| 熔融Sn—S/ZnCl_2-NaCl体系界面脱硫反应动力学的阻抗分析 |
| 王淑兰;李光强;隋智通 |
| 东北大学材料与冶金学院;沈阳;110006;东北大学材料与冶金学院;沈阳;110006;东北大学材料与冶金学院;沈阳;110006 |
|
| THE IMPEDANCE ANALYSIS OF REACTION KINETICS AT THE INTERFACE OF MOLTEN Sn-S/ZnCl_2-NaCl SYSTEM |
| WANC Shulan; LI Guangqiang; SUI Zhitong (School of Materials and Metallurgy; Northeastern University; Shenyang 110006) |
引用本文:
王淑兰;李光强;隋智通. 熔融Sn—S/ZnCl_2-NaCl体系界面脱硫反应动力学的阻抗分析[J]. 金属学报, 1998, 34(5): 521-525.
,
,
.
THE IMPEDANCE ANALYSIS OF REACTION KINETICS AT THE INTERFACE OF MOLTEN Sn-S/ZnCl_2-NaCl SYSTEM[J]. Acta Metall Sin, 1998, 34(5): 521-525.
1蒋国昌,徐匡迪,邓健雄.金属学报,1990;26:B33(Jiang Guochang, Xu Kuangdi, Deng Jianxiong. Acta Metall Sin, 1990 26: B33) 2Xu C S, Tang X. ISIJ Int, 1992; 32: 1081 3焉毓璋,兰洪.金属学报,1991; 27:B224(Yan Yuzhang,Lan Hong.Acta Metall Sin,1991; 27:B224) 4 Ross Macdonald J.Applications of Impedance Spectroscopy Newyork:Wirey—Interscience Publication,1987 5Hino M, Nitta T, Chida S, Banya S Proc 3rd Int Conf on Molten Slags and Fluexs, London: The Inst Met,1988:286 6Gabrielli C.Identification of Electrochemical Processes by Frequency Response Analysis,Technical Report Number 004/83;Solartron Instrument,A Division of Schlumberger Electroniocs (UK)Ltd.1984;2:15 7小野阳一,石飞精助,铁钢,1977;60:1533(Ono YOichi, Ishitobi Seisuke.Tetsu Hagane;1974 60: 1533) 8 Khodov N V; Alfortsev V M, Danilin L A. Tszetnaya Metaplugiya,1987 4: 113 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|