P含量对Inconel 706合金凝固过程中(Laves+γ)共晶反应的影响
收稿日期: 2010-01-09
修回日期: 2010-04-07
网络出版日期: 2010-07-11
EFFECTS OF P CONTENT ON (LAVES+γ) EUTECTIC REACTION DURING INCONEL 706 ALLOY SOLIDIFICATION
Received date: 2010-01-09
Revised date: 2010-04-07
Online published: 2010-07-11
研究了P对Inconel 706合金元素偏析和铸态组织的影响. 结果表明, P在合金凝固过程中显著地偏聚于剩余液相中, 并促进Nb和Ti等元素的偏聚, 从而促进富Nb的Laves相和富Ti的η-Ni3Ti相析出; 含0.004%P(质量分数)的Inconel 706合金枝晶间析出细小的(Laves+γ)共晶和少量针状η-Ni3Ti相; P含量超过0.016%以后, 枝晶间析出块状Laves相, Laves相颗粒之间析出大量密集的η-Ni3Ti板条; 此外, P含量由0.004%升高至0.016%, Laves相的初熔温度由1170-1180℃之间下降至1160-1170℃之间. 分析认为, 高度富集于剩余液相中的P强烈阻碍γ相的析出, 因此, P含量增加使合金的终凝温度降低, 而且导致合金的凝固结束反应由(Laves+γ)共晶转化为先析出富P的Laves相再析出γ基体的离异共晶反应.
关键词: Inconel 706合金; P含量; 凝固组织; 偏析
信昕 , 孙文儒 , 杨洪才 , 张伟红 , 刘芳 , 胡壮麒 , 祁峰 , 黄爱华 . P含量对Inconel 706合金凝固过程中(Laves+γ)共晶反应的影响[J]. 金属学报, 2010 , 46(7) : 873 -878 . DOI: 10.3724/SP.J.1037.2010.00038
The effects of P on elemental segregation and as-cast microstructure in Inconel 706 alloy were investigated in this paper. The results showed that P was markedly enriched in residual liquid and enhanced the segregation of Nb and Ti, which promoted the precipitation of Nb-enriched Laves phase and Ti-enriched η-Ni3Ti phase. In the as-cast alloy doped with 0.004% P (mass fraction), fine (Laves+γ) eutectic and needle like $\eta$ phase were formed in interdendritic region. As the P dopant was higher than 0.016%, blocky Laves phase was formed and lath η particles were precipitated among Laves particles. Moreover, with P increasing from 0.004\% to 0.016%, the incipient melting-point was found to drop from 1170-1180 ℃ to 1160-1170 ℃. In high P-doped alloys, the enrichment of P in the residual liquid was believed to hinder the solidification of γ phase, as a result, the final solidification temperature was found to be decreased and the solidification was terminated by the solidification of γ phase prior to the formation of P-bearing Laves phase rather than forming the (Laves+γ) eutectic.
Key words: Inconel 706 alloy; P content; solidified microstructure; segregation
[1] Schilke P W, Pepe J J, Schwant R C. In: Loria E A ed., Superalloys 718,625,706 and Various Derivatives, Warrendale, PA: TMS–AIME, 1994: 1
[2] Schilke P W, Schwant R C. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS–AIME, 2001: 25
[3] Long Z D. Mater Rev, 1995; 5: 14
(龙正东. 材料导报, 1995; 5: 14)
[4] Hu Z Q, Sun W R, Guo S R, Lu D Z. Chin J Nonferrous Met, 2001; 11: 947
(胡壮麒, 孙文儒, 郭守仁, 卢德忠. 中国有色金属学报, 2001; 11: 947)
[5] Sun WR, Guo S R, Guo J T, Lu D Z, Hu Z Q. Acta Metall Sin, 1995; 31: 346
(孙文儒, 郭守仁, 郭建亭, 卢德忠, 胡壮麒. 金属学报, 1995; 31: 346)
[6] Sun WR, Guo S R, Lee J H, Park P K, Yoo Y S, choe S J, Hu Z Q. Mater Sci Eng, 1998; A247: 173
[7] Cao W D, Kennedy R L. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS–AIME, 1994: 463
[8] Song H W. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 1999
(宋洪伟. 中国科学院金属研究所博士论文, 沈阳, 1999)
[9] Huang L F. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2007
(黄历锋. 中国科学院金属研究所博士论文, 沈阳, 2007)
[10] Yang S L. PhD Thesis, Northeastern University, Shenyang, 2006
(杨树林. 东北大学博士论文, 沈阳, 2006)
[11] Yang S L, Sun W R, Wang J X, Wang K L, Guo S R, Hu Z Q. Acta Metall Sin, 2009; 45: 815
(杨树林, 孙文儒, 王健熙, 王克亮, 郭守仁, 胡壮麒. 金属学报, 2009; 45: 815)
[12] Fesland J P, Petit P. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS– AIME, 1994: 229
[13] Meng X N, Sun W R, Guo S R, Lu D Z, Li N. Acta Metall Sin, 2004; 40: 613
(孟晓娜, 孙文儒, 郭守仁, 卢德忠, 李 娜. 金属学报, 2004; 40: 613)
[14] Chen C, Thompson R G, Davis S W. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS–AIME, 1991: 81
/
| 〈 |
|
〉 |