(Y, Gd)2O3∶Eu3+纳米粒子制备过程中的合成动力学

  • 马伟民 ,
  • 朱红艳
展开
  • 1. 沈阳化工大学材料科学与工程学院~辽宁省稀土化学及应用重点实验室, 沈阳 110142
    2. 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016
    3. 东北大学材料与冶金学院, 沈阳 110819
朱红艳, 女, 1987年生, 硕士生

收稿日期: 2011-11-28

  修回日期: 2012-04-16

  网络出版日期: 2012-06-11

基金资助

辽宁省自然科学基金项目20062001和 沈阳市科技攻关计划项目F10-053-2-00资助

SYNTHESIS KINETICS OF (Y, Gd)2O3∶Eu3+ NANO-POWDERS DURING PROCESS OF PREPARATION

  • MA Wei-Min ,
  • ZHU Hong-Yan
Expand
  • 1. Key Laboratory for Rare-earth Chemical and Applying of Liaoning Province, School of Material Science and Engineering, Shenyang University of Chemical Technology, Shenyang 110142
    2. Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences,Shenyang 110016
    3. Institute of Metallurgy and Materials, Northeastern University, Shenyang 110819

Received date: 2011-11-28

  Revised date: 2012-04-16

  Online published: 2012-06-11

摘要

采用反向滴定共沉淀法制备出(Y, Gd)2O3∶Eu3+前躯体, 再在不同温度下煅烧, 获得(Y, Gd)2O3∶Eu3+纳米粒子, 用XRD和SEM对样品物相组成及形貌进行了表征; 用TG--DTA获得了样品在不同升温速率下的热分解曲线. 结果表明, 前躯体在煅烧过程中的物相变化分为3个阶段, 用Doyle-Ozawa法和Kissinger法分别计算出各个反应阶段的表观活化能, 其平均值分别为191.54, 557.05和236.58 kJ·mol-1, 并建立了动力学方程; (Y, Gd)2O3∶Eu3+晶粒生长活化能是35.58 kJ·mol-1, 纳米粒子形核过程中的晶粒长大由晶界扩散控制.

本文引用格式

马伟民 , 朱红艳 . (Y, Gd)2O3∶Eu3+纳米粒子制备过程中的合成动力学[J]. 金属学报, 2012 , 48(6) : 671 -677 . DOI: 10.3724/SP.J.1037.2011.00735

Abstract

Using NH3·H2·O and NH4HCO3 blended solution as a complex precipitation agent, (Y, Gd)2O3∶Eu3+ nano--particles were synthesized by co--precipitation reaction. XRD and SEM were applied to analyze the crystallization and morphology of the sample. The thermal decomposition curves of samples were analysed by TG-DTA at different heating rates. Results showed that under the conditions of pH=10 and reverse titration, the change process of (Y, Gd)2O3∶Eu3+ precursors is divided into three steps. The apparent activation energy of each step was calculated by using the Doyle--Ozawa and Kissinger methods. The calculated results are 191.54, 557.05 and 236.58 kJ·mol-1. The dynamic equations have been also established. The activation energy of (Y, Gd)2O3∶Eu3+ grain growth is 35.58 kJ·mol-1, indicating that  grain growing is primarily controlled by interfacial reaction during process of preparation.

参考文献

[1] van Eijk C W E.  Phys Med Biol, 2002; 47: 85

[2] Hell E, Knuepfer W, Mattern D.  Nucl Instrum Methods Phys Res, 2000; 454A: 40

[3] Jung Y S, Kim K H, Jang T Y, Tak Y, Baeck S H.  Curr Appl Phys, 2011; 11: 358·

[4] Louardi A, Rmili A, Ouachtari F, Bouaoud A, Elidrissi B, Erguig H. J Alloys Compd, 2011; 509: 9183

[5] Selvam N C S, Kumar R T, Yogeenth K, Kennedy L J, Sekaran G,Vijaga J J.  Powder Technol, 2011; 211: 250

[6] Gunawidjaja R, Myint T, Eilers H.  Ceram Int, 2012; 38: 775

[7] Taniguchi T, Watanabe T, Katsumata K, Okada K, Matsushita N. J Phys Chem, 2010; 114C: 3763

[8] Chien J T, Hsu D J, Inbaraj B S, Chen B H. Int J Mol Sci, 2010; 11: 2805

[9] Matiadis D, prousis K C, Markopoulou O I.  Molecules, 2009; 14: 3914

[10] Si W, Wang J, Wang X H, Gao H, Zhai Y C.  J Inorg Mater,2011; 26: 726

     (司伟, 王晶, 王修慧, 高宏, 翟玉春. 无机材料学报, 2011; 26: 726)

[11] Si W, Gao H, Wang J, Jiang D, Zhai Y C.  Chin J Inorg Chem,2010; 26: 1443

     (司伟, 高宏, 王晶, 姜妲, 翟玉春. 无机化学学报,2010; 26: 1443)

[12] Jie X F, Liang G C, Wang L, Zhi X K, Gao L M.  Adv Mater Res,2010; 178: 172

[13] Yu H Y, Ren W T, Zhang Y.  J Appl Polym Sci, 2009; 113: 17

[14] Zhuang Y X, Xing P F, Duan T F, Shi H Y, He J C.  J Rare Earths,2011; 29: 793

[15] Wang C S, Wang R Q, Wang Y, Fu Y X.  Key Eng Mater, 2012; 501: 349

[16] Dai J F, Ling R Q, Wang K Z.  Adv Mater Res, 2012; 418: 282

[17] Kok M V.  Fuel Process Technol, 2012; 96: 134

[18] Ma W M, Wen L, Shen S F, Liu J, Wang H D.  Acta Metall Sin,2009; 45: 759

     (马伟民, 闻雷, 沈世妃, 刘晶, 王华栋. 金属学报, 2009; 45: 759)

[19] Ozawa T.  Bull Chem Soc Jpn, 1965; 38: 1881

[20] Doyle C D.  J Appl Polym Sci, 1961; 5: 285

[21] Kisssinger H E.  J Res Nat Bue Stand, 1965; 57: 217

[22] Kissingger H E.  Anal Chem, 1957; 29: 1702

[23] Zhao Y N, Zhang W L.  Adv Mater Res, 2011; 194: 558

[24] Mullaugh K M, Luther G W.  J Nanopart Res,2011; 13: 393
 
文章导航

/