论文

CBr4-C2Cl6共晶合金生长的三维多相场模拟
II.层片间距对形态演化的影响

  • 杨玉娟 ,
  • 严彪
展开
  • 同济大学材料科学与工程学院~上海市金属功能材料开发应用重点实验室, 上海 200092
杨玉娟, 女, 1981年生, 博士

收稿日期: 2010-02-19

  修回日期: 2010-05-10

  网络出版日期: 2010-07-11

基金资助

中国博士后科学基金项目20090460654, 上海市科委项目0752nm004和08DZ2201300资助

THREE DIMENSIONAL MULTI-PHASE FIELD SIMULATION OF GROWTH OF EUTECTIC CBr4-C2Cl6  ALLOY
II. Effect of Lamellar Spacing on Morphology Evolution

  • YANG Yu-Juan ,
  • YAN Biao
Expand
  • School of Materials Science and Engineering, Shanghai Key Lab of Development and Application for Metal Functional Materials, Tongji University, Shanghai 200092

Received date: 2010-02-19

  Revised date: 2010-05-10

  Online published: 2010-07-11

Supported by

Supported by China Postdoctoral Science Foundation (No.20090460654) and Shanghai Science and Technology Committee (Nos.0752nm004 and 08DZ2201300)

摘要

利用KKSO三维多相场模型, 在等层片宽度和厚度条件下, 研究了 CBr4-C2Cl6共晶合金在不同初始层片间距条件下的三维形态演化过程、层-棒转变及三维层片间距调整机制. 研究表明, 对于亚共晶、共晶成分的CBr4-C2Cl6合金, 不同的初始层片间距可能导致共晶形态发生层--棒转变, 且发生层--棒转变的趋势与初始层片间距的大小有关; 而过共晶成分的CBr4-C2Cl6合金不会发生层-棒转变, 维持层片生长. 而且当无量纲初始层片间距在0.598-2.336之间变化时, 随着层片间距的增加, 其演化顺序为: 层片湮没后形成 1λO→T-xλO→1λO→2λO→分叉与形核→Z字型分叉→无序组织. 研究还表明,三维层片间距调整机制与二维层片间距调整机制类似, 基本机制为层片湮没和层片分叉. 当初始层片间距较小时, 发生层片湮没现象. 而当初始层片间距较大时, 层片发生分叉. 但由于多了第三方向的限制作用, 三维层片间距调整机制比二维复杂.

本文引用格式

杨玉娟 , 严彪 . CBr4-C2Cl6共晶合金生长的三维多相场模拟
II.层片间距对形态演化的影响[J]. 金属学报, 2010
, 46(7) : 787 -793 . DOI: 10.3724/SP.J.1037.2010.00092

Abstract

Using KKSO multi-phase field model, with equal lamellar width and thickness, three dimensional (3D) morphology evolution, lamellar-rod transition and the mechanism of adjustment of lamellar spacing of CBr4-C2Cl6   alloys are investigated at different initial lamellar spacings. It's found that, as for the hypoeutectic and eutectic CBr4-C2Cl6   alloy, different initial lamellar spacings may lead to lamellar-rod transition, which is related to the initial lamellar spacings. The CBr4-C2Cl6   hypereutectic lamellar alloy can't transit to rod-like eutectic, with the increase of the dimensionless initial lamellar spacings Λ in the range of 0.598-2.336, the sequence of morphology evolution is: lamellar merges to form 1λO→T-xλO→1λO→2λO→lamellar branching→zigzag bifurcation$\rightarrow$lamellar destabilizes to form the disordered pattern. The simulated results also showed that the mechanism of adjustment of lamellar spacing in 3D of the CBr4-C2Cl6   hypereutectic alloy is similar to that in two dimensions (2D), which is lamellar annihilation and branching on the whole, the lamellar annihilation takes place with a smaller initial lamellar spacing while the lamellar branching takes place with a bigger initial lamellar spacing. The adjustment mechanism of the lamellar spacing in 3D is more complex than that in 2D because of the additional effect of the third dimension.

参考文献

[1] Cochrane R F, Greer A L, Eckler K, Herlach D M. Mater Sci Eng, 1991; A133: 698
[2] Li J F, Zhou Y H. Acta Mater, 2005; 53: 2351
[3] Kurz W, Fisher D J. Fundamentals of Solidification. 4th Ed., Switzerland, Germany, UK and USA: Trans Tech Publication, 1998: 93
[4] Davis H S. Theory of Solidification. New York: Cambridge University Press, 2001: 255
[5] Huang W D, Shan B L, Zhou Y H. Acta Phy Sin, 1991; 40: 323
(黄卫东, 商宝禄, 周尧和. 物理学报, 1991; 40: 323)
[6] Langer J S. In: Souletie J, Vannimenus J, Stora R, eds., Chance and Matter: Les Houches, Session XLVI, 1986, Amsterdam: Elsevier Science Publisher B. V., 1987: 629
[7] Caginalp G, Fife P. Phys Rev, 1986; 33B: 7792
[8] Karma A, Rappel W J. Phys Rev, 1998; 57E: 4323
[9] Yang Y J, Yan B. Acta Metall Sin, 2010; 46: 781
(杨玉娟, 严彪. 金属学报, 2010; 46: 781)
[10] Yang Y J, Wang J C, Zhang Y X, Zhu Y C, Li J J, Yang G C. J Crys Growth, 2009; 311: 2496
[11] Hurle D T J, Jakeman E. J Crys Growth, 1968; 3–4: 574
[12] Jackson K A, Hunt J D. Trans Metall Soc of AIME, 1966; 236: 1129
[13] Liu S, Lee J H, Enlow D, Trivedi R. In: Rappaz M, Beckerman C, Trivedi R, eds., Proc Symposium Sponsored by the Solidification Committee of MPMD of TMS, Charlotte, North Carolina: TMS Publication, 2004: 257
[14] Yang Y J, Wang J C, Zhang Y X, Zhu Y C, Li J J, Yang G C. Metall Mater Trans, 2009; 40A: 1670
[15] Karma A, Sarkissian A. Metall Mater Trans, 1996; 27A: 635
[16] Datye V, Langer J S. Phys Rev, 1981; 24B: 4155
[17] Walker H, Liu S, Lee H J, Trivedi R. Metall Mater Trans, 2007; 38A: 1417

文章导航

/

〈 〉