外应力对NiTi合金中共格Ni4Ti3沉淀相长大行为影响的相场法模拟

  • 柯常波 ,
  • 张新平 ,
  • 马骁
展开
  • 华南理工大学材料科学与工程学院, 广州 510640
柯常波, 男, 1981年生, 博士生

收稿日期: 2010-01-14

  修回日期: 2010-04-22

  网络出版日期: 2010-08-10

基金资助

国家自然科学基金项目50871039和50801029以及国家建设高水平大学公派研究生项目2008615024资助

PHASE FIELD SIMULATION OF THE EFFECT OF APPLIED EXTERNAL STRESS ON GROWTH KINETICS OF COHERENT Ni4Ti3 PRECIPITATE IN NiTi ALLOY

  • KE Chang-Bei ,
  • ZHANG Xin-Beng ,
  • MA Xiao
Expand
  • School of Materials Science and Engineering, South China University of Technology, Guangzhou 510640

Received date: 2010-01-14

  Revised date: 2010-04-22

  Online published: 2010-08-10

Supported by

Supported by National Natural Science Foundation of China (Nos. 50871039 and 50801029) and Chinese Government Graduate Student Overseas Study Program (No.2008615024)

摘要

运用相场模型模拟了外加应力对NiTi形状记忆合金中Ni4Ti3沉淀相组织形貌及长大行为的影响。无外加应力作用的时效过程中,4组Ni4Ti3变体均沿着各自对应的(111)B2惯习面从NiTi基体相中析出;而在<111>B2方向施加压应力时,则只有一组Ni4Ti3变体从NiTi基体相中析出,其惯习面法线方向平行于外加应力方向;单轴压应力作用下时效时, Ni4Ti3形核数量明显增加。外加单轴压应力可促进Ni4Ti3变体的形核和长大,但并不改变变体的面积分数、长度、宽度以及长度-宽度比等参数随时效时间变化的趋势;相同时刻,压应力增大使变体长度及宽度均略微增加,但均小于无应力作用下的情形;而相同时刻,变体的面积分数随外加应力的增大而增加。相场模拟结果与实验观察能较好地吻合。

本文引用格式

柯常波 , 张新平 , 马骁 . 外应力对NiTi合金中共格Ni4Ti3沉淀相长大行为影响的相场法模拟[J]. 金属学报, 2010 , 46(8) : 921 -929 . DOI: 10.3724/SP.J.1037.2010.00027

Abstract

The presence and distribution of Ni4Ti3 particles in NiTi alloys have a significant influence on martensitic phase transformation path by favoring the formation of R–phase rather than B19’ phase since the latter produces larger lattice deformation. To deeply understand the above, some experimental studies have been done by using differential scanning calorimetry (DSC) and in situ transmission electron microscopy (TEM). Meanwhile, some preliminary simulations have also been performed focusing on the morphology evolution of single and multiple Ni4Ti3 variants in single NiTi alloy system as well as considering the effect of external loads on selective precipitate growth. Whereas, in engineering application, the NiTi alloys often undergo the external load which may affect the growth kinetics of Ni4Ti3 precipitates. Therefore, it is necessary to investigate the effect of applied load on growth kinetics of Ni4Ti3 precipitates. In this paper, the phase field method has been extended to study the microstructure evolution and growth kinetics of Ni4Ti3 precipitates in NiTi alloys during zero–stress and stress–assisted aging. The simulation results show that during stress–free aging, four groups of the variants precipitate along the corresponding (111)B2 habit plane; when the NiTi matrix is under <111>B2 comprssive stress–assisted aging, there is only one group of the variants with the normal lines parallel to <111>B2 to be precipitated. Although the uniaxial compressive stress apparently promotes the nucleation and slightly accelerates the growth of Ni4Ti3 variants in each group, the trends of aging time dependences of the area fraction, variant length, variant width and length–width ratio seem unchanged. The larger stresses can cause length and width of the variant slightly larger, but the area fraction of the Ni4Ti3 particles increases with increasing stress level. The simulation results are in good coincidence with the experimental results available.

参考文献

[1] Allafi J K, Dlouhy A, Eggeler G. Acta Mater, 2002; 50: 4255 [2] Michutta J, Somsen C, Yawny A, Dlouhy A, Eggeler G. Acta Mater, 2006; 54: 3525 [3] Moore K T, Howe J M. Acta Mater, 2000; 48: 4083 [4] Bosze W P, Trivedi R. Metall Trans, 1974; 5: 511 [5] Enomoto M, Aaronson H I. Scr Metall, 1989; 23: 55 [6] Enomoto M, Hirth J P. Metall Mater Trans, 1996; 27A: 1491 [7] Ke C B, Ma X, Zhang X P. Acta Metall Sin, 2010; 46:84 (柯常波, 马骁, 张新平. 金属学报. 2010; 46:84) [8] Dlouhy A, Allafi J K, Eggeler G. Philos Mag, 2003; 83: 339 [9] Michutta J, Carrol M C, Yawny A, Somsen C, Neuking K, Eggeler G. Mater Sci Eng, 2004; A378: 152 [10] Li D Y, Chen L Q. Acta Mater, 1996; 45: 2435 [11] Li D Y, Chen L Q. Acta Mater, 1996; 45: 471 [12] Li D Y, Chen L Q. Acta Mater. 1997; 46: 639 [13] Khachaturyan A G. Theory of structural transformation in solid. New York: Wiley-Interscience, 1983: 213 [14] Wagner M F, Windl W. Acta Mater, 2008; 56: 6232 [15] Wagner M F, Windl W. Acta Mater, 2009; 60: 207 [16] Sharma S K, Macht M P, Naundorf V. Phys Rev, 1994; 49B: 6655 [17] Wang G, Xu D S, Ma N, Zhou N, Payton E J, Yang R, Mills M J, Wang Y. Acta Mater, 2009;57: 316 [18] Shen C, Chen Q, Wen Y H, Simmons J P, Wang Y. Scr Mater, 2004; 50: 1023 [19] Shen C, Chen Q, Wen Y H, Simmons J P, Wang Y. Scr Mater, 2004; 50: 1029 [20] Wang Y, Banerjee D, Su C C, Khachaturyan A G.. Acta Mater, 1998; 46: 2983 [21] Zhou N. PhD Thesis, The Ohio State University, 2008