论文

定向凝固Al-40%Cu合金三维微观组织重构及共晶间距演变

  • 李双明 ,
  • 赵朋 ,
  • 傅恒志
展开
  • 西北工业大学凝固技术国家重点实验室, 西安 710072
赵朋, 男, 1987年生, 硕士生

收稿日期: 2011-07-15

  修回日期: 2011-12-12

  网络出版日期: 2012-01-11

基金资助

国家自然科学基金项目50971101和51074127及西北工业大学基础研究基金项目JC201029资助

THREE-DIMENSIONAL MICROSTRUCTURE RECONSTRUCTION AND THE EUTECTIC SPACING ADJUSTMENT DURING DIRECTIONAL SOLIDIFICATION OF Al-40%Cu HYPEREUTECTIC ALLOY

  • LI Shuang-Meng ,
  • DIAO Peng ,
  • FU Heng-Zhi
Expand
  • State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072

Received date: 2011-07-15

  Revised date: 2011-12-12

  Online published: 2012-01-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50971101 and 51074127) and Basic Research Foundation of NWPU (No.JC201029)

摘要

本文利用连续切片技术研究了定向凝固Al-40%Cu过共晶合金中金属间化合物Al2Cu 初生相的三维微观组织, 以及抽拉速率跃迁下, 三维共晶组织形态的演变和间距调整. 结果表明: 抽拉速率为5 µm/s时, 初生Al2Cu三维组织沿生长方向存在棱面和棱角, 表现出明显的棱面相生长形态; 凝固过程中初生Al2Cu相释放的结晶潜热使得生长界面发生局部重熔, 三维组织中出现孔洞, 形成拓扑缺陷. 在Al-40%Cu合金三维共晶组织中,  Al2Cu 相和Al相的体积分数分别为56.8%和43.2%, 且Al2Cu相的生长方向与试样轴向夹角为5.1o. 当抽拉速率从2 μm/s突然跃迁到500 μm/s时, 三维共晶组织形态从层片向棒状转变, 这种转变不是由合金中两相体积分数变化造成的. 三维共晶组织间距调整机制不同于二维组织中的分叉、内凹和界面重新形核, 而是通过三维空间非同一平面连续的分叉、分枝进行, 在三维下并没有观察到二维下的重新形核共晶间距调整机制.

本文引用格式

李双明 , 赵朋 , 傅恒志 . 定向凝固Al-40%Cu合金三维微观组织重构及共晶间距演变[J]. 金属学报, 2012 , 48(1) : 33 -40 . DOI: 10.3724/SP.J.1037.2011.00450

Abstract

Three-dimensional (3D) microstructures can clearly reveal the size, shape and distribution of the phases, providing a novel way to deeply understand the formation mechanism of the solidified phases. In this paper, by using the serial sectioning technique, the 3D microstructure of the primary Al2Cu phase was reconstructed and the eutectic spacing adjustment was investigated during directional solidification of Al-40%Cu hypereutectic alloy. The results show that the primary Al2Cu phase pattern was observed faceting due to the growing faceted angle and plane parallel to the solidification direction at the pulling rate of 5 μm/s. Further, there existed some hopper-like cavities in the 3D microstructure of the primary Al2Cu phase that caused by remelting owing to a large amount of the latent heat difficult to be extracted from the solidification interface. For the 3D eutectic microstructures of the Al-40%Cu alloy, the growth direction of the Al and Al2Cu phases in the coupled eutectics had a deviation angle of 5.1o with the heat flux direction and the phase volume fractions of the  Al and Al2Cu phases were measured directly to be 56.8% and 43.2%, respectively. In addition, at the abrupt change in pulling rate from 2 μm/s to 500 μm/s, the lamellar-to-rod eutectic transition was observed and the continuously splitting and branching occurred in different planes responsible for the eutectic spacing adjustment in the 3D microstructure of the Al-40%Cu alloy. Meanwhile the renuleation mechanism in the 2D microstructure for the adjustment of the eutectic spacing did not work in the 3D eutectic microstructure of the Al-40%Cu alloy.

