论文

超轻α固溶体基Mg-6Li-3Zn合金的位错蠕变

  • 曹富荣 ,
  • 崔建忠 ,
  • 李英龙 ,
  • 周舸 ,
  • 丁桦
展开
  • 1.东北大学材料与冶金学院; 沈阳 110819
    2.东北大学材料电磁过程教育部重点实验室; 沈阳 110819
曹富荣, 男, 1964年生, 副教授, 博士

收稿日期: 2009-09-07

  修回日期: 2010-02-06

  网络出版日期: 2010-06-11

基金资助

国家自然科学基金项目50774023和50974038, 国家高技术研究发展计划项目2007AA03Z111及中央高校基本科研业务费090502003资助

DISLOCATION CREEP IN SUPER–LIGHT α SOLID SOLUTION BASE Mg–6Li–3Zn ALLOY

  • CAO Fu-Rong ,
  • CUI Jian-Zhong ,
  • LI Yang-Long ,
  • ZHOU Ge ,
  • DING Hua
Expand
  • 1.College of Materials and Metallurgy; Northeastern University; Shenyang 110819
    2.Key Lab of Materials Electromagnetic Process; Ministry of Education; Northeastern University; Shenyang 110819

Received date: 2009-09-07

  Revised date: 2010-02-06

  Online published: 2010-06-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50774023 and 50974038), National High Technology Research and Development Program of China (No.2007AA03Z111) and China Central University Basic Research Transaction Expenses (No.090502003)

摘要

采用熔铸和大变形轧制制备了Mg-6Li-3Zn合金板材, 研究了合金的高温变形行为、显微组织、空洞与位错蠕变机制. 在623 K和1.67×10-3 s-1条件下获得了300%的最大延伸率. OM, TEM和SEM观察显示, 合金带状晶粒组织在573 K和1.67×10-3 s-1条件下发生显著的动态再结晶, 亚晶轮廓不清晰,位错分布比较均匀. 合金在573-623 K和1.67×10-3 s-1条件下断裂形式为韧性断裂. 获得了新型的位错黏性滑移与位错攀移转变蠕变机制图,表明Mg-6Li-3Zn合金带状晶粒组织在573 K和1.67×10-3 s-1条件下高温变形机制为晶格扩散控制的位错黏性滑移, 其应力指数为3(应变速率敏感性指数0.33), 变形激活能为134.8 kJ/mol, 与Mg的晶格扩散激活能相同.获得了新型的考虑聚合的空洞长大图, 合金在573 K和1.67×10-3 s-1条件下的空洞长大机制为塑性控制的空洞长大.

本文引用格式

曹富荣 , 崔建忠 , 李英龙 , 周舸 , 丁桦 . 超轻α固溶体基Mg-6Li-3Zn合金的位错蠕变[J]. 金属学报, 2010 , 46(6) : 715 -722 . DOI: 10.3724/SP.J.1037.2009.00582

Abstract

Mg–6Li–3Zn alloy was prepared by Jackson’s melting and casting method and the sheets of 1.2 mm in thickness processed by hot rolling at 573 K and cold rolling with a total reduction of more than 92% were obtained. The high–temperature mechanical behavior at temperatures ranging
from 423 to 673 K and initial strain rates ranging from 1.67×10−3 to 5×10−2 s−1 were investigated. The microstructure evolution, such as grains, subgrains, dislocations, cavities and fracture morphology, were investigated by OM, TEM and SEM. Yavari–Langdon model describing the transition between dislocatoviscous glide and dislocation climb was used to construct a new dislocatiocreep mechanism map which consists of Cottrell’s solute atmosphere breakaway dislocation climb regime, dislocation viscous glide regime and Cottrell’s solute atmosphere incorporated dislocation climb regime. A new cavity growth map considering cavity coalescence was obtained according to the cavity growth models. The maximum elongation to failure of 300% was demonstrated at 623 K and an initial strain rate of 1.67×10−3 s−1. Significant dynamic recrystallization occurred in band–like structure at 573 K and an initial strain rate of 1.67×10−3 s−1, the subgrain contour was ambiguous and dislocation distribution was relatively uniform. Fracture mode of the alloy at 573—623 K and an initial strain rate of 1.67×10−3 s−1 is ductile fracture. It is shown by the dislocation creep mechanism map that the high–temperature deformation mechaism in Mg–6Li–3Zn alloy sheet with bad–like structure at 573 K and an initial strain rate of .67×10−3 s−1 is dislocation viscous glide cotrolled by lattice diffusion, the stress exponent is 3 (strain rate sesitivity exponent 0.33) and deformation activation energy is 134.8 kJ/mol, which is the samas the lattice diffusion activation energy of Mg. The cavity growth mechanism of the alloy at 573 K and iitial strain rate of 1.67×10−3 s−1 is plasticity controlled cavity growth.

