用质子导体传感法研究钢在脱氢热处理中氢的行为

  • 厉英 ,
  • 丁玉石 ,
  • 胡井涛 ,
  • 王常珍
展开
  • 东北大学材料与冶金学院, 沈阳 110819
国家自然科学基金项目50774018和51074038资助

收稿日期: 2010-11-16

  修回日期: 2011-01-13

  网络出版日期: 2011-05-11

基金资助

国家自然科学基金项目50774018和51074038资助

STUDY ON THE BEHAVIOR OF HYDROGEN IN STEEL HEAT TREATMENT PROCESS WITH PROTON CONDUCTOR SENSOR

  • LI Yang ,
  • DING Yu-Shi ,
  • HU Jing-Shou ,
  • YU Chang-Zhen
Expand
  • College of Materials and Metallurgy, Northeastern University, Shenyang 110819

Received date: 2010-11-16

  Revised date: 2011-01-13

  Online published: 2011-05-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50774018 and 51074038)

摘要

采用CaZr0.9In0.1O3-α质子导体传感法测定了钢脱H热处理过程中H的行为. 氢传感器的阻抗谱表明氢传感器工作稳定, 测定的数据精确可靠. 测量了2钢种的pH2随温度的变化, 及在600和800℃恒温时, pH2随时间的变化, 分析了不同温度下钢脱H的效果, 研究了H析出过程的速度限制步骤.实验结果表明, 所研究的钢样去H热处理温度应高于600℃才能有效脱H, 而温度大于727℃并不能进一步脱H.本文实验说明质子导体传感器可以用于在线、连续地检测固体钢中pH2的变化.

本文引用格式

厉英 , 丁玉石 , 胡井涛 , 王常珍 . 用质子导体传感法研究钢在脱氢热处理中氢的行为[J]. 金属学报, 2011 , 47(5) : 553 -558 . DOI: 10.3724/SP.J.1037.2010.00615

Abstract

The dehydrogenation behavior in two steels during heat treatment process was investigated by using CaZr0.9In0.1O3-α proton conductor hydrogen sensor and electrochemical impedance spectroscopes of these steels have been measured and analyzed. Based on the changes of hydrogen partial pressure in these steels with temperature and with time at constant temperatures of 600℃ and 800℃, it is found that the dehydrogenation begins only when heat treatment temperature is higher than 600℃. Although this temperature exceeds higher than 727℃, the dehydrogenation behavior is not significantly improved. This means that the reasonable heat treatment temperature is in the range of 600-730℃. The experimental results show that the CaZr0.9In0.1O3-α proton conductor hydrogen sensor could be used to monitor in situ changes of partial hydrogen pressure during dehydrogenation of solid state steels as a suitable sensor.

参考文献

[1] Nagumo M, Yagi T, Saitoh H. Acta Mater, 2000; 48: 943

[2] Ohmisawa T, Uchiyama S, Nagumo M. J Alloys Compd, 2003; 356–357: 290

[3] Nagumo M, Matsuda H. Philos Mag, 2002; 82A: 3415

[4] Zhu J C, Li D C. Foundry Technol, 2003; 24(2): 83

(朱家琛, 李德臣. 铸造技术, 2003; 24(2): 83)

[5] Kanezaki T, Narazaki C, Mine Y, Matsuoka S, Murakami Y. Int J Hydrogen Energy, 2008; 10: 2604

[6] Singh S, Altstetter C. Metall Trans, 1982; 10A: 1799

[7] Zheng C L, Zhang F C, L¨u B, Wang T S, Zheng Y Z. Trans Mater Heat Treat, 2008; 29(2): 71

(郑春雷, 张福成, 吕 博, 王天生, 郑炀曾. 材料热处理学报, 2008; 29(2): 71)

[8] Melnick L M. Translated by Liu C S. Determination of Gaseous Elements in Metals. Beijing: Metallurgy Industry Press, 1987: 19

(Melnick L M, 刘崇嗣译. 金属中气体元素的测定. 北京: 冶金工业出版社, 1987: 199)

[9] Bilic A, Gale J D. Solid State Ionics, 2008; 179: 871

[10] Mercier V M M, Sluis P V D. Solid State Ionics, 2001; 145: 17

[11] Pollet M, Daturi M, Marinel S. J Eur Ceram Soc, 2004; 24: 1805

[12] Yajima T, Kazeoka H, Yogo T, Iwahara H. Solid State Ionics, 1991; 47: 271

[13] Iwahara H, Shimura T, Matsumoto H. Electrochemistry, 2000; 68: 154

[14] Katahira K, Matsumoto H, Iwahara H, Koide K, Iwamoto T. Sens Actuators, 2001; 73B: 130

[15] Hang Z T. Industrial Catalysis. Beijing: Chemical Industry Press, 2006: 50

(黄仲涛. 工业催化. 北京: 化学工业出版社, 2006: 50)
文章导航

/

〈 〉