| 短纤维增强复合材料的仿生模型──Ⅲ.脆性基体复合材料中哑铃状纤维的强化作用 |
| 赵晓鹏;周本濂;罗春荣;刘建伟 |
| 中国科学院金属研究所;中国科学院国际材料物理中心;西北工业大学 |
|
| A BIOMIMETIC MODEL OF SHORT FIBRE REINFORCED COMPOSITE MATERIALS Ⅲ. Intensiting Effect of Dumbbell Fibre-Reinforced Composite with Brittle Matrix |
| ZHAO Hiaopeng; ZHOU Benlian(Institute of Metal Research; Chinese Academy of Sciences; International Centre for Materials Physics; Chinese Academy of Sciences; Shenyang 110015); LUO Chunrong; LIU Jianwei(Northwestern Polytechnical University; Xi'an 710072) (Manuscript received 1995-07-29; in revised form 1995-10-03) |
引用本文:
赵晓鹏;周本濂;罗春荣;刘建伟. 短纤维增强复合材料的仿生模型──Ⅲ.脆性基体复合材料中哑铃状纤维的强化作用[J]. 金属学报, 1996, 32(4): 438-442.
,
,
,
.
A BIOMIMETIC MODEL OF SHORT FIBRE REINFORCED COMPOSITE MATERIALS Ⅲ. Intensiting Effect of Dumbbell Fibre-Reinforced Composite with Brittle Matrix[J]. Acta Metall Sin, 1996, 32(4): 438-442.
| 1ReinhardtHW,NaamanAE.MaterStruct,1992;25:602田晓滨,赵晓鹏,周本濂.金属学报,1994;30:B1803赵晓鹏,田晓滨,周本濂,李世红.金属学报,1994;30:B1874李荫余.建筑材料与试验.南京:南京工学院出版社,1991:75NaamanAE,HomrichJR.ACIMaterJ,1989;86:2446贾贤,成会明,周本濂.见:’94秋季中国材料研讨会论文摘要集,中国材料研究学会,北京,1995:1353 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|