论文

热处理温度对电刷镀Ni-P镀层组织的影响

  • 李志明 ,
  • 钱士强 ,
  • 王伟 ,
  • 刘继华
展开
  • 上海工程技术大学材料工程学院, 上海 201620
李志明, 男, 1986年生, 硕士生

收稿日期: 2010-02-11

  修回日期: 2010-04-28

  网络出版日期: 2010-07-11

基金资助

上海市科委纳米专项基金项目0852nm01400和上海市重点学科建设项目J51402资助

EFFECTS OF HEAT-TREAT TEMPERATURE ON MICROSTRUCTURE OF ELECTRO-BRUSH PLATING Ni-P COATINGS

  • LI Zhi-Meng ,
  • QIAN Shi-Jiang ,
  • YU Wei ,
  • LIU Ji-Hua
Expand
  • College of Material Engineering, Shanghai University of Engineering Science, Shanghai 201620

Received date: 2010-02-11

  Revised date: 2010-04-28

  Online published: 2010-07-11

Supported by

Supported by Special Project of Shanghai Nano--technology (No.0852nm01400) and Shanghai Leading Academic Discipline Project (No.J51402)

摘要

利用XRD研究了电刷镀Ni--P镀层经不同温度热处理后的组织结构. 研究表明, 镀态电刷镀Ni-P镀层呈非晶态; 热处理温度在350 ℃以上时, Ni, Ni3P形核生长; 热处理温度在500 ℃以上时, 镀层中有NiO生成. 镀层的结晶度与热处理温度呈典型的“S”形关系变化,晶化激活能为(237.9±10.46) kJ?mol-1. 随热处理温度升高, Ni的晶格常数先增大后减小;而Ni3P的晶格常数a随热处理温度上升而变小, 而c略微增大; Ni和Ni3P晶粒大小随热处理温度的上升均增大; Ni和Ni3P晶体长大的表观活化能分别为(66.85±3.15) kJ?mol-1和 (133.41±4.69) kJ?mol-1, 前者仅为后者的50%, 表明在热处理过程中Ni晶体有优先长大的趋势.

本文引用格式

李志明 , 钱士强 , 王伟 , 刘继华 . 热处理温度对电刷镀Ni-P镀层组织的影响[J]. 金属学报, 2010 , 46(7) : 867 -872 . DOI: 10.3724/SP.J.1037.2010.00086

Abstract

The effects of heat-treat temperature on the structural of electro-brush plating Ni-P coatings were investigated using X-ray diffraction (XRD) analysis. The results show that the eletro-brush plating Ni-P coating is mainly in amorphous state. When heat-treat temperature above 350 ℃, Ni and Ni3P crystal appear, NiO is generated as the heat-treat temperature is above 500 ℃. There is a typical S-shaped relationship between the crystallinity and heat-treat temperature. The activation energy of crystallization is (237.9±10.46) kJ±mol-1. As the heat-treat temperature rises, Ni crystal cell parameter a increases firstly and then decreases, Ni3P crystal cell parameter a decreases but $c$ has a little increase. The crystal size of both Ni and Ni3P has some increase with the rise of heat-treat temperature. The activation energies for the growth of Ni and Ni3P are (66.85$\pm$3.15) kJ?mol-1 and (133.41±4.69) kJ?mol-1, respectively, and the great disparity imply that Ni crystal has dynamic for preferred growth.\par

参考文献

[1] Lee H B, Wuu D S, Lee C Y, Lin C S. Tribol Int, 2010; 43: 235
[2] Raju M, Ananth M V, Vijayaraghavan L. J Alloys Compd, 2009; 475: 664
[3] Sharma R, Agarwala R C, Agarwala V. J Alloys Compd,2009; 467: 357
[4] Elansezhian R, Ramamoorthy B, Kesavan Nair P. Surf Coat Technol, 2008; 203: 709
[5] Xu J. Surf Coat Technol, 2003; 168: 156
[6] Wu B, Xu B, Zhang B, Lv Y. Surf Coat Technol, 2007; 201: 6933
[7] Kornosky R, Lindsay J H. Plat Surf Finish, 2006; 93: 24
[8] Hou K H, Jeng M C, Ger M D. J Alloys Compd, 2007; 437: 289
[9] Liu H Z, Hu W B, Gu M Y, Wu R J. J Inorg Mater, 2002; 17: 429
(刘河洲, 胡文彬, 顾明元, 吴人洁. 无机材料学报, 2002; 17: 429)
[10] Tan G T, Chen Z H. Acta Phys Sin, 2007; 56: 1702
(谈国太, 陈正豪. 物理学报, 2007; 56: 1702)
[11] Jiang C H, Cheng F X, Wu J S. Acta Metall Sin, 2005; 41: 487
(姜传海, 程凡雄, 吴建生. 金属学报, 2005; 41: 487)
[12] Hong B, Jiang C H, Wang X J, Wu J S. Acta Metall Sin, 2006; 42: 699
(洪 波, 姜传海, 王新建, 吴建生. 金属学报, 2006; 42: 699)
[13] Keong K G, Sha W, Malinov S. J Alloys Compd, 2002; 334: 192
[14] Lu K, Wang J T, Dong L. Acta Metall Sin, 1991; 27: B31
(卢 柯, 王景唐, 董 林. 金属学报, 1991; 27: B31)
[15] Liu Y H, Liu P A. X–ray diffraction analysis Principles and Applications. Beijing: Chemical Industry Press, 2003: 138
(刘粤惠, 刘平安. XRD分析原理与应用. 北京: 化学工业出版社, 2003: 138)
[16] Malek J. Thermochim Acta, 1995; 267: 61
[17] Henderson D W. J Non–Cryst Solids, 1979; 30: 301
[18] Sui M L. Acta Metall Sin, 1998; 34: 650
(隋曼龄. 金属学报, 1998; 34: 650)
[19] Feng D, Qiu D R. Metal Physics (Vol.1): Structure and Defect. Beijing: Science press, 1987: 221
(冯端, 邱第荣. 金属物理学(第一卷)--结构与缺陷. 北京: 科学出版社, 1987: 221)
[20] Jin Y, Sun X S, Xue Q. X–ray Diffraction Analysis. Beijing: National Defense Industry Press, 2008: 251
(晋 勇, 孙小松, 薛屺. XRD分析技术. 北京: 国防工业出版社, 2008: 251)
[21] Hu L H, Dai J, Liu W Q, Wang K J, Dai S Y. Acta Phys Sin, 2009; 58: 1115
(胡林华, 戴 俊, 刘伟庆, 王孔嘉, 戴松元. 物理学报, 2009; 58: 1115)

文章导航

/

〈 〉