论文

马氏体相变中应变自协调效应的三维相场研究

  • 满蛟 ,
  • 张骥华 ,
  • 戎咏华
展开
  • 上海交通大学材料科学与工程学院, 上海 200240
满蛟, 男, 1972年生, 博士生

收稿日期: 2010-01-27

  修回日期: 2010-04-13

  网络出版日期: 2010-07-11

基金资助

国家自然科学基金资助项目50871069

THREE-DIMENSIONAL PHASE FIELD STUDY ON STRAIN SELF-ACCOMMODATION IN MARTENSTIC TRANSFORMATION

  • MEN Jiao ,
  • ZHANG Ji-Hua ,
  • RONG Yong-Hua
Expand
  • School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240

Received date: 2010-01-27

  Revised date: 2010-04-13

  Online published: 2010-07-11

Supported by

Supported by National Natural Science Foundation of China (No.50871069)

摘要

本文通过三维相场模型, 模拟了孪晶结构马氏体的生长, 计算了马氏体生长过程中的能量变化. 结果表明, 在马氏体变体长大阶段, 随演变时间的延长, 对于2个变体马氏体组成的体系, 其总弹性应变能增加; 而对于3个马氏体变体组成的体系, 其总弹性应变能降低. 本文的相场模拟揭示了3个马氏体变体具有最佳的的应变自协调效应.

本文引用格式

满蛟 , 张骥华 , 戎咏华 . 马氏体相变中应变自协调效应的三维相场研究[J]. 金属学报, 2010 , 46(7) : 775 -780 . DOI: 10.3724/SP.J.1037.2010.00051

Abstract

The number of martensitic variants depends on the grain size and orientation of parent phase. Although the growth of polytwin structure with the combination of different martensitic variants was studied by in situ dynamic observation, the energy change during the growth of martensite cannot be revealed, and in turn the strain self-accommodation of martensitic transformation (MT) cannot be confirmed. Based on the recent study of the phase field model, describing proper martensitic transformation for a single-crystal system under a fully constrained boundary, a three-dimensional (3D) phase field simulation is performed to demonstrate the microstructure evolution of plolytwin structure in this paper, meanwhile, the energy change during the growth of martensite is calculated. The results indicate that during the growth of two martensitic variants the total strain energy increases with prolonging microstructural evolution time, however, the opposite change occurs during the growth of three martensite variants. The 3D phase field simulation reveals that the growth of three martensitic variants possesses the best strain self-accommodation effect.

参考文献

[1] Xu Z Y. Martensitic Transformation and Martensite. 2nd ed., Beijing: Science Press, 1999: 69
(徐祖耀. 马氏体与马氏体相变. 第二版. 北京: 科学出版社, 1999: 69)
[2] Xu Z Y, Jiang B H. Shape Memory Materials. Shanghai: Shanghai Jiao Tong University Press, 2000: 5
(徐祖耀, 江伯鸿. 形状记忆材料. 上海: 上海交通大学出版社, 2000: 5)
[3] Khachaturyan A G. Sov Phys Solid State, 1967; 8: 2163
[4] Khachaturyan A G, Shatalov G A. Sov Phys Solid State, 1969; 11: 118
[5] Khachaturyan A G. Theory of Structural Transformations in Solids. New York: John Wiley & Sons, 1983: 198
[6] Gunton J P, Miquel M S, Sahni P S. In Phase Transition and Critical Phenomena. New York: Academic Press, 1983: 267
[7] Wang Y, Khachaturyan A G. Acta Mater, 1997; 45: 759
[8] Artemev A, Jin Y M, Khachaturyan A G. Acta Mater, 2001; 49: 1165
[9] Man J, Zhang J H, Rong Y H. Appl Phys Lett, 2010; 96: 131904
[10] Shimizu K, Okumura Y, Kubo H. Trans JIM, 1982; 23: 53
[11] Bhattacharya K. Arch Rational Mech Anal, 1992; 120: 201
[12] Li D Y, Chen L Q. Acta Mater, 1998; 46: 639
[13] Wang Y U, Jin Y M, Khachaturyan A G. Acta Mater, 2004; 52: 1039
[14] Liu J, Zhang J X. Solid State Commu, 1996; 98: 539
[15] Fukuhara M, Yin F, Ohsawa Y, Takamori S. Mater Sci Eng, 2006; A442: 439
[16] Zhang J H, Rong Y H, Hsu T Y. Philos Mag, 2010; 90: 159

文章导航

/

〈 〉