| 非原位单芯MgB2/Fe带的织构和Jc的各向异性研究 |
| 索红莉 马红霞 王 颖 刘 敏 赵 跃 马 麟 周美玲 |
| 北京工业大学材料学院功能材料教育部重点实验室; 北京 100022 |
|
| Texture and Anisotropy of Jc of ex situ MgB2/Fe Mono—Filamentary Tapes |
| SUO Hongli; MA Hongxia; WANG Ying; LIU Min; ZHAO Yue; MA Lin; ZHOU Meiling |
| Key Laboratory of Advanced Functional Materials of Education Ministry; College of Materials Science and Engineering; Beijing University of Technology; Beijing 100022 |
引用本文:
索红莉; 马红霞; 王颖; 刘敏; 赵跃; 马麟 ; 周美玲 . 非原位单芯MgB2/Fe带的织构和Jc的各向异性研究[J]. 金属学报, 2006, 42(11): 1121-1124 .
,
,
,
,
,
,
.
Texture and Anisotropy of Jc of ex situ MgB2/Fe Mono—Filamentary Tapes[J]. Acta Metall Sin, 2006, 42(11): 1121-1124 .
[1] Nagamatzu J, Nakagawa N, Muranka T, Zenitanim Y, Akimitzu J. Nature, 2001; 410: 63 [2] Kovac P, Husek I, Grovenor C, Salter C. Supercond Sci Technol, 2003; 16: 292 [3] Kitaguchi H, Matzumoto A, Hatakeyama H. Supercond Sci Technol, 2004; 17: 486 [4] Yamamoto K, Osamura K, Balamurugan S, Nakamura T, Hoshino T, Muta I. Supercond Sci Technol, 2003; 16: 1052 [5] Suo H L, Beneduce C, Dhall M, Musolino N, Su X D, Flukiger R. Adv Cryog Eng, 2002; 48: 872 [6] Suo H L, Beneduce C, Dhall M, Musolino N, Genoud J Y, Flukiger R. Appl Phys Lett, 2001; 79: 3116 [7] Goldacker W, Schlachter S I, Obst B, Eisterer M. Supercond Sci Technol, 2004; 17: 490 [8] Feng Y, Yan G, Zhao Y, Liu C F, Liu X H, Zhang P X, Zhou L, Sulpice A, Mossang E, Hebral B J. Phys Condens Matter, 2004; 16: 1803 [9] Yamada H, Hirakawa M, Kumakura H, Matzumoto A. Appl Phys Lett, 2004; 84: 1728 [10] Flukiger R, Lezza P, Beneduce C, Musolino N, Suo H L. Supercond Sci Technol, 2003; 16: 264 [11] Grasso G, Malagoli A, Marre D, Bellingeri E, Braccini V, Roncallo S, Scati N, Siri A S. Physica, 2002; 378C: 899 [12] Flukiger R, Grasso G, Grivel J C, Marti F, Dhalle M, Huang Y. Supercond Sci Technol, 1997; 10: 68 [13] Young R A. The Rietveld Method. Oxford, UK: Oxford Univesity Press, 1993: 156 [14] Suo H L, Wang Y, Ma H X, Liu M, Zhao Y, Ma L, Li Y M, Zhang Z L, Zhou M L. Chin J Nonferrous Met, 2006; to be published (索红莉,王颖,马红霞,刘敏,赵跃,马麟,李亚明,张子立,周美玲,中国有色金属学报,2006,待发表) [15] Keijser T H, Langford J I, Mittemeier E J, Vogels B P. J Appl Cryst allogr, 1982; 15: 308 [16] Choi E M, Kim H J, Gupta S K, Chowdhury P, Kim K H, Lee S I, Kang W N. Phys Rev, 2004; 69B: 224 [17] Angst M, Puzniak R, Wisniewski A, Jun J, Kazakov S M, Karpinski J, Roos J, Keller H. Phys Rev Lett, 2002; 88: 16 [18] Flukiger R, Suo H L, Musolino N, Beneduce C, Toulemonde P, Lezza P. Physica, 2003; 385C: 286 [19] Senatore C. PhD Dissertation Dipartimento di Fisica, Universita degli studi di Salerno, Salerno, Italy, 2004: 167 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|