| 20MnMo钢内裂纹修复现象的发现及其金属组织的变化 |
| 韩静涛;赵钢;曹起骧 |
| 北京科技大学;中国人民解放军1202工厂;清华大学 |
|
| DISCOVERY OF INNER CRACK RECOVERY AND ITS STRUCTURE CHANGE IN 20MnMo STEEL |
| HAN Jingtao (University of Science and Technology Beijing; Beijing 100083);ZHAO Gang (The 1202 Factory of PLA; Beijing 100036); CAO Qixiang(Tsinghua University; Beijing 100084) (Manuscript received 1995-11-10; in revised form 1996-02-14) |
引用本文:
韩静涛;赵钢;曹起骧. 20MnMo钢内裂纹修复现象的发现及其金属组织的变化[J]. 金属学报, 1996, 32(7): 723-729.
,
,
.
DISCOVERY OF INNER CRACK RECOVERY AND ITS STRUCTURE CHANGE IN 20MnMo STEEL[J]. Acta Metall Sin, 1996, 32(7): 723-729.
| 1曹起骧,韩静涛,马庆贤,郑 涛,谢云灿,李福利.塑性工程学报,1994,1(1):142 ShapiroE,DieterGE.MetallTrans,1970,1:17113金宁.清华大学博士学位论文,1990 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|