| 复合型 LaNi5/Ni-S 合金镀层在碱液中的析氢反应 |
| 韩庆;陈建设;刘奎仁;魏绪钧 |
| 东北大学材料与冶金学院 |
|
| Hydrogen evolution reaction on the composite LaNi5/Ni-S alloy film in alkaline medium |
| ;;; |
| 东北大学 |
引用本文:
韩庆; 陈建设; 刘奎仁; 魏绪钧 . 复合型 LaNi5/Ni-S 合金镀层在碱液中的析氢反应[J]. 金属学报, 2008, 44(7): 887-891 .
,
,
,
.
Hydrogen evolution reaction on the composite LaNi5/Ni-S alloy film in alkaline medium[J]. Acta Metall Sin, 2008, 44(7): 887-891 .
[1]Norsk H.Netherlands Pat,7801955,1978 [2]Hine F,Yasuda M,Watanabe M.Denki Kagaku,1979;47: 401 (日根富郎,安田正雄,渡边正男.电气化学,1979;47:401) [3]Gonsalez E R,Avaca L A,Tremiliosi-Filho G.Int J Hy- drogen Energy,1994;19:17 [4]Sabela R,Paseka I.J Appl Electrochem,1990;20:500 [5]Paseka I.Electrochim Acta,1993;38:2449 [6]de Giz M J,Ferreira M,Gonzalez E R.J Appl Electrochem, 1993;23:641 [7]Vandenborre H,Vermeiren Ph,Leysen R.Electrochim Acta,1984;29:297 [8]Wen T C,Lin S M,Tsai J M.J Appl Electrochem,1994; 24:233 [9]Valand T,Burchardt T,Grontoft T.Int J Hydrogen En- ergy,2002;27:39 [10]Xu Y H,He G R,Wang X L.Int J Hydrogen Energy,2003; 28:961 [11]Kitamura T,Iwakura C,Tamura H.Chem Left,1981:965 [12]Kitamura T,Iwakura C,Tamura H.Chem Left,1981:1755 [13]Hu W K.Int J Hydrogen Energy,2000;25:111 [14]Bocutti R,Saeki M J,Florentino A O.Int J Hydrogen Energy,2000;25:1051 [15]Han Q,Liu K R,Chen J S.Int J Hydrogen Energy,2003; 28:1207 [16]Bard A J,Fauikner L R.Electrochemical Methods Fun- damentals and Applications.2nd Ed.,New York:John Wiley & Sons,INC,2003:135 [17]Carvalho J D,Tremiliosi-Filho G,Avaca L A.In:Srini- vasan S,Wagner S,Wroblowa H,eds.,Electrode Materials and Processes .for Energy Conversion and Storage.Pen- nington:The Electrochem Soc Inc,1987:356 [18]Vandenborre H,Vermeiren P,Leysen R.Electrochim Acta, 1984;29:297 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|