论文

交流电对Q235钢腐蚀电位的影响规律研究

  • 姜子涛 ,
  • 杜艳霞 ,
  • 董亮 ,
  • 路民旭
展开
  • 北京科技大学新材料技术研究院, 北京 100083
姜子涛, 男, 1986年生, 博士生

收稿日期: 2011-01-17

  修回日期: 2011-04-26

  网络出版日期: 2011-08-11

基金资助

北京市自然基金重大项目3080001和北京市科技计划重大项目D08050303450802资助

EFFECT OF AC CURRENT ON CORROSION POTENTIAL OF Q235 STEEL

  • JIANG Zi-Shou ,
  • DU Yan-Xia ,
  • DONG Liang ,
  • LUO Min-Xu
Expand
  • Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083

Received date: 2011-01-17

  Revised date: 2011-04-26

  Online published: 2011-08-11

Supported by

Supported by Major Project of Beijing Natural Science Foundation (No.3080001) and Beijing Science and Technology Program of Major Projects (No.D08050303450802)

摘要

利用室内模拟实验研究了交流电密度、电解质组分以及交流电频率对Q235钢腐蚀电位的影响规律. 研究结果表明, 交流电会使Q235钢腐蚀电位发生正向或负向偏移, 偏移方向与Q235钢在不同电解质中阴、阳极极化速率有一定的相关性; 偏移量随交流电密度增大而增大,随交流电频率增大而减小. 结合金属界面双电层模型和腐蚀产物分析,对交流电引起Q235钢腐蚀电位偏移的机理进行了探讨.

本文引用格式

姜子涛 , 杜艳霞 , 董亮 , 路民旭 . 交流电对Q235钢腐蚀电位的影响规律研究[J]. 金属学报, 2011 , 47(8) : 997 -1002 . DOI: 10.3724/SP.J.1037.2011.00040

Abstract

With the rapid development of electricity, petroleum and transport industry, more and more pipelines are buried in parallel with high–voltage transmission lines or electrified railways, and the resulting AC corrosion phenomenon has attracted more attentions. In this work, the effects of AC current density, electrolyte composition and AC current frequency on corrosion potential of Q235 steel were studied through simulation experiments, and the results are as follows: AC current makes corrosion potential of Q235 steel deviate positively or negatively depending on polarization rate of anode/cathode within different electrolytes, and the offset of corrosion potential becomes more significant as the AC current density increases or the AC current frequency decreases. Besides, the inherent mechanism of such offset induced by AC current was also studied through double layer model of interface and corrosion products analyses.

参考文献

[1] Wakelin R G, Gummow R A, Segall S M. Corrosion–1998, Houston: NACE, 1998: 565

[2] Gummow R A, Wakelin R G, Segall S M. Corrosion–1998, Houston: NACE, 1998: 566

[3] Linhardt P, Ball G. Corrosion–2006, Houston: NACE, 2006: 160

[4] Wakelin R G. Corrosion–2004, Houston: NACE, 2004: 205

[5] Kim D K, Muralidharan S, Ha T H, Bae J H, Ha Y C, Lee H G, Scatlebury J D. Electrochim Acta, 2006; 51: 5259

[6] Muralidharan S, Kim D K, Ha T H, Bae J H, Ha Y C, Lee H G, Scantlebury J D. Desalination, 2007; 216: 103

[7] Ormellese M, Lazzari L, Brenna A. Corrosion–2010, Houston: NACE, 2010: 109

[8] Ormellese M, Lazzari L, Brenna A, Trombetta A. Corrosion–2010, Houston: NACE, 2010: 032

[9] Panossian Z, Filho S E A, de Almeida N L, Pereira Filho M L, Silva D D L, Laurino EW, Oliver J H D L, Pimenta G D S, Albertini J A D C. Corrosion–2009, Houston: NACE, 2009: 541

[10] Goidanich S, Lazzari L, Ormellese M. Corros Sci, 2010; 52: 916

[11] Goidanich S, Lazzari L, Ormellese, M. Corros Sci, 2010; 52: 491

[12] Bosch R W, Bogaerts W F. Corros Sci, 1998; 40: 323

[13] Lalvani S B, Lin X. Corros Sci, 1996; 38: 1709

[14] Bertocci U. Corrosion, 1979; 35: 211

[15] Fu A Q, Cheng Y F. Corros Sci, 2010; 52: 612

[16] Li Z L, Ding Q M, Zhang Y F, Li J J, Li S L. Corros Prot, 2010; 31: 436

(李自力, 丁清苗, 张迎芳, 李静静, 李胜利. 腐蚀与防护, 2010; 31: 436)

[17] Ying K H, Tang M H, Xiong X J. J Chin Soc Corros Prot, 1982; 2: 33

(尹可华, 唐明华, 熊祥键. 中国腐蚀与防护学报, 1982; 2: 33)

[18] Kulman F E. Corrosion, 1961; 17(3): 34

[19] Goidanich S, Lazzari L, Ormellese M, Pedeferri M. Corrosion–2005, Houston: NACE, 2005: 189

[20] Jones D A. Corrosion, 1978; 34: 428

[21] Cao C N. Principles of Electrochemistry of Corrosion. Beijing: Chemical Industry Press. 2008: 53

(曹楚楠. 腐蚀电化学原理. 北京: 化学工业出版社, 2008: 53)
文章导航

/

〈 〉