MELTS ON SOLIDIFACATION MICROSTRUCTURES OF Au-20Sn EUTECTIC ALLOY

  • GUO Deyan SONG Jiajia CAI Liang MAO Yong
Expand
  • Department of Materials Science and Engineering, School of Physical Science and Technology, Yunnan University, Kunming 650091

Received date: 2012-06-20

  Revised date: 2012-07-20

  Online published: 2012-11-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50964014 and 51161024)

摘要

研究了高低温熔体混合处理对Au-20Sn(质量分数, \)共晶合金凝固组织的影响, 分析了Au-20Sn合金凝固组织随熔体混合处理中高温熔体温度变化(低温熔体温度均为283 ℃)的演变规律. 结果表明, 高低温熔体混合处理能有效改善合金凝固组织结构, 采用适当的高温熔体(350 ℃)与低温熔体(283 ℃)进行熔体混合自然冷却凝固, 会抑制初生相ζ'-Au5Sn的析出, 得到细小全层片共晶组织. 但当高温熔体温度偏高(360 ℃)或偏低(340 ℃)时, Au-20Sn共晶合金凝固组织中均存在初生相ζ'-Au5Sn. 高低温熔体混合处理改善合金凝固组织的主要原因是降低了凝固过程中Au富集的偏析现象, 改变了ζ'-Au5Sn相的结晶析出行为. 在220 ℃热压缩变形过程中, 熔体混合得到的细小全层片组织具有良好的热压缩变形能力, 表现为具有较低的屈服应力和恒应力-应变平台.

本文引用格式

郭德燕 宋佳佳 蔡亮 毛勇 . 高低温熔体混合对Au-20Sn共晶合金凝固组织的影响[J]. 金属学报, 2012 , 48(11) : 1387 -1393 . DOI: 10.3724/SP.J.1037.2012.00365

Abstract

The effects of melt mixing with high-temperature and low-temperature melts on Au-20Sn (mass fraction, %) eutectic alloy solidification microstructures have been studied. The solidification microstructure evolutions of Au-20Sn eutectic alloy by the temperatures of high-temperature melt were investigated. Melt mixing with high-temperature and low-temperature melts can effectively improve the solidification microstructure of Au-20Sn alloy. Adopting an appropriate melt mixing condition, which is high-temperature melt with 350 ℃ and low-temperature melt with 283 ℃, the precipitation of primary phase ζ'-Au5Sn will be inhibited during solidification process, and the full lamellar eutectic microstructure was obtained. When the temperature of high-temperature melt is high (360 ℃) or low (340 ℃), the primary phase ζ'-Au$_{5}$Sn will also exist in the solidification microstructure. Melt mixing with high-temperature and low-temperature melts can effectively decrease the Au atom segregation and modify the precipitation behavior of primary phase ζ'-Au5Sn. The compressive behavior at 220 ℃ exhibits a low yielding stress and a low stress platform for the alloy with full lamellar eutectic microstructure prepared by melt mixing, which indicates that the hot--workability of Au-20Sn alloy can be improved by melt mixing.

参考文献

[1] Ohmi T, Tanaka Y, Kudoh M, Itoh Y. J Jpn Inst Met, 1992; 56: 1064

[2] Ohmi T, Matsuura K, Kudoh M, Itoh Y. J Jpn Inst Light Met, 1998; 48: 42

[3] Ohmi T, Iguchi M. Mater Sci Forum, 2010; 631: 367

[4] Jian Z Y, Yang G C, Zhou Y H. Trans Nonferrous Met Soc China, 1995; 5: 133

(坚增运, 杨根仓, 周尧和. 中国有色金属学报, 1995; 5: 133)

[5] He S X, Sun B D, Wang J, Zhou Y H. Trans Nonferrous Met Soc China, 2001; 11: 834

(何树先, 孙宝德, 王俊, 周尧和. 中国有色金属学报, 2001; 11: 834)

[6] Wang J, He S X, Sun B D, Li K, Shu D, Zhou Y H. Mater Sci Eng, 2002; A338: 101

[7] Wang J, He S X, Sun B D, Guo Q X, Nishio M. J Mater Process Technol, 2003; 141: 29

[8] Wang Y S,Wang L D, Zhu D Y, QingW, Wen H Y, Liao L. Mater Mech Eng, 2011; 35(2): 12

[9] Oppermann H. In: Zschech E, Whelan C, Mikolajick T eds., Materials for Information Technology. London: Springer–Verlag Press, 2005: 377

[10] Ciulik J, Notis M R. J Alloys Compd, 1993; 191: 71

[11] Liu Z G, Chen D Q, Luo X M. Precious Met, 2005; 26: 62

(刘泽光, 陈登权, 罗锡明. 贵金属, 2005; 26: 62)

[12] Tsai J Y, Chang C W, Shieh Y C, Hu Y C, Kao C R. J Electron Mater, 2005; 34: 182

[13] Zhang G S, Jing H Y, Xu L Y, Wei J, Han Y D. J Alloys Compd, 2009; 476: 138

[14] Chidambaram V, Hattel J, Hald J. J Alloys Compd, 2010; 49: 170

[15] Chidambaram V, Hald J, Hattel J. J Alloys Compd, 2009; 49: 323

[16] Tan Q B, Deng C, Mao Y, He G. Gold Bull, 2011; 44: 27

[17] Novakovic R, Ricci E, Gnecco F, Giuranno D, Borzone G. Surf Sci, 2005; 599: 230

[18] Balagurusamy V S K, Streitel R, Shpyrko O G, Pershan P S, Meron M, Lin B H. Phys Rev, 2007; 15(10)B: 61

文章导航

/

〈 〉