时效处理和La含量对AZ91合金组织和力学性能的影响

  • 王社斌 ,
  • 祁小叶 ,
  • 张金玲 ,
  • l刘璐
展开
  • 1.太原理工大学材料科学与工程学院, 太原 030024
    2.太原理工大学教育部新材料界面与工程重点实验室, 太原 030024
王社斌, 男, 1962年生, 教授

收稿日期: 2010-10-21

  修回日期: 2011-03-03

  网络出版日期: 2011-06-11

基金资助

国家自然科学基金项目50901048和山西省回国留学人员科研项目2008-39资助

EFFECT OF AGING TREATMENT AND La CONTENT ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF AZ91 ALLOY

  • YU She-Bin ,
  • ZHI Xiao-Xie ,
  • ZHANG Jin-Ling
Expand
  • 1. College of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan 030024
    2. Key Laboratory of Interface Science and Engineering in Advanced Materials Taiyuan University of Technology, Ministry of Education, Taiyuan 030024

Received date: 2010-10-21

  Revised date: 2011-03-03

  Online published: 2011-06-11

Supported by

Supported by National Natural Science Foundation of China (No.50901048) and Returned Overseas Graduates Scientific Research Projects of Shanxi Province (No.2008–39)

摘要

借助XRD, SEM, EDS和显微硬度仪等分析测试手段, 研究了时效处理和La含量对真空精炼的AZ91合金显微组织和力学性能的影响. 结果表明: 时效处理可以使第二类β相大量析出, 且β相呈不连续层片状沿晶界两侧分布.随La含量的增加, β相的尺寸逐渐减小, 而α相的尺寸则呈现先减小后增加的趋势. 铸态和时效态试样的力学性能参数均随La含量的增加呈现出先增加后减小的趋势. 时效态试样的抗拉强度、屈服强度、延伸率和Vickers硬度分别比铸态试样提高12.65%, 16.85%, 13.71%和37.24%. 当La含量达到0.1648%时,抗拉强度、屈服强度、延伸率和Vickers硬度分别达到276 MPa, 208 MPa, 13.85%和132 HV.

本文引用格式

王社斌 , 祁小叶 , 张金玲 , l刘璐 . 时效处理和La含量对AZ91合金组织和力学性能的影响[J]. 金属学报, 2011 , 47(6) : 743 -750 . DOI: 10.3724/SP.J.1037.2010.00560

Abstract

The effects of aging treatment and La content on the microstructures and mechanical properties of AZ91 magnesium alloys were investigated by XRD, SEM, EDS and microhardness meter. The results showed that a great number of β–phases were precipitated and distributed along the grain boundaries after aging treatment. As the content of La increased, the grain size of β–phase decreased gradually, while α–phase decreased first and then increased. The mechanical properties of as–cast and aged specimens increased first and then decreased as the cotet of La increased. The tensile strength, yield strength, elongatin and Vickers hardness of aged magesium alloys were increased by 12.65%, 16.85%, 13.71% and 37.24%, espectively. When the content of La was 0.1648%, the tensile strength, yield strength, elongation and Vickers hardness achieved 276 MPa, 208 MPa, 13.85% and 132 HV, respectively.

参考文献

[1] Aghion E, Bronfin B, Eliezer D. J Mater Process Technol, 2001; 117: 381

[2] Mordike B L, Ebert T. Mater Sci Eng, 2001; A302: 37

[3] Wang S B, Li X B, Fan J P, Wang S, Xu B S. Chin J Nonfer Met, 200919: 831

(王社斌, 李晓斌, 范晋平, 王 帅, 许并社. 中国有色金属学报, 2009; 19: 831)

[4] Cizek L, Greger M, Pawlica L, Dobrzanski L A, Tanski T. J Mater Process Technol, 2004; 157–158: 466

[5] Li P J, Tang B, Kandal ova E G. Mater Lett, 2005; 59: 671

[6] Zeng X Q, Wu Y J, Peng L M, Lin D, Ding W J, Peng Y H. Acta Metall Sin, 2010; 46: 1043

(曾小勤, 吴玉娟, 彭立明, 林栋樑, 丁文江, 彭赢红. 金属学报, 2010; 46: 1043)

[7] Wang K Q, Wang G J, Zhang J L, Wang S B, Xu B S. J Taiyuan Univ Technol, 2011; 1: 67

(王克勤, 王国军, 张金玲, 王社斌, 许并社. 太原理工大学学报, 2011; 1: 67)

[8] Wang S B, Zhang J L, Qi X Y, Xu B S. J Mater Eng, 2009; (Suppl. 1): 304

(王社斌, 张金玲, 祁小叶, 许并社. 材料工程, 2009; (增刊1): 304)

[9] Zhao Y H, Chen Y G, Tang Y B, Xiao S F, Wei S H, Zhang X P, Wang Q, Tu M J. Rare Met Mater Eng, 2010; 39: 844

(赵源华, 陈云贵, 唐永柏, 肖素芬, 魏尚海, 章晓萍, 王卿, 涂铭旌. 稀有金属材料与工程, 2010; 39: 844)

[10] Ma Y, Pan Z F, Zhang H F, Hao Y. J Lanzhou Univ Technol, 2009; 5: 9

(马 颖, 潘振峰, 张洪锋, 郝 远. 兰州理工大学学报, 2009; 5: 9)

[11] Ma Y L, Peng H D, Pan C C, Qin X, Du Y. Hot Work Technol, 2008; 37(10): 51

(麻彦龙, 彭华东, 潘承聪, 秦旭, 杜勇. 热加工工艺, 2008;37(10): 51)

[12] Xiao X L, Luo C P. Acta Metall Sin, 2001; 37: 2

(肖晓玲, 罗承萍. 金属学报, 2001; 37: 2 )

[13] Luo C P, Xiao X L, Liu J W. Acta Metall Sin, 2002; 38: 709

(罗承萍, 肖晓玲, 刘江文. 金属学报, 2002; 38: 709)

[14] Tang W, Han E H, Xu Y B, Liu L. Acta Metall Sin, 2005; 41: 1204

(唐 伟, 韩恩厚, 许永波, 刘 路. 金属学报, 2005; 41: 1204)

[15] Zhang J M, Jang B L, WanZ H, Yuan S, Xia P J. Heat Treat Met, 2007; 32: 7

(张菊梅, 蒋百灵, 王志虎, 袁 森, 夏鹏举. 金属热处理, 2007; 32: 7)

[16] Duly D, Cheynet M C, Brechet Y. Acta Metall Mater, 1994; 42: 3855

[17] Ren Z Y. Master Dissertation, Southwest University of Science and Technology, Mianyang, 2007

(任志远. 西南科技大学硕士学位论文, 绵阳, 2007)

[18] Xu B S, Wang S B, Zhang J L, Zhang J Y, Li M Z, Yao X H, Chen J, Wei Y H. Chin Pat, 0102168.9, 2008

(许并社, 王社斌, 张金玲, 张俊远, 李明照, 姚宪华, 陈 津, 卫英慧.中国专利, 0102168.9, 2008)

[19] Zhang J L. Master Dissertation, Taiyuan University of Technology, 2007

(张金玲. 太原理工大学硕士学位论文, 2007)

[20] Li Z J, Jin Q L, Jiang Y H, Zhou R. Acta Metall Sin, 2009; 45: 928

(李再久, 金青林, 蒋业华, 周荣. 金属学报, 2009; 45: 928)
文章导航

/

〈 〉