外加电位对X80管线钢在鹰潭土壤模拟溶液中应力腐蚀行为的影响

  • 王长朋 ,
  • 杜翠薇 ,
  • 刘智勇 ,
  • 李晓刚
展开
  • 1) 北京科技大学腐蚀与防护中心, 北京 100083
    2) 北京市腐蚀、磨蚀与表面技术开放实验室, 北京 100083
刘智勇, 男, 1978年生, 博士

收稿日期: 2011-01-19

  修回日期: 2011-07-25

  网络出版日期: 2011-11-11

基金资助

国家自然科学基金项目50901041和中央高校基本科研业务费专项资金项目FRF-TP-09-029B资助

EFFECT OF APPLIED POTENTIALS ON STRESS CORROSION CRACKING OF X80 PIPELINE STEEL IN SIMULATED YINGTAN SOIL SOLUTION

  • YU Zhang-Peng ,
  • DU Cui-Wei ,
  • LIU Zhi-Yong ,
  • LI Xiao-Gang
Expand
  • 1) Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083
    2) Key Lab of Corrosion, Erosion and Surface Technique of Beijing, Beijing 100083

Received date: 2011-01-19

  Revised date: 2011-07-25

  Online published: 2011-11-11

Supported by

Supported by National Natural Science Foundation of China (No.50901041) and the Fundamental Research Funds for the Central Universities (No.FRF-TP-09-029B)

摘要

采用电化学动电位极化技术、慢应变速率拉伸(SSRT)实验和SEM对X80管线钢在鹰潭土壤模拟溶液中的应力腐蚀行为进行了研究. 结果表明: X80管线钢在酸性土壤环境中具有较高的SCC敏感性, 其断口模式为穿晶SCC; SCC机制随外加电位的不同而改变, 在外加电位高于-930 mV时, 其SCC机制由阳极溶解和氢致腐蚀两种电极过程控制, 呈现阳极溶解和氢脆复合机制; 当电位低于该电位时, 其SCC为氢脆机制. 随着外加阴极电位的降低, X80管线钢的SCC敏感性不断增大; 与X70钢相比, 氢脆作用在X80管线钢SCC过程中发挥了更重要的作用.

本文引用格式

王长朋 , 杜翠薇 , 刘智勇 , 李晓刚 . 外加电位对X80管线钢在鹰潭土壤模拟溶液中应力腐蚀行为的影响[J]. 金属学报, 2011 , 47(11) : 1434 -1439 . DOI: 10.3724/SP.J.1037.2011.00046

Abstract

Stress corrosion cracking (SCC) of X80 pipeline steel in a simulated solution of the acidic soil environments in Yingtan China was studied by means of potentiodynamic polarization curves, slow strain rate test (SSRT) and corrosion morphologies characterized by SEM. The results show that X80 pipeline steel has high SCC susceptibility in the simulated solution and the failure mode is transgranular cracking. The SCC mechanism would vary with the applied cathodic potential. When the applied potential is positive to about -930 mV, the SCC behavior is controlled by the combined effect of anodic dissolution (AD) and hydrogen embrittlement (HE), i.e. the SCC mechanism is AD+HE. However, when the applied potentials are lower than -930 mV, such as -1000 and -1200 mV,  the process of hydrogen evolution plays the dominant role in SCC occurrence, meaning that the SCC mechanism is HE under such applied potentials. Moreover, SCC susceptibility increases with decreasing applied cathodic potential. Compared with X70 pipeline steel in acidic soil environments, HE plays a more important role in affecting SCC occurrence.

参考文献

[1] Liu Z Y, Li X G, Du C W, Zhai G L, Cheng Y F. Corros Sci, 2008; 50: 2251

[2] Zhai G L, Liu Z Y, Du C W, Li X G, Wang L X. Corros Prot, 2009; 30: 149

(翟国丽, 刘智勇, 杜翠薇, 李晓刚, 王立贤. 腐蚀与防护, 2009; 30: 149)

[3] L¨u X Y, Wang Y, Li J C. Electr Weld Machine, 2009; 39(5): 121

(吕向阳, 王义, 李景昌. 电焊机, 2009; 39(5): 121)

[4] Liang P, Du C W, Li X G, Chen X, Zhang L. Int J Miner, Metall Mater, 2009; 16: 407

[5] Gu B, Luo J L, Mao X. Corrosion, 1999; 55: 96

[6] Gu B, Yu W Z, Luo J L,Mao X. Corrosion, 1999; 55: 312

[7] Wang B Y, Huo L X, Wang D P, Deng C Y. J Tianjin Univ, 2007; 40: 757

(王炳英, 霍立兴, 王东坡, 邓彩艳. 天津大学学报, 2007; 40: 757)

[8] Su D L, Feng Y, Chen J B. Mechanical Properties of Engineering Materials. Beijing: China Machine Press, 2005: 1

(束德林, 凤 仪, 陈九磅. 工程材料力学性能. 北京: 机械工业出版社, 2005: 1)

[9] Chu W Y, Qiao L J, Chen Q Z. Fault Rupture and the Environment. Beijing: Science Press, 2000: 109

(禇武扬, 乔利杰, 陈奇志. 断裂与环境断裂. 北京: 科学出版社, 2000: 109)

[10] Ogundele G I, White W E. Corrosion, 1986; 42: 71

[11] Zhang L F. J Iron Steel Res Int, 2006; 13(3): 01

[12] Garet M, Brass A M, Haut C, Solana F G. Corros Sci, 1998; 40: 1073

[13] Parkins R N. Corros Sci, 1980; 20: 147

[14] Liu Z Y, Li X G, Du C W, Zhai G C, Cheng Y F. Corros Sci, 2008; 50: 2251

[15] Cheng Y F, Niu L. Electrochem Commun, 2007; 9: 558

[16] Chen W, Fang K, Vokes E. Corrosion, 2002; 58: 267

[17] Liu Z Y, Zhai G L, Du C W, Li X G. Acta Metall Sin, 2008; 44: 209

(刘智勇, 翟国丽, 杜翠薇, 李晓刚. 金属学报, 2008; 44: 209)

[18] Liu Z Y, Li X G, Du C W, Lu L, Zhang Y R, Cheng Y F. Corros Sci, 2009; 51: 895
文章导航

/

〈 〉