| X60管线钢在湿气和溶液介质中的H2S/CO2腐蚀行为 |
| 杨建炜;张雷;丁睿明;孙建波;路民旭 |
| 北京科技大学材料科学与工程学院 |
|
| H2S/CO2 CORROSION OF X60 PIPELINE STEEL IN WET GAS AND SOLUTION |
| YANG Jian Wei |
| 北京科技大学腐蚀与防护中心 |
引用本文:
杨建炜; 张雷; 丁睿明; 孙建波; 路民旭 . X60管线钢在湿气和溶液介质中的H2S/CO2腐蚀行为[J]. 金属学报, 2008, 44(11): 1366-1371 .
,
,
,
,
.
H2S/CO2 CORROSION OF X60 PIPELINE STEEL IN WET GAS AND SOLUTION[J]. Acta Metall Sin, 2008, 44(11): 1366-1371 .
[1]Vitse F,Alam K,Gunaltun Y,de Torreben D L,Duchet- Suchaux P.Corrosion 2002,NACE,Paper No.02245, 2002 [2]Chen C F,Lu M X,Zhao G X,Bai Z Q,Yah M L,Yang Y Q.Acta Metall Sin,2003;39:94 (陈长风,路民旭,赵国仙,白真权,严密林,杨延清.金属学报,2003;39:94) [3]Sun W,Nesic S,Papavinasam S.Corrosion 2006,NACE, Paper No.06644,2006 [4]Abayarathna D,Naraghi A,Wang S H.Corrosion 2005, NACE,Paper No.05624,2005 [5]Bai Z Q,Li H L,Liu D X,Wang X F.Mater Prot,2003; 36(4):32 (白真权,李鹤林,刘道新,王献昉.材料保护,2003:36(4):32) [6]Li G M,Liu L W,Zheng J S.J Chin Soc Corros Prot, 2000;20:204 (李国敏,刘烈伟,郑家燊.中国腐蚀与防护学报,2000;20:204) [7]Kvarekval J,Nyborg R,Choi H,Aramco S.Corrosion 2003,NACE,Paper No.03339,2003 [8]Bich N N.Corrosion 2006,NACE,Paper No.06642,2006 [9]Gunaltun Y M,Supriyataman D,Achmad J.Corrosion 1999,NACE,Paper No.36,1999 [10]Jiang F,Dai H Q,CaoX Y,Huang H B.Chem Eng Oil Gas,2005;34:213 (姜放,戴海黔,曹小燕,黄红兵.石油与天然气化工,2005;34:213) [11]Zhang Z,Hinkson D,Singer M,Wang H,Nesic S.Corro- sion 2007,NACE,Paper No.07556,2007 [12]Smith S N,Pacheco J L.Corrosion 2002,NACE,Paper No.02241,2002 [13]Pots B F M,John R C,Rippon I J,Thomas M J J S, Kapusta S D,Girgis M M,Whitham T.Corrosion 2002, NA CE,Paper No.02235,2002 [14]Agrawal A K,Durr C,Koch G H.Corrosion 2004,NACE, Paper No.04383,2004 [15]Wikjord A G,Rummery T E,Doern F E,Owen D G. Corros Sci,1980;20:651 [16]Murowchick,James B,Barnes H L.Am Mineral,1986;71: 1243 [17]Arnold R G.Economic Geology,1969;64:405 [18]Schoonen M A A,Barnes H L.Geochim Cosmochim Acta, 1991;55:1495 [19]Zhang Y,Zhao P.Steel Pipe,2003;32(4):10 (张毅,赵鹏.钢管,2003;32(4):10) [20]Hoffmeister H.Corrosion 2007,NACE,Paper No.07501, 2007 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|