较低剪切速率下过冷熔体非枝晶组织的形成与演化

  • 赵力宁 ,
  • 林鑫 ,
  • 黄卫东
展开
  • 西北工业大学凝固技术国家重点实验室, 西安 710072
黄卫东

收稿日期: 2010-10-06

  修回日期: 2010-11-28

  网络出版日期: 2011-04-11

基金资助

国家自然科学基金项目50771083和凝固技术国家重点实验室自主研究课题项目02-TZ-2008资助

FORMATION AND EVOLUTION OF THE NON-DENDRITIC MORPHOLOGY IN UNDERCOOLING MELT WITH LOWER SHEARING RATE

  • DIAO Li-Ning ,
  • LIN Xin ,
  • HUANG Wei-Dong
Expand
  • State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072
HUANG Weidong

Received date: 2010-10-06

  Revised date: 2010-11-28

  Online published: 2011-04-11

Supported by

Supported by National Natural Science Foundation of China (No.50771083) and Fund of the State Key Laboratory of Solidification Processing (NWPU) (No.02-TZ-2008)

摘要

采用SCN-5H2O(摩尔分数, \%)透明模型合金研究了较低剪切速率范围内过冷合金熔体中晶体的生长与演化行为. 结果表明, 在较大过冷度下, 存在一个剪切速率阈值, 当熔体剪切速率高于阈值, 晶体能够以球状形态生长; 当剪切速率低于阈值, 晶体以枝晶形态生长. 在较低剪切速率下, 过冷度较大时, 球晶失稳后呈枝晶形态, 过冷度较小时, 球晶失稳后呈玫瑰晶形态. 球晶失稳形成玫瑰晶是由球晶界面扰动胞低速生长过程中尖端发生持续分叉所造成的.

本文引用格式

赵力宁 , 林鑫 , 黄卫东 . 较低剪切速率下过冷熔体非枝晶组织的形成与演化[J]. 金属学报, 2011 , 47(4) : 403 -409 . DOI: 10.3724/SP.J.1037.2010.00519

Abstract

With the development of the semisolid metal processing technology, many efforts have been made to understand the relationship of the microstructural evolution with the shear rate and the melt undercooling. The globular and rosette microstructures can be obtained under the different shearing rates and melt undercooling. Since the microstructure evolves rapidly under the general high shearing rate in the previous researches, it is difficult to reveal the formation process of semisolid microstructure in detail. In this work, the evolutions of globular and rosette crystals were studies by using a transparent organic alloy Succinonitrile-5%H2O (molar fraction) with a small shearing rate. It is found that there is a critical value of the shearing rate in the semisolid process above which the morphology of the globular crystal could be stable and below which it would be destabilized to form equiaxed dendrite. In addition, when the interface lost the stability, the globular crystals will evolve to dendrite under a higher melt undercooling and to rosette under a lower undercooling. The continuous splitting of the tip of the perturbation cells in the globular crystal induces the formation of the rosette morphology.

参考文献

[1] Spencer D B, Mehrabian R, Flemings M C. Metall Trans, 1972; 3A: 1925 [2] Flemings M C. Metall Trans, 1991; 22B: 957

[3] Vogel R A, Cantor B. J Cryst Growth, 1977; 37: 309

[4] Vogel A, Doherty R D, Cantor B. Proc Conf on Solidification and Casting of Metals, Sheffield, 1977, London: Metal Society, 1977: 518

[5] Vogel A. Met Sci, 1978; 12: 576

[6] Molenaar J M M, Salemans F W H C, Katgerman L. J Mater Sci, 1985; 20: 4335

[7] Doherty R D. Met Sci, 1982; 16: 1

[8] Mullis A M. Acta Mater, 1999; 47: 1783

[9] Ji S, Fan Z. Metall Mater Trans, 2002; 33A: 3511

[10] Li T, Huang W D, Lin X. Chin J Nonferrous Met, 2000; 10: 635

(李涛, 黄卫东, 林 鑫. 中国有色金属学报, 2000; 10: 635)

[11] Lin X, Li T, Huang W D. Solid State Phenom, 2006; 16–17: 155

[12] Li T, Lin X, Huang W D. Acta Mater, 2006; 54: 481

[13] Ji S, Fan Z, Bevis M J. Mater Sci Eng, 2001; A299: 210

[14] Martinez R A, Flemings M C. Metall Mater Trans, 2005; 36A: 2205

[15] Li T. PhD Thesis, Northwestern Polytechnical Universty, Xi’an, 2003

(李涛. 西北工业大学博士学位论文. 西安, 2003)

[16] Bian X F, Wang W M, Li H, Ma J J. The Melt Structure of Metal. Shanghai: ShangHai Jiao Tong University Press, 2003: 39

(边秀房, 王伟民, 李 辉, 马家骥. 金属熔体结构. 上海: 上海交通大学出版社, 2003: 39)

[17] Min N B. The Physical Fundamental of Crystal Growth. Shanghai: Shanghai Science and Technology Press, 1981: 226

(闵乃本. 晶体生长的物理基础. 上海: 上海科学技术出版社, 1981: 226)
文章导航

/

〈 〉