论文

夹具拘束模型在焊接过程有限元分析中的建立及应用

  • 张增磊 ,
  • 史清宇 ,
  • 鄢东洋 ,
  • 蔡志鹏 ,
  • 李德成
展开
  • 1.清华大学机械工程系; 北京 100084
    2.中国运载火箭技术研究院首都航天机械公司; 北京 100076
张增磊, 男, 1985年生, 硕士

收稿日期: 2009-03-30

  修回日期: 2009-10-14

  网络出版日期: 2010-02-10

基金资助

国家高技术研究发展计划资助项目2006AA04Z139

ESTABLISHMENT AND APPLICATION OF FIXTURE CONSTRAINT MODELS IN FINITE ELEMENT ANALYSIS OF WELDING PROCESS

  • ZHANG Ceng-Lei ,
  • SHI Qing-Yu ,
  • YAN Dong-Xiang ,
  • SA Zhi-Peng ,
  • LI De-Cheng
Expand
  • 1.Department of Mechanical Engineering; Tsinghua University; Beijing 100084
    2.China Academy of Launch Vehicle Technology; Capital Aerospace Machinery Corporation; Beijing 100076

Received date: 2009-03-30

  Revised date: 2009-10-14

  Online published: 2010-02-10

Supported by

Supported by National High Technology Research and Development Program of China (No.2006AA04Z139)

摘要

夹具及垫板的拘束作用对被焊平板试样残余应力与变形的演变历程具有重要影响.将夹具和垫板作为弹塑性体包含到焊接数值 模拟模型中,采用4种模型模拟夹具及垫板与被焊平板试样之间的相互作用,能够提高焊接数值模拟研究方法的科学性和准确性. 数值 模拟结果表明,夹具拘束作用的不同处理方式对平板试样焊后残余应力分布与变形趋势有重要影响.不同拘束条件下的平板试样残余变 形模拟结果,与平板试样在自由状态下和夹具夹持状态下焊接实验获得的变形趋势均一致.在焊接过程初期阶段, 平板试样上下表面的横向 应力分布差异,对决定平板试样的残余变形趋势有重要影响.

本文引用格式

张增磊 , 史清宇 , 鄢东洋 , 蔡志鹏 , 李德成 . 夹具拘束模型在焊接过程有限元分析中的建立及应用[J]. 金属学报, 2010 , 46(2) : 189 -194 . DOI: 10.3724/SP.J.1037.2009.00198

Abstract

The mechanical interaction between welded panel and fixture has a remarkable influence on the distribution of weld–induced residual stress and distortion. Unfortunately, the influence of fixture is not generally included in conventional numerical simulations of welding process. In the present study, it is proposed that the numerical models in which the mechanical interaction between welded panel and fixture is considered as contact pair in the finite element analysis (FEA) of welding process. This could make the FEA of welding process more scientific and accurate. The fixture constraint plays an important role in accurate modeling of welding process. In the simulations, various mechanical constraint boundary conditions in welding process were thought about to establish the relationships of the normal and tangential mechanical interactions between welded panel and fixture. In Free model, the fixture restraint was not considered. In Mech model, the displacements of nodes where welded panel contacted with fixture were restricted in x, y, z directions. Hard model and Tabular model were contact models which included the fixture. In the normal direction, once welded panel and fixture were in contact, the transmitted contact pressure could be infinite in Hard model. While data pairs of contact pressure vs over–closure or clearance were specified to define a piecewise–linear relationship in the normal direction in Tabular model. A penalty friction coefficient of 0.3 was applied in tangential direction in both Hard and Tabular models. Fixture and welded panel were separated and the contact relationships were removed after the welding process in both Hard and Tabular models. The simulation results of contact models including fixture were more accurate, compared to models containing only welded panel with rigid retrictions. The distortiomode of welded panels under different fixture constrait conditions corresponded well with xperimental results. The differences between the distributions of transverse sresses on top and bottom surfaces f welded panel at the beginning of welding process had a crucial influence on the distortion mode f welded panel.

参考文献

[1] Dong P. Sci Technol Weld Joining, 2005; 10: 389
[2] Liu C, Zhang J X. Sci Technol Weld Joining, 2009; 14: 26
[3] Preston R V, Shercliff H R, WitherP J, Smith S. Acta Mater, 2004; 52: 4973
[4] Deng D, Murakawa H. Comput Mater Sci, 2008; 43: 591
[5] Li T, Shi Q Y, Li H K. Sci Technol Weld Joining, 2007; 12: 664
[6] Yang J G, Li J, Liu X S, Fang H Y. China Weld, 2008; 17: 39
[7] Tian X T. Weld Structure. Beijing: China Machine Press, 1995: 10
(田锡唐. 焊接结构. 北京: 机械工业出版社, 1995: 10)
[8] Preston R V, Shercliff H R, Withers P J, Smith S D. Sci Technol Weld Joining, 2003; 8: 10
[9] Schmidt H, Hattel J. Modell Simul Mater Sci Eng, 2005; 13: 77
[10] Abid M, Siddique M. Modell Simul Mater Sci Eng, 2005; 13: 919
[11] Zhang L, Silvanus J, Li H K, Shi Q Y. Sci Technol Weld Joining, 2008; 13: 422
[12] Zhang G D, Zhou C Y. Acta Metall Sin, 2008; 44: 848
(张国栋, 周昌玉. 金属学报, 2008; 44: 848)
[13] Yu S R, Fan D, Xiong J H. Trans Chin Weld Inst, 2008; 29: 25
(余淑荣, 樊 丁, 熊进辉. 焊接学报, 2008; 29: 25)
[14] Yan D Y, Si Q Y, Wu A P, Silvanus J, Liu Y, Zhang Z L. Acta Metall Sin, 2009; 45: 183
(鄢东洋, 史清宇, 吴爱萍, Silvanus J, 刘园, 张增磊. 金属学报, 2009; 45: 183)
[15] Nishikawa H, Serizawa H, Murakawa H. Sci Technol Weld Joining, 2007; 12: 147
[16] Zhang S L, Ren S Z. A Concise Handbook of Aluminum Alloy. 2nd Ed., Shanghai: Shanghai Scientific and Technological Literature Press, 2006: 9
(张士林, 任颂赞. 简明铝合金手册(第2版). 上海: 上海科学技术文献出版社, 2006: 9)
[17] Hibbitt, Karlsson & Sorensen, Inc.. ABAQUS/Standard User’s Manuals. Vol.3, Version 6.3, 2003: 120

文章导航

/

〈 〉