铝合金钢盐浴硫氮碳共渗层中合金元素的分布及组织特征 |
宫秀敏;牛龙江;叶卫平;李兴红;朱凤璋 |
武汉汽车工业大学;武汉气门厂 |
|
MICROSTRUCTURE AND DISTRIBUTION OF ELEMENTS IN SALT BATH SULFONITRO-CARBURIZING LAYER OF AI-CONTAINING ALLOY STEELS |
GONG Hiumin; NIU Longjiang;YE Weiping; LI Hinghong (Wuhan Automotive Polytechnic University; Wuhan 430070); ZHU Fengzhang (Wuhan Valve Factory;Wuhan 430070)(Manuscript received 1995-09-26; in revised form 1996-03-25) |
引用本文:
宫秀敏;牛龙江;叶卫平;李兴红;朱凤璋. 铝合金钢盐浴硫氮碳共渗层中合金元素的分布及组织特征[J]. 金属学报, 1996, 32(8): 829-833.
,
,
,
,
.
MICROSTRUCTURE AND DISTRIBUTION OF ELEMENTS IN SALT BATH SULFONITRO-CARBURIZING LAYER OF AI-CONTAINING ALLOY STEELS[J]. Acta Metall Sin, 1996, 32(8): 829-833.
1AB著,田至敏译.钢与铸铁的硫碳氮共渗.北京:机械工业出版社,1982:712ThelningK-E.SteelandItsHeatTreatment.London:Butterworths,1975:3773著,郭铮匀译,钢的氮化,北京:国防工业出版社,1979:104胡以正.材料保护,1985;D(5):525宫秀敏.机械工程材料,1993;(10):166宫秀敏.热加工工艺,1994;(3):11" |
|