参考文献

[1] Counts W A, Friak M, Raabe D, Neugebauer J. Acta Mater, 2009; 57: 69
[2] Kim W J, Kim M J, Wang J Y. Mater Sci Eng, 2009; A516: 17
[3] Cao F R, Lei F, Cui J Z, Wen J L. Acta Metall Sin, 1999; 35: 770
(曹富荣, 雷方, 崔建忠, 温景林. 金属学报, 1999; 35: 770)
[4] Nayeb–Hashemi A A, Clark J B, Pelton A D. Bull Alloy Phase Diagram, 1984; 5: 365
[5] Raynor G V. The Physical Metallurgy of Magnesium and Its Alloys. London: Pergamon Press, 1959: 25
[6] Kassner M E, Perez–Prado M T. Prog Mater Sci, 2000; 45: 1
[7] Yavari P, Langdon T G. Acta Metall, 1982; 30: 2181
[8] Somekawa H, Hirai K, Watanabe H, Takigawa Y, Higashi K. Mater Sci Eng, 2005; A407: 53
[9] Li Y, Langdon T G. Acta Mater, 1998; 46: 1143
[10] Weinberg A F, Levinson D W, Rostoker W. Trans ASM, 1956; 48: 855
[11] Cao F R, Ding H, Li Y L, Zhou G, Cui J Z. Mater Sci Eng, 2010, A527: 2335
[12] Sherby O D, Wadsworth J. In: Krauss G ed., Deformation, Processing and Structure. Metals Park, Ohio: ASM, 1982: 355
[13] Hirai K, Somekawa H, Takigawa Y, Higashi K. Scr Mater, 2007; 56: 237
[14] King H W. J Mater Sci, 1966; 1: 79
[15] Murr L E. Interfacial Phenomena in Metals and Alloys. Mass: Addison Wesley, 1975: 55
[16] Koster W. Z Metallk, 1948; 39: 1
[17] Friedel J. Dislocations. Oxford: Pergamon Press, 1964: 202
[18] Wang J S, Nix W D. Acta Metall, 1986; 34: 545
[19] Fuentes–Samaniego R, Nix W D. Scr Metall, 1981; 15: 15
[20] Brown A W, Ashby M F. Acta Metall, 1980; 28: 1085
[21] Wolfenstine J, Gonzalez–Docel G, Sherby O D. J Mater Res, 1990; 5: 1359
[22] Ruano O A, Wadsworth J, Sherby O D. J Mater Sci, 1985; 20: 3735
[23] Pilling J, Ridley N. Superplasticity in Crystalline Solids. London: The Institute of Metals, 1989: 118
[24] Cao F R. PhD Thesis, Northeastern University, Shenyang, 1999
(曹富荣. 东北大学博士学位论文, 沈阳, 1999)
[25] Stowell M J, Livesey D W, Ridley N. Acta Metall, 1984; 32: 35
[26] Mukherjee A K. Mater Sci Eng, 1971; 8: 83
[27] Taleff E M, Ruano O A, Wolfenstine J, Sherby O D. J Mater Res, 1992; 7: 2131

文章导航

/

〈 〉