1500 MPa级低合金超高强钢的微观组织与力学性能
收稿日期: 2009-12-23
修回日期: 2010-03-19
网络出版日期: 2010-06-11
基金资助
“十一五”国家科技支撑计划资助项目2006BAE03A06
MICROSTRUCTURE AND MECHANICAL PROPERTIES OF 1500 MPa GRADE ULTRA–HIGH STRENGTH LOW ALLOY STEEL
Received date: 2009-12-23
Revised date: 2010-03-19
Online published: 2010-06-11
Supported by
Supported by Project of Scientific and Technical Supporting Program of China during the 11th Five–Year Plan (No.2006BAE03A06)
设计了一种新型1500 MPa级Si-Mn-Cr-Ni-Mo多组元系低合金超高强度结构钢, 对比研究了控轧+控冷(TMCP)、控轧+空冷、控轧+直接淬火、控轧+直接淬火+250 ℃回火4种不同工艺对其微观组织和力学性能的影响. 结果表明: 直接淬火态钢板抗拉强度最高, 可达1890 MPa, 屈服强度为1280 MPa, 延伸率为13\%; 250 ℃回火30 min后抗拉强度降低为1820 MPa, 而屈服强度升高为1350 MPa, 分析认为这归因于位错亚结构的回复软化过程与残余奥氏体分解为马氏体、析出ε-碳化物强化机制的综合作用; 空冷与TMCP工艺获得板条贝氏体+马氏体+少量残余奥氏体的复相组织, 贝氏体分割马氏体板条束, 使实验钢具有良好的强塑性. 低碳马氏体相变过程存在C扩散现象. 研究发现, 回火过程不仅包含残余奥氏体分解, 也包含C从马氏体或贝氏体向奥氏体的分配过程. 证明了立方结构的析出粒子在奥氏体中形核, 在整个冷却过程长大、粗化, 而相变后的马氏体或贝氏体未出现大量第二相析出核心.
王立军 , 武会宾 , 蔡庆伍 , 余伟 , 雷爱娣 . 1500 MPa级低合金超高强钢的微观组织与力学性能[J]. 金属学报, 2010 , 46(6) : 687 -694 . DOI: 10.3724/SP.J.1037.2009.00855
A novel sort of 1500 MPa grade ultra–high strength low alloy structural steel with multi–element of Si–Mn–Cr–Ni–Mo was designed. Effects of four different processes of TMCP (thermo–mechanical controlled processing), controlled rolling+air–cooled, controlled rolling + direct quenching and controlled rolling+direct quenching+tempering at 250℃ on the microstructure and mechanical properties were investigated. The results indicate that the directly quenched steel has a maximum tensile strength of 1890 MPa, yield strength of 1280 MPa and elongation of 13%. After tempered at 250 ℃ for 30 min, the tensile strength of the steel decreased to 1820 MPa, while the yield strength increased to 1350 MPa, which is ascribed to the comprehensive effect of the softening mechanism due to the recoverof dislocation sub–structure and the strengthening mechanism due to the decomposition of retained austenite and "–carbide precipitation. Duplex phase microstructure involving lath bainite, martensite segmented by bainite, and retained austenite was obtained by the process of air–cooling and TMCP, so that it has excellent strength and plasticity. Carbon diffusion phenomenon exists in the quenching process of low–carbon steel. Both the decomposition of retained austenite and the carbon partitioning into austenite from martensite or bainite were found during tempering process. The paper demonstrates that the precipitation particles of cubic structure nucleated in austenite, growing up and coarsning uring the whole cooling process. Futhermore, the emergence of a lage number of second–phasprecipitation cores was not found in martensite or bainite after phase tansformation.
[1] Fan C G, Dong H, Yong Q L, Weng Y Q, Wang M Q, Shi J, Hui W J. Mater Mech Eng, 2006; 30: 1
(范长刚, 董瀚, 雍岐龙, 翁宇庆, 王毛球, 时捷, 惠卫军. 机械工程材料, 2006; 30: 1)
[2] Guo J W, Sun J B, Li H B, Rong S F. J Jiamusi Univ, 2002; 20: 23
(郭继伟, 孙建波, 李洪波, 荣守范. 佳木斯大学学报, 2002; 20: 23)
[3] Garrison Jr W M, Maloney J L. Mater Sci Eng, 2005; A403: 299
[4] Maloney J L, Garrison Jr W M. Acta Mater, 2005; 53: 533
[5] Ji G L, Li F G, Li Q H, Li H Q, Li Z. Mater Sci Eng, 2010; A527: 1165
[6] Li J, Guo F, Li Z, Wang J L, Yan M G. J Iron Steel Res Int, 2007; 14: 254
[7] hang L C, Bhadesha H K D H. Mater Sci Eng, 1994; A184: 17
[8] Sule Y S, Kahraman S, Erdinc K. Mater Charact, 2008; 59: 351
[9] Zhirafar S, Rezaeian A, Pugha M. J Mater Process Technol, 2007; 186: 298
[10] Fang H S, Liu D Y, Chang K D, Zhang C, Gu J L, Zhang W Z, Bai B Z, Yang Z G. J Iron Steel Res, 2001; 13(3): 31
(方鸿生, 刘东雨, 常开地, 张驰, 顾家琳, 张文征, 白秉哲, 杨志刚. 钢铁研究学报, 2001; 13(3): 31)
[11] Liu D Y, Fang H S, Bai B Z. Trans Mater Heat Treat, 2002; 23(4): 5
(刘东雨, 方鸿生, 白秉哲. 材料热处理学报, 2002, 23(4): 57)
[12] Fan C G, Dong H, Shi J, Liu Y L, Yong Q L, Hui W J, Wang M Q, Weng Y Q. Ordnance Mater Sci Eng, 2006;29(2): 31
(范长刚, 董瀚, 时捷, 刘燕林, 雍歧龙, 惠卫军, 王毛球, 翁宇庆. 兵器材料科学与工程; 2006; 29(2): 31)
[13] Wang L D, Ding F C, Wang B M, Zhu M, Zhong Y L, Liang J K. Acta Metall Sin, 2009; 45: 292
(王六定, 丁富才, 王佰民, 朱明, 钟英良, 梁锦奎. 金属学报, 2009; 45: 292)
[14] Gao K, Wang L D, Zhu M, Chen J D, Shi Y J, Kang M K. Acta Metall Sin, 2007; 43: 315
(高宽, 王六定, 朱民, 陈景东, 施易军, 康沫狂. 金属学报, 2007; 43: 315)
[15] Jing C N, Wang Z C, Han F T. Met Heat Treat, 2005; 30: 26
(景财年, 王作成, 韩福涛. 金属热处理, 2005; 30: 26)
[16] Gregg J M, Bhadeshia H K D H. Acta Mater, 1997; 45: 739
[17] Xu Z Y. Shanghai Met, 1995; 171
(徐祖耀. 上海金属, 1995; 17: 1)
[18] Zhou Y, Wu G H.Analysis Methods in Materials Science. 2nd Ed., Harbin: Harbin Institute of Technology Press, 2007: 95
(周玉, 武高辉. 材料分析测试技术. 第二版, 哈尔滨: 哈尔滨工业大学出版社, 2007: 95)
[19] Xu Z Y. Martensitic Transformation and Martensite. 2nd Ed., Beijing: Science Press, 1999: 84
(徐祖耀. 马氏体相变与马氏体. 第二版, 北京: 科学出版社, 1999: 84)
[20] Yong Q L. Secondary Phases in Steels. Beijing: Metallurgy Industry Press, 2006: 225, 247
(雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 225, 247)
/
| 〈 |
|
〉 |