参考文献

[1] Spanos G. Scr Mater, 2006; 55: 3

[2] Isheim D, Kolli R P, Fine M E, Seidman D N. Scr Mater, 2006; 55: 35

[3] Liu H H, Schmidt S, Poulsen H F, Godfrey A, Liu Z Q, Sharon J A, Huang X. Science, 2011; 332: 833

[4] Khor K H, Buffiere J Y, Ludwig W, Sinclair I. Scr Mater, 2006; 55: 47

[5] Spowart J E. Scr Mater, 2006; 55: 5

[6] Mendoza R, Savin I, Thornton K, Voorhees P W. Nat Mater, 2004; 3: 385

[7] Wu D T. Nat Mater, 2004; 3: 353

[8] Kammer D, Voorhees P W. Acta Mater, 2006; 54: 1549

[9] Kammer D, Mendoza R, Voorhees P W. Scr Mater, 2006; 55: 17

[10] Luo L S, Wang X, Su Y Q, Li X Z, Guo J J, Fu H Z. Mater Rev, 2010; 24: 1

(骆良顺, 王新, 苏彦庆, 李新中, 郭景杰, 傅恒志. 材料导报, 2010; 24: 1)

[11] Lee J H, Liu S, Trivedi R. Metall Mater Trans, 2005; 36A: 3111

[12] Norris S A, Davis S H, Watson S J, Voorhees P W. J Cryst Growth, 2008; 310: 414

[13] Dantzig J A, Rappaz M. Solidification. Swiss: EPFL Press, 2009: 362

[14] Walkers H, Liu S, Lee J H, Trivedi R. Metall Mater Trans, 2007; 38A: 1417

[15] Quan Q R, Li S M, Fu H Z. Acta Metall Sin, 2010; 46: 500

(全琼蕊, 李双明, 傅恒志. 金属学报, 2010; 46: 500)

[16] Contieri R J, Rios C T, Zanotello M, Caram R. Mater Charact, 2008; 59: 693

[17] Singh H, Gokhale A M, Tewari A, Zhang S, Mao Y. Scr Mater, 2009; 61: 441

[18] Lee S G, Gokhale A M, Sreeranganathan A. Mater Sci Eng, 2006; 427: 92

[19] Liu S, Lee J H, Enlow D, Trivedi R. In: Rappaz M, Beckermann C, Trivedi R eds., Solidification Processes and Microstructures. Charlotte: TMS, 2004: 257

[20] Hunt J D, Liu S Z. Handbook of Crystal Growth, Vol.2, North–Holland: Elsevier, 1994: 1113

[21] Stefanescu D M. Science and Engineering of Casting Solidification. 2nd Ed., Berlin: Springer, 2009: 215

[22] Kurz W, Fisher D J. Fundamentals of solidification. 4th Ed., Switzerland: Trans Tech Pub, 2005: 109

[23] Tang L, Li S M, Fu H Z. Rare Met Mater Eng, 2007; 36: 617

(唐玲, 李双明, 傅恒志. 稀有金属材料与工程, 2007; 36: 617)

[24] Sunagawa I. Morphology and Perfection. Cambridge: Cambridge University Press, 2005: 370

[25] Colfen H, Antonietti M. Mesocrystals and Nonclassical Crystallization. Mississauga: John Wiley & Sons Ltd, 2008: 25

[26] Singh H, Gokhale A M, Mao Y, Tewari A, Sachdev A K. J Cryst Growth, 2009; 311: 4454

[27] Cantor B, Chadwick G A. J Cryst Growth, 1974; 23: 12

[28] Seetharamn V, Trivedi R. In: Stefanescu D M, Abbashian G J eds., Solidification Processing of Eutectic Alloys. Cincinnati: TMS, 1988: 65

[29] Hu H Q. Theory of Metal Solidification. 2nd Ed., Beijing: China Machine Press, 2000: 175

(胡汉起. 金属凝固原理. 第2版, 北京: 机械工业出版社, 2000: 175)
文章导航

/

〈 〉