论文

基于马氏体区域化形成的免训练铸造Fe-Mn-Si-Cr-Ni形状记忆合金 II.退火对形状记忆效应的影响

  • 刘刚 ,
  • 彭华备 ,
  • 文玉华 ,
  • 杨坤 ,
  • 李宁
展开
  • 四川大学制造科学与工程学院; 成都 610065
刘刚, 男, 1986年, 硕士生

收稿日期: 2009-09-24

  修回日期: 2009-12-18

  网络出版日期: 2010-03-11

基金资助

国家自然科学基金项目50501015和50871072以及新世纪优秀人才支持计划项目NCET--06--0793资助

A TRAINING-FREE CAST Fe-Mn-Si-Cr-Ni SHAPE MEMORY ALLOY BASED ON FORMATION OF MARTENSITE IN A DOMAIN MANNER II. Influence of annealing on shape memory effect

  • LIU Gang ,
  • PENG Hua-Bei ,
  • WEN Yu-Hua ,
  • YANG Kun ,
  • LI Ning
Expand
  • College of Manufacturing Science and Engineering; Sichuan University; Chengdu 610065

Received date: 2009-09-24

  Revised date: 2009-12-18

  Online published: 2010-03-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50501015 and 50871072) and Program for New Century Excellent Talents in University (No.NCET-06-0793)

摘要

采用OM和铁素体测量仪研究了铸态Fe-18Mn-5.5Si-9.5Cr-4Ni合金的微观组织随退火温度的改变及其对合金形状记忆效应的影响. 结果表明, 在773-1173 K之间退火处理能进一步提高合金的形状记忆效应. 经973 K退火30 min后, 合金的可恢复变形量达到了6.4%, 比训练4次的常规 Fe-14Mn-5Si-8Cr-4Ni合金高1.2%. 当铸态合金在低于1173 K退火30 min后, δ铁素体仍为条状, 变形时能使应力诱发ε马氏体以区域化的方式形成, 合金具有良好的形状记忆效应; 当退火温度高于1273 K时, δ铁素体将固溶到奥氏体中, 体积分数减少. 当退火温度进一步升高到1423 K时, δ铁素体的体积分数显著增加, 形态由条状演变为岛状. 条状δ铁素体体积分数的减少和岛状δ铁素体的形成导致δ铁素体不能有效分割奥氏体晶粒, 合金的形状记忆效应显著下降.

本文引用格式

刘刚 , 彭华备 , 文玉华 , 杨坤 , 李宁 . 基于马氏体区域化形成的免训练铸造Fe-Mn-Si-Cr-Ni形状记忆合金 II.退火对形状记忆效应的影响[J]. 金属学报, 2010 , 46(3) : 288 -293 . DOI: 10.3724/SP.J.1037.2009.00644

Abstract

The microstructure and memory property evolutions of as-cast Fe-18Mn-5.5Si-9.5Cr-4Ni alloy with annealing temperature were investigated using OM, ferrite measuring instrument and bending method. The results showed that when the as-cast Fe-18Mn-5.5Si-9.5Cr-4Ni alloy was annealed between 773 and 1173 K, its shape memory effect (SME) was further improved. A high recovery strain of 6.4% was obtained only through annealing the as-cast alloy at 973 K for 30 min, which is 1.2% higher than that of the conventional Fe-14Mn-5Si-8Cr-4Ni alloy after four times thermo-mechanical training. When the as-cast Fe-18Mn-5.5Si-9.5Cr-4Ni alloy was annealed below 1173 K for 30 min, the morphology of δ ferrite phase was still lathy and it could make the stress-induced ε martensite form in a domain manner during deformation, which is the reason why the good SME was obtained in the as-cast alloy annealed below 1173 K for 30 min. When the annealing temperature was above 1273 K, the δ ferrite phase would dissolve in the austenite and its amount decreased. When the annealing temperature was further increased to 1423 K, the amount of δ ferrite phase remarkably increased and its morphology evolved into the island from the lath. The austenite grains could not be well subdivided into smaller domains due to the decrease of lathy δ ferrite phase or the formation of island δ ferrite phase. The SME of this as-cast alloy dramatically decreased when annealed above 1273 K.

参考文献

[1] Kubo H, Ostuka H, Farjami S, Maruyama T. Scr Mater, 2006; 55: 1059
[2] Li J C, Zhao M, Jiang Q. J Mater Eng Perform, 2002; 11: 313
[3] Zhao M, Li J C, Jiang Q. Mat–wissu Werkstofftech, 2003; 34: 756
[4] Peng H B, Liu G, Wen Y H, Sun P P, Li N. Acta Metall Sin, 2009; 46: 282
(彭华备, 刘刚, 文玉华, 孙盼盼, 李宁. 金属学报, 2009; 46: 282)

[5] Stanford N, Dunne D P. J Mater Sci, 2006; 41: 4883
[6] Bergeon N, Guenin G, Esnouf C. Mater Sci Eng, 1998; A242: 77
[7] Lippold J C, Kotecki D J. Welding Metallurgy and Weldability of Stainless Steel. Hoboken: John Wiley & Sons Inc, 2005: 13
[8] Sato A, Chishima E, Soma K, Mori T. Acta Metall Mater, 1982; 30: 1177
[9] Sato A, Chishima E, Soma K, Mori T. Acta Metall Mater, 1984; 32: 539
[10] Sato A, Yamaji Y, Mori T. Acta Metall Mater, 1986; 34: 287
[11] Kajiwara S. Mater Sci Eng, 1999; A273–275: 67
[12] Inagaki H. Z Metall, 1992; 83: 90
[13] Inagaki H. Z Metall, 1992; 83: 97
[14] Inagaki H. Z Metall, 1992; 83: 304
[15] Wen Y H, Zhang W, Li N, Peng H B, Xiong L R. Acta Mater, 2007; 55: 6526
[16] Wen Y H, Xiong L R, Li N, Zhang W. Mater Sci Eng, 2008; A474: 60

文章导航

/

〈 〉