论文

重碳酸盐溶液中SO42-和Cl-对低碳钢活化/钝化腐蚀行为的影响

  • 董俊华 ,
  • 阳靖峰 ,
  • 柯伟
展开
  • 中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016
阳靖峰, 男, 1983年生, 博士生

收稿日期: 2011-03-15

  修回日期: 2011-05-03

  网络出版日期: 2011-10-11

基金资助

国家自然科学基金资助项目51071160

EFFECTS OF SO42− AND Cl ON ACTIVE/PASSIVE CORROSION BEHAVIORS OF LOW CARBON STEEL IN DEAERATED BICARBONATE SOLUTION

  • DONG Jun-Hua ,
  • YANG Jing-Feng ,
  • KE Wei
Expand
  • State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences,
    Shenyang 110016

Received date: 2011-03-15

  Revised date: 2011-05-03

  Online published: 2011-10-11

Supported by

Supported by National Natural Science Foundation of China (No.51071160)

摘要

在除O2的0.1 mol/L NaHCO3, 0.1 mol/L NaHCO3+0.1 mol/LNa2SO4以及0.1 mol/L NaHCO3+0.1 mol/L NaCl溶液中,用恒电位法在低碳钢电极表面制备腐蚀产物, 并原位监测低碳钢的开路电位,用SEM观察腐蚀形貌, 用XRD确定腐蚀产物的相组成. 结果表明,在0.1 mol/L NaHCO3溶液中, 低碳钢的开路电位最终处于再钝化区间,其表面未观察到明显的腐蚀现象; 在0.1 mol/L NaHCO3+0.1 mol/L Na2SO4溶液中, 低碳钢的开路电位最终处于再活化区间, 其表面发生均匀腐蚀; 在0.1 mol/L NaHCO3+0.1 mol/L NaCl溶液中, 低碳钢的开路电位最终亦处于再活化区间, 而其表面却发生局部腐蚀. XRD结果表明, 低碳钢表面的腐蚀产物主要为 Fe3O4和α-FeOOH.

本文引用格式

董俊华 , 阳靖峰 , 柯伟 . 重碳酸盐溶液中SO42-和Cl-对低碳钢活化/钝化腐蚀行为的影响[J]. 金属学报, 2011 , 47(10) : 1321 -1326 . DOI: 10.3724/SP.J.1037.2011.00134

Abstract

The corrosion behaviors of low carbon steel, a kind of materials used in making metal container sealing high–level radioactive waste, in three deaerated bicarbonate solutions simulated the ground water, 0.1 mol/L NaHCO3 solution, 0.1 mol/L NaHCO3+0.1 mol/L Na2SO4 solution and 0.1 mol/L NaHCO3+0.1 mol/L NaCl solution, were examined. The results in potential evolution revealed that the low carbon steel moved up to the passive state in 0.1 mol/L NaHCO3 solution while moved up to the re–active state in the other solutions. SEM observations showed that the low carbon steel was not corroded in 0.1 mol/L NaHCO3 solution, while homogeneous corrosion occurred in 0.1 mol/L NaHCO3+0.1 mol/L Na2SO4 solution and local corrosion in the third solution. XRD analyses illustrated that the corrosion products are composed of Fe3O4 and α–FeOOH.

参考文献

[1] Wang J, Su R, Chen W M, Guo Y H, Jin Y X, Wen Z J, Liu Y M. Chin J Rock Mech Eng, 2006; 25: 649

(王 驹, 苏锐, 陈伟明, 郭永海, 金远新, 温志坚, 刘月妙.岩石力学与工程学报, 2006; 25: 649)

[2] Guo Y H, Wang J, Wang Z M, Liu S F, Su R. Bull Mineral Petrol Geochem, 2007; z1: 607

(郭永海, 王驹, 王志明, 刘淑芬, 苏锐. 矿物岩石地球化学通报, 2007; z1: 607)

[3] Nagayama M, Cohen M. J Electrochem Soc, 1963; 110: 670

[4] Castro E B, Valentini C R, Moina C A, Vilche J R, Arvia A J. Corros Sci, 1986; 26: 781

[5] Rangel C M, Leitao R A, Fonseca I T. Electrochim Acta, 1989; 34: 255

[6] El–Naggar M M. Appl Surf Sci, 2006; 252: 6179

[7] Zhao J M, Zuo Y, Xiong J P, Tian L P. Corros Sci Prot Technol, 2001; 13: 77

(赵景茂, 左禹, 熊金平, 田连朋. 腐蚀科学与防护技术, 2001; 13: 77)

[8] Cao J S, Chen J J, Cao D Z. Corros Sci Prot Technol, 1991; 3: 2

(曹家绶, 陈家坚, 曹殿珍. 腐蚀科学与防护技术, 1991; 3: 2)

[9] Val´eria A A, Christopher Brett M A. Electrochim Acta, 2002; 47: 2081

[10] Zeng Y M, Luo J L. Electrochim Acta, 2003; 48: 3551

[11] Li D G, Feng Y R, Bai Z Q, Zhu J W, Zheng M S. Electrochim Acta, 2007; 52: 7877

[12] Yang J F, Dong J H, Ke W, Chen N. Acta Metall Sin, 2011; 47: 152

(阳靖峰, 董俊华, 柯伟, 陈楠. 金属学报, 2011; 47: 152)

[13] Pourbaix M. Lectures on Electrochemical Corrosion. New York: Plenum Press, 1973: 29

[14] Cao C N. Principle of Electrochemistry Corrosion. Beijing: Chemical Industry Press, 2004: 292

(曹楚南. 腐蚀电化学原理. 北京: 化学工业出版社, 2004: 292)
文章导航

/