Please wait a minute...
金属学报  2009, Vol. 45 Issue (3): 257-269    
  论文 本期目录 | 过刊浏览 |
关于洁净钢的若干基本问题
徐匡迪1;2
1 中国工程院; 北京 100088
2 上海大学; 上海 200072
CERTAIN BASIC SUBJECTS ON CLEAN STEEL
XU Kuangdi1;2
1 Chinese Academy of Engineering; Beijing 100088
2 Shanghai University; Shanghai 200072
引用本文:

徐匡迪. 关于洁净钢的若干基本问题[J]. 金属学报, 2009, 45(3): 257-269.
. CERTAIN BASIC SUBJECTS ON CLEAN STEEL[J]. Acta Metall Sin, 2009, 45(3): 257-269.

全文: PDF(2844 KB)  
摘要: 

洁净钢是针对客户提出的质量要求, 钢厂不断改进工艺、装备后, 逐步提高洁净度的各类钢. 介绍了典型钢种的洁净度要求及近半个世纪来商用钢中杂质能达到的最低水平. 钢中总氧量对钢的洁净度至关重要, 列举了国内外主要钢厂精炼、凝固过程中钢中总氧量的变化及降低总氧量的相关理论. 减少钢中夹杂物数量及控制其形态也是洁净钢的重要任务, 讨论了脱氧产物、脱氧剂再氧化及顶渣与耐火材料成分的影响, 对430系不锈钢中夹杂物控制及精炼时最佳搅拌强度作了介绍, 简述了钙处理使铝镇静钢夹杂物转形的基础理论. 对超低磷、超低硫钢生产的冶金原理作了重点阐述, 介绍了抗氢致开裂(HIC)的管线钢中超低硫和硫化物的形态控制. 对钢中其它杂质元素去除的可能途径也进行了讨论.

关键词 : 洁净钢,  洁净度,  总氧量,  夹杂物形态控制,  超低硫钢,  超低磷钢    
Abstract:

Clean steel is a general designation of certain types of steel with higher cleanness upgraded gradually by steel factories with promotion of process and equipment step by step according to the customer demands on product quality. The requirements for cleanness of typical steel and the possible lowest level of impurity in commercial steel since last half century were introduced. The total oxygen content in steel is extremely important for its cleanness. Relevant theories of changes and decreases of total oxygen content during refining and solidification processes used by major steel factories at home and abroad were enumerated. Decreasing the inclusion amount and controlling its shape are also key tasks for clean steel production. The influences of deoxidization products, re--oxidation of deoxidizer as well as top slag composition and refractory materials on the cleanness were mentioned separately, inclusion control in stainless steel series 430 and optimum stirring intensity in refining process were introduced, the theory foundation of inclusion transformation in aluminum--killed steel treated by calcium was briefly outlined, the metallurgical principles of ultra--low phosphorus steel and ultra--low sulphur steel productions were emphasized, ultra--low sulphur and sulphide shape control which are required by anti--HIC of linepipe steel was introduced, the possible ways of removing other impurities from steel were also discussed.

Key words: clean steel    cleanness    total oxygen content    inclusion shape control    ultra--low sulphur steel    ultra--low phosphorus steel
收稿日期: 2008-10-22     
ZTFLH: 

TG142

 
作者简介: 徐匡迪, 男, 1937年生, 教授, 中国工程院院士

[1] Kiessling R. Clean Steel (Special Report 77), London, The Iron and Steel Institute, 1962
[2] Burty M, Louis C, Dunand P, Osmont P, Meyer F R, Nadif M, Penet F, Isono T, Takeuchi E, Toh T. La Revue de M`etallurgie–CIT, 2000: 775
[3] Birat J P. Ironmaking Steelmaking, 2001; 28: 152
[4] Liu Z Z, Cai K K. Iron Steel, 2000; 35(2): 64
(刘中柱, 蔡开科. 钢铁, 2000; 35(2): 64)

[5] Xu K D. The Abstract Compile of 125th Xiangshan Conference Report, Beijing: 2000; 10: 31
(徐匡迪. 第125次香山科学会议报告摘要汇编, 北京, 2000; 10: 31)

[6] Turkdogan E T. Arch Eisenhˇuttennews, 1983; 54: 1
[7] Ito K. 165th–166th Nishiyama Memorial Seminar, Tokyo: ISIJ, 1997: 1
[8] Rein R H, Chipman J. Trans AIME, 1965; 233: 415
[9] Turkdogan E T. Ironmaking Steelmaking, 1985; 12: 64
[10] Kreutger H W. Stahl Eisen, 1972, 92: 766
[11] Zhang L F, Thomas B G. ISIJ Int, 2003; 43: 271
[12] Zhang L, Cai K. 84th Steelmaking Conf Proc, ISS, Warrandale, PA, 2001, 275
[13] Yoon B H, Heo K H, Kim J S, Sohn H S. Ironmaking Steelmaking, 2002; 29: 215
[14] Poirier J, Guiban M A, Blumenfeld Ph, Boher M, Bourrier Ph. La Revue de M`etallurgie–CIT, 2000: 1145
[15] Kim D S, Park J H, Park J H (POSCO), Lee S B, Lee H G. La Revue de M`etallurgie–CIT, 2004: 291
[16] Riboud P V, Gatellier C. Ironmaking Steelmaking, 1985; 12: 79
[17] Wrampelmeyer J C, Janke D. Proc 5th Int Iron Steel Congress, Washington D.C., 1986: 653
[18] Kn¨uppel H, Oeters F. Stahl Eisen, 1964; 81: 1347
[19] Engell H J, K¨ohler M, Fleischer H J, Thielmann R, Sch¨urmann E. Stahl Eisen, 1984; 104: 443
[20] Olette M, Gatellier C, Vasse R. Progress in Ladle Steel Refining Int Symp Physical Chemistry of Iron and Steelmaking. part 11, Toronto, 1982: 1
[21] Turdogan E T. Arch Eisenhˇuttnews, 1983; 53: 1
[22] Oeters F. Metallurgy of Steelmaking, 1994: 101
[23] Xu K D. Shanghai Met, 1986; 8(4): 1
(徐匡迪. 上海金属, 1986; 8(4): 1)

[24] Hu X C, Xu L P. Report of National Advanced Iron Materials Center for 2007, 2007
(胡晓春, 许珞萍. 2007国家先进钢铁材料中心报告, 2007)

[25] Cui J, Zheng Y Y, Zhu L X. Eng Sci, 2005; 7(6): 21
(崔健, 郑贻裕, 朱立新. 中国工程科学, 2005; 7(6): 21)

[26] Gu W B, Liu X, Yang B Q. Iron Steel, 2000; 35(3): 16
(顾文兵, 刘晓, 杨宝权. 钢铁, 2000; 35(3): 16)

[1] 王强, 王连钰, 李宏侠, 蒋佳伟, 朱晓伟, 郭占成, 赫冀成. 钢包出钢末期漩涡抑制机理探究及防漩设计[J]. 金属学报, 2018, 54(7): 959-968.
[2] 徐匡迪 肖丽俊 干勇 刘浏 王新华. 新一代洁净钢生产流程的理论解析[J]. 金属学报, 2012, 48(1): 1-10.
[3] 高翱 王强 李德军 柴海山 赵立佳 赫冀成. 电磁出钢系统中Fe-C合金的状态研究[J]. 金属学报, 2011, 47(2): 219-223.
[4] 高翱 王强 李德军 金百刚 王凯 赫冀成. 电磁引流技术的出钢效率及其影响因素[J]. 金属学报, 2010, 46(5): 634-640.