论文

晶粒尺寸和内应变不同的2种Fe粉的微加工过程与电磁性能

  • 周静 ,
  • 王维 ,
  • 孙志刚 ,
  • 官建国
展开
  • 武汉理工大学材料复合新技术国家重点实验室, 武汉 430070
周静, 女, 1986年生, 硕士生

收稿日期: 2010-03-10

  修回日期: 2010-05-06

  网络出版日期: 2010-08-10

基金资助

国家高技术研究发展计划项目2006AA03A209和霍英东青年教师基金项目101049资助

THE MICRO–FABRICATING PROCESS AND ELECTROMAGNETIC PROPERTIES OF TWO KINDS OF Fe POWDERS WITH DIFFERENT GRAIN SIZES AND INTERNAL STRAINS

  • ZHOU Jing ,
  • YU Wei ,
  • XUN Zhi-Gang ,
  • GUAN Jian-Guo
Expand
  • State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology, Wuhan 430070

Received date: 2010-03-10

  Revised date: 2010-05-06

  Online published: 2010-08-10

Supported by

Supported by National High Technology Research and Development Program of China (No.2006AA03A209) and Young Teachers from Fok Ying Tung Education Foundation (No.101049)

摘要

对比研究了2种内应变水平和晶粒大小不同的Fe粉在微加工过程中的形貌演变和微波电磁性能的变化规律. 结果表明, 与羰基Fe粉相比, 表面粗糙度和内应变水平较大, 晶粒较小的自制Fe粉在形状控制剂的协助下, 经10 h的微加工就能得到大而薄的片状Fe粉; 延长微加工时间($t$)至12 h, 存在的高内应变使片状结构破碎, 宽度减小; 进一步延长至t=24 h, Fe粉继续变薄, 制备出宽厚比较大、宽度较小的片状Fe粉. 该片状Fe粉同时具有高的磁导率和较低的介电常数, 用其组成的环氧树脂基复合材料在体积分数为20%, 厚度为1.5 mm时反射率小于-10 dB的带宽为8.2 GHz, 最低反射率为-14.6 dB.

本文引用格式

周静 , 王维 , 孙志刚 , 官建国 . 晶粒尺寸和内应变不同的2种Fe粉的微加工过程与电磁性能[J]. 金属学报, 2010 , 46(8) : 967 -972 . DOI: 10.3724/SP.J.1037.2010.00117

Abstract

The micro–fabricating process and electromagnetic properties of two kinds of Fe powders with different grain sizes and internal strains were studied. The results show that the homemade Fe powders with smaller grain size, larger internal strain and surface roughness than the carbonyl Fe powders, evolve into big and thin Fe flakes by micro–fabricating for 10 h with the help of the process control agent (PCA). When micro–fabrication for t=12 h, these Fe flakes will fracture and their average width will reduce due to strong internal strain. When t is further prolonged to 24 h, these Fe flakes become thinner, finally, those with larger aspect ratio and smaller width can be obtained, which show high permeability and low permittivity. The epoxy resin-based microwave absorbing materials containing such Fe flakes of 20% (volume fraction) exhibit a reflection loss less than −10 dB in the 9.4—17.9 GHz frequency range with a minimal peak of −14.6 dB, whose average thickness is 1.5 mm.

参考文献

[1] Walser R M, Win W, Valanju P M. IEEE Trans Magn, 1998; 34: 1390
[2] Deng L J, Zhou P H, Xie J L, Zhang L. J Appl Phys, 2007; 101: 103916
[3] Zhou P H, Deng L J, Xie J L, Liang D F. J Alloys Compd, 2008; 448: 303
[4] Xian W, Gong R Z, Li P G, Liu L Y, Cheng W M. Mater Sci Eng, 2007; 466A: 178
[5] Cho E K, Kwon H T, Cho E M, Song Y S, Sohn K Y, Park W W. Mater Sci Eng, 2007; A449–451: 368
[6] Zhang B S, Lu G, Feng Y, Xiong J, Lu H X. J Magn Magn Mater, 2006; 299: 205
[7] Moon B G, Sohn K Y, Park W W, Lee T D. Mater Sci Eng, 2007; A449–451: 426
[8] Huang J J. PhD Thesis, Lanzhou University, 2007
(黄娟娟. 兰州大学博士学位论文, 2007)
[9] Zhang X N. PhD Thesis, Beijing Institute of Technology, 2003
(张晓宁. 北京工业大学博士学位论文, 2003)
[10] Nie Y, He H H, Zhao Z S, Gong R Z, Yu H B. J Magn Magn Mater, 2006; 306: 125
[11] Dong D M, Guan J G,WangW, LiW, Zhou J. Acta Metall Sin, 2009; 45: 1141
(董德明, 官建国, 王维, 李维, 周静. 金属学报, 2009; 45: 1141)
[12] Wang Q, Guan J G, Liu S Q,Wang W, Zhang Q J. J Alloy Compd, 2006; 413: 155
[13] Tong G X,Wang W, Guan J G, Zhang Q J. J Inorg Mater, 2006; 21: 1461
(童国秀, 王维, 官建国, 张清杰. 无机材料学报, 2006; 21: 1461)
[14] Fan X A, Guan J G, Li Z Z, Mou F Z, Tong G X, Wang W. J Mater Chem, 2010; 20: 1676
[15] Pan J S, Tong J M, Tian M B. Material Science. 6th ed, Beijing: Tsinghua University Press, 1998: 205
(潘金生, 仝健民, 田民波. 材料科学基础. 第6版, 北京: 清华大学出版社, 1998: 205)
[16] Chen Z H, Chen D. Mechanical Alloying and Solid–Liquid Reaction Milling. 4th ed, Beijing: Chemical Industry Press, 2006: 58
(陈振华, 陈鼎. 机械合金化与固液反应球磨. 第4版, 北京: 化学工业出版社, 2006: 58)
[17] Fan X A, Guan J G, Wang W, Tong G X. J Phys, 2009; 42D: 075006