论文

板坯连铸结晶器内钢凝固过程热行为研究  II. 模型验证与结果分析

  • 蔡兆镇 ,
  • 朱苗勇
展开
  • 东北大学材料与冶金学院, 沈阳 110004
蔡兆镇, 男, 1982年生, 博士生

收稿日期: 2010-12-09

  修回日期: 2011-03-31

  网络出版日期: 2011-06-11

基金资助

国家杰出青年科学基金项目50925415和教育部基本科研业务费项目N100102001资助

SIMULATION OF THERMAL BEHAVIOR DURING STEEL SOLIDIFICATION IN SLAB CONTINUOUS CASTING MOLD II. Model Verification and Results Analysis

  • SA Zhao-Tian ,
  • ZHU Miao-Yong
Expand
  • School of Materials and Metallurgy, Northeastern University, Shenyang 110004

Received date: 2010-12-09

  Revised date: 2011-03-31

  Online published: 2011-06-11

Supported by

Supported by National Outstanding Young Scientist Foundation of China (No.50925415) and Fundamental Research Funds for the Central University of China (No.N100102001)

摘要

基于建立的二维瞬态热/力耦合有限元模型, 模拟计算了国内某钢厂实际板坯连铸工况下结晶器内某高强船板钢凝固过程的热行为, 并利用现场实测温度数据验证了模型的可靠性. 在此基础上重点研究分析了该钢在结晶器凝固过程角部区域气隙厚度、坯壳--铜板间的保护渣(包括液渣层和固渣层)分布及其热行为变化规律和对应区域的热流与表面温度变化特征,并揭示了拉速、结晶器锥度和保护渣性能变化对该钢种在结晶器内凝固热行为的影响.

本文引用格式

蔡兆镇 , 朱苗勇 . 板坯连铸结晶器内钢凝固过程热行为研究  II. 模型验证与结果分析[J]. 金属学报, 2011 , 47(6) : 678 -687 . DOI: 10.3724/SP.J.1037.2010.00664

Abstract

Based on the thermal–mechanical coupling finite element model described in Part I of present work, the thermal behavior of one high strength ship plate steel solidifying in slab continuous casting mold was simulated with the practical continuous casting conditions of a steel plant, and the availability of the model was verified by in–plant measurement temperature. With this model, the thickness distributions and thermal behavior of air gap, mold flux (including liquid flux and solidified flux), and the variation characteristics of heat flux and surface temperature, as well as the influence of casting speed, mold taper, and mold flux properties on thermal behavior of the steel solidifying in mold were investigated.

参考文献

[1] Yamauchi A, Emi T, Seetharaman S. ISIJ Int, 2002; 42: 1084

[2] Cho J W, Shibata H, Emi T. ISIJ Int, 1998; 38: 440

[3] Yamauchi A, Sorimachi K, Sakuraya T, Fujii T. ISIJ Int, 1993; 33: 140

[4] Thomas B G, Moitra A, McDavid R. Iron Steelmaker (ISS Transaction), 1996; 23: 57

[5] CaZ Z, Zhu M Y. Acta Metall Sin, 2011; 47: 671

(蔡兆镇, 朱苗勇. 金属学报, 2011; 47: 671)

[6] Liu X D, Zhu M Y, Cheng N L. Acta Metall Sin, 2006; 42:1081

(刘旭东, 朱苗勇, 程乃良. 金属学报, 2006; 42: 1081)

[7] Li C S, Thomas B G. Metall Trans, 2004; 35B: 1151

[8] Han H N, Lee J E, Yeo T, Won Y M, Kim K H, Oh K H, Yoon J K. ISIJ Int, 1999; 39: 445

[9] Mizukami H, Murakami K. Tetsu Hagan´e, 1977; 63: S652

(水上秀昭, 村上腾彦. 铁と钢,1977; 63: S652)

[10] Uehara M, Samarasekera I V, Brimacombe J K. Ironmaking Steelmaking, 1986; 13: 138

[11] Anand L. Trans ASME, 1982; 104: 12

[12] Brown S B, Kim K H, Anand L. Int J Plast, 1989; 5: 95

[13] Koric S, Thomas B G. J Mater Process Technol, 2008; 197:408

[14] Saraswat R, Maijer D M, Lee P D, Mills K. ISIJ Int, 2007;47: 95

[15] Nakada H, Susa M, Seko Y, Hayashi M, Nagata K. ISIJ Int, 2008; 48: 446
文章导航

/

〈 〉