PZT铁电陶瓷力电耦合的三维相场模拟
刘苹莉;马星桥;褚武扬;乔利杰
THREE DIMENSIONS PHASE FIELD SIMULATION OF MECHATRONIC COUPLE FOR FERROELECTRIC MATERIALS
;;;
引用本文:

刘苹莉; 马星桥; 褚武扬; 乔利杰 . PZT铁电陶瓷力电耦合的三维相场模拟[J]. 金属学报, 2008, 44(8): 927-932 .
, , , . THREE DIMENSIONS PHASE FIELD SIMULATION OF MECHATRONIC COUPLE FOR FERROELECTRIC MATERIALS[J]. Acta Metall Sin, 2008, 44(8): 927-932 .

全文: PDF(4330 KB)  
摘要: 利用三维相场理论模拟了铁电材料的自发极化、电滞回线以及力电耦合对畴变的影响. 结果表明, 外场下的畴变是通过新畴形核及畴壁移动所引起的长大实现的. 逐渐改变外场时, 在矫顽场附近各类电畴均发生90°畴变, 从而导致极化强度突变. 沿垂直电场方向加 拉、压应变能阻止或促进沿电场方向的畴变.
关键词 : 铁电材料,  力电耦合,  三维相场模拟,  畴变    
Abstract:Using 3D-phase field theory, spontaneous polarization, hysteresis loop and mechatronic coupling of ferroelectric materials of have been simulated. The results show that the domain switching under applied electric field is carried out through initiating and growing of new domain and/or domain wall motion of the domains along the applied field. 90°domain switching of all kind of domains induces jump in the polarization near the coercive field. A tensile or compressive strain applied perpendicular to the electric field can hinder or promote domain switching.
Key words: ferroelectric materials    mechatronic coupling    3D phase field simulation    domain switching
收稿日期: 2008-03-14     
ZTFLH:  TG111.91  
[1]Yang W.Mechatronic Reliability.Heidelberg,Germany: Springer,2002:120
[2]Wang R M,Zhao X W,Chu W Y,Su Y J,Qiao L J.Mater Lett,2007;61:1162
[3]Wang F,Su Y J,He J Y,Qiao L J,Chu W Y.Scr Mater, 2006;54:603
[4]Wang R M,Chu W Y,Su Y J,Li J X,Qiao L J.Mater Sci Eng,2006:B135:141
[5]Zhao X W,Chu W Y,Su Y J,Li J X,Gao K W,Qiao L J.Acta Metall Sin,2006;42:13 (赵显武,褚武扬,宿彦京,李金许,高克玮,乔利杰.金属学报,2006;42:13)
[6]Huber J E,Fleck N A,Landis C M,McMeeking R.M.J Mech Phys Solids,1999;47:1663
[7]Hwang S C,Lynch C S,McMeeking R M.Acta Metall Mater,1995;43:2073
[8]Hwang S C,McMeeking R M.Int J Solids Struct,1999; 36:1541
[9]Wang J,Shi S Q,Chen L Q,Li Y L,Zhang T Y.Acta Mater,2004;52:749
[10]Wang J,Li Y L,Chen L Q,Zhang T Y.Acta Mater,2005; 53:2495
[11]Hu H L,Chen L Q.J Am Ceram Soc,1998;81:492
[12]Li Y L,Choudhury S,Liu Z K,Chen L Q.Appl Phys Lett, 2003;83:1608
[13]Loge R E,Suo Z.Acta Mater,1996;44:3429
[14]Huang H Y,Chu W Y,Su Y J,Li J X,Qiao L J.Appl Phys Lett,2006;89:142904
[1] 姜冰 郭志猛 邢献然. 外场作用下BaTiO3单晶裂纹扩展和畴变[J]. 金属学报, 2011, 47(5): 605-610.
[2] 满蛟 张骥华 戎咏华. 马氏体相变中应变自协调效应的三维相场研究[J]. 金属学报, 2010, 46(7): 775-780.
[3] 赵显武 褚武扬 乔利杰. 垂直电场下BaTiO3单晶的畴变与压痕裂纹的演化[J]. 金属学报, 2010, 46(3): 340-345.
[4] 赵显武 褚武扬 乔利杰. 恒位移下BaTiO3单晶在空气中亚临界裂纹扩展与畴变[J]. 金属学报, 2010, 46(2): 167-171.
[5] 姜冰; 白杨; 禇武扬; 乔利杰; 宿彦京 . 湿度对恒电场下BaTiO3单晶中畴变的影响[J]. 金属学报, 2008, 44(9): 1090-1094 .
[6] 钮萼 . 湿空气中恒磁场导致(Tb, Dy)Fe 2合金的滞后开裂[J]. 金属学报, 2006, 42(4): 369-373 .
[7] 张飒; 程璇; 张颖 . 铁电陶瓷畴变的原位Raman谱观测[J]. 金属学报, 2005, 41(6): 663-668 .
[8] 王瑞敏; 褚武扬; 宿彦京; 高克玮; 乔利杰 . 浸蚀促进BaTiO3单晶的畴变和裂纹扩展的研究[J]. 金属学报, 2005, 41(3): 297-301 .
[9] 陈志武; 程璇; 张颖 . Al--Li--Cu--Mg--Zr alloy, fatigue,[J]. 金属学报, 2004, 40(3): 230-234 .
[10] 张颖; 陈志武; 程璇; 张飒 . 原位XRD法研究电疲劳过程中铁电陶瓷PLZT的畴变[J]. 金属学报, 2004, 40(12): 1299-1304 .