DZ125镍基高温合金高温持久断裂后的位错组态

  • 丁智 ,
  • 张军 ,
  • 王常帅 ,
  • 苏海军 ,
  • 刘林 ,
  • 傅恒志
展开
  • 西北工业大学凝固技术国家重点实验室, 西安 710072
丁 \ \ \ 智, 男, 1984年生, 硕士生

收稿日期: 2010-10-12

  修回日期: 2010-11-09

  网络出版日期: 2011-01-11

基金资助

国家自然科学基金项目50931004和50827102, 国家重点基础研究发展计划项目2010CB631202和2011CB610406及国家高技术研究发展计划项目2007AA03Z552资助

DISLOCATION CONFIGURATION IN DZ125 Ni-BASED SUPERALLOY AFTER HIGH TEMPERATURE STRESS RUPTURE

  • DING Zhi ,
  • ZHANG Jun ,
  • YU Chang-Shuai ,
  • SU Hai-Jun ,
  • LIU Lin ,
  • FU Heng-Zhi
Expand
  • State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072

Received date: 2010-10-12

  Revised date: 2010-11-09

  Online published: 2011-01-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50931004 and 50827102), National Basic Research Program of China (Nos.2010CB631202 and 2011CB610406), and National High Technology Research and Development Program of China (No.2007AA03Z552)

摘要

研究了熔体超温处理工艺对DZ125镍基高温合金铸态及热处理态高温持久试样位错组态的影响. 结果表明: 铸态试样的高温持久寿命随熔体超温处理温度的升高而增加. 热处理态试样的高温持久寿命随超温处理温度的升高表现为先增加后减少, 当超温处理温度为 1650℃时, 持久寿命达到最大值. 随熔体超温处理温度的升高, 铸态试样位错密度增大且位错多呈波浪形和不规则网络状分布, 热处理态试样中出现规则的多边形位错网, 有利于持久性能的提高. 位错网中位错的Burgers矢量为a/2<110>和 a<100>. 高温持久变形机制为位错的切割或攀移. 随超温处理温度的升高, 切入γ'相的位错数量减少, 并且有位错列和位错对列攀移通过γ'相.

本文引用格式

丁智 , 张军 , 王常帅 , 苏海军 , 刘林 , 傅恒志 . DZ125镍基高温合金高温持久断裂后的位错组态[J]. 金属学报, 2011 , 47(1) : 47 -52 . DOI: 10.3724/SP.J.1037.2010.00544

Abstract

The influence of the melt superheating treatment on the dislocation configuration in the as-cast and heat-treated samples of DZ125 Ni-based superalloy after high temperature stress rupture is studied. The results show that with the increase of the melt superheating temperature, the stress rupture life of the as-cast sample is increased and that of the heat-treated sample is first increased and then reduced. When the superheating temperature is 1650℃, the stress rupture life of the heat-treated sample reaches the maximum. With the increase of the melt superheating temperature, the dislocation density is increased and the waved or irregular dislocation networks appear in the as-cast sample, while the regular polygonal dislocation networks appear in the heat-treated sample, which is helpful to elevate the stress rupture property. The Burgers vectors of dislocations in the network are respectively a/2<110> and a<100>. The high temperature stress rupture deformation mechanism is mainly shearing and climbing of dislocation. It is demonstrated that there are few dislocations shearing the γ' phase and there are dislocation arrays or pairs climbing over the γ' phase.

参考文献

[1] Zhang J X, Wang J C, Harada H, Koizumi Y. Acta Mater, 2005; 53: 4623

[2] Shui L, Jin T, Tian S G, Hu Z Q. Mater Sci Eng, 2007; A454–455: 461

[3] Mayr C, Eggeler G, Dlouhy A. Mater Sci Eng, 1996; A207: 51

[4] Feller–Kniepmeier M, Link T. Mater Sci Eng, 1989; A113: 191

[5] Kolbe M, Dlouhy A, Eggeler G. Mater Sci Eng, 1997; A246: 133

[6] Probst–Hein M, Dlouhy A, Eggeler G. Acta Mater, 1999; 47: 2497

[7] Srinivasan R, Eggeler G F, Mills M J. Acta Mater, 2000; 48: 2497

[8] Zhang J X, Murakumo T, Koizumi Y. Harada H. J Mater Sci, 2003; 38: 4883

[9] ZouMM, Zhang J, Liu L, Fu H Z. Acta Metall Sin, 2008; 44: 59

(邹敏明, 张 军, 刘林, 傅恒志. 金属学报, 2008; 44: 59)

[10] Wang C S, Zhang J, Liu L, Fu H Z. J Alloys Compd, 2010; 508: 440

[11] Yin F S, Sun X F, Li Y B, Yu Y, Zheng Q, Guan H R, Hu Z Q. Acta Metall Sin, 2003; 39: 75

(殷凤仕, 孙晓峰, 李耀彪, 于洋, 郑启, 管恒荣, 胡壮麒. 金属学报, 2003; 39: 75)

[12] Tian S G, Zhou H H, Zhang J H, Yang H C, Xu Y B, Hu Z Q. Chin J Mater Res, 1999; 13: 632

(田素贵, 周惠华, 张静华, 杨洪才, 徐永波, 胡壮麒. 材料研究学报, 1999; 13: 632)

[13] Hong B D, Cui Y X. Material Electron Microscopy Analysis Technique. Harbin: Harbin Institute of Technology Press, 1990: 52

(洪班德, 崔约贤. 材料电子显微分析技术. 哈尔滨: 哈尔滨工业大学出版社, 1990: 52)

[14] Zhou L, Li S X, Wang Y C, Wang Z G. Acta Metall Sin, 2005; 44: 245

(周丽, 李守新, 王跃臣, 王中光. 金属学报, 2005; 415: 245)

[15] Liu L R, Jin T, Zhao N R, Wang Z H, Sun X F, Guan H R, Hu Z Q. Acta Metall Sin, 2004; 40: 858

(刘丽荣, 金涛, 赵乃仁, 王志辉, 孙晓峰, 管恒荣, 胡壮麒. 金属学报, 2004; 40: 858)

[16] Pollock T M, Argon A S. Acta Metall Mater, 1992; 40: 1

[17] Milligan W, Antolovich D. Metall Trans, 1991; 22: 2309

[18] Liu L R, Jin T, Zhao N R, Wang Z H, Sun X F, Guan H R, Hu Z Q. Acta Metall Sin, 2005; 44: 1215

(刘丽荣, 金 涛, 赵乃仁, 王志辉, 孙晓峰, 管恒荣, 胡壮麒. 金属学报, 2005; 41: 1215)

[19] Sarosi P M, Srinivasan R, Eggeler G F, Nathal M V, Mills M J. Acta Mater, 2007; 55: 2509

[20] Link T, Epishin A, Klaus M, Bruckner U, Reznicek A. Mater Sci Eng, 2005; A405: 254
文章导航

/

〈 〉