| Ni52Ga28Fe20-xCox合金的马氏体相变和磁性转变 |
| 罗丰华 陈嘉砚 及川胜男 石田清仁 |
| 中南大学粉末冶金国家重点实验室; 长沙 410083 |
|
| Martensitic Transformation and Magnetic Transition of Ni52Ga28Fe20-xCox Alloy |
| LUO Fenghua; CHEN Jiayan; OIKAWA Katsunari; ISHIDA Kiyohito |
| State Key Laboratory for Powder Metallurgy; Central South University; Changsha 410083 |
引用本文:
罗丰华; 陈嘉砚; 及川胜男; 石田清仁 . Ni52Ga28Fe20-xCox合金的马氏体相变和磁性转变[J]. 金属学报, 2006, 42(1): 93-98 .
,
,
,
.
Martensitic Transformation and Magnetic Transition of Ni52Ga28Fe20-xCox Alloy[J]. Acta Metall Sin, 2006, 42(1): 93-98 .
[1]Ullakko K,Huang J K,Kanter C,Kokorin V V,O'Handley R C.Appl Phys Lett,1996;69:1966 [2]Sozinov A,Likhachev A A,Lanska N,Ullakko K.Appl Phys Lett,2002;80:1746 [3]Vasil'ev A N,Buchel' nikov V D,Takagi T,Khovailo V V,Rstrin E I.Phys Uspekhi,2003;46:559 [4]Morito S,Kakeshita T,Hirata K,Otsuka K.Acta Mater,1998;46:5377 [5]James R D,Wuttig M.Philos Mag,1998;77A:1273 [6]Kakeshita T,Takeuchi T,Fukuda T,Saburi T,Oshima R,Muto S,Kishio K.Mater Trans JIM,2000;41:882 [7]Wuttig M,Li J,Craciunescu C.Scr Mater,2001;44:2393 [8]Oikawa K,Wulff L,Iijima T,Gejima F,Ohmori T,Fujita A,Fukamichi K,Kainuma R,Ishida K.Appl Phys Lett,2001;79:3290 [9]Oikawa K,Ota T,Ohmori T,Tanaka Y,Morito H,Fujita A,Kainuma R,Fukamichi K,Ishida K.Appl Phys Lett, ??2002;81:5201 [10]Sato M,Okazaki T,Furuya Y,Wuttig M.Mater Trans JIM,2003;44:372 [11]Morito H,Fujita A,Fukamichi K,Kainuma R,Ishida K.Appl Phys Lett,2002;81:1657 [12]Liang Y,Sutou Y,Wada T,Lee C,Taya M,Mori T.Scr Mater,2003;48:1415 [13]Oikawa K,Ota T,Sutou Y,Ohmori T,Kainuma R,Ishida K.Mater Trans JIM,2002;43:2360 [14]Omori T,Kamiya N,Sutou Y,Oikawa K,Kainuma R,Ishida K.Mater Sci Eng,2004;A378:403 [15]Sutou Y,Kamiya N,Kainuma R,Ishida K,Oikawa K.Appl Phys Lett,2004;84:1275 [16]Morito H,Fujita A,Fukamichi K,Ota T,Kainuma R,Ishida K,Oikawa K.Mater Trans JIM,2003;44:661 [17]Liu Z H,Zhang M,Cui Y T,Zhou Y Q,Wang W H,Wu G H,Zhang X X,Xiao G.Appl Phys Lett,2003;82:424 [18]Li J Q,Liu Z H,Yu H C,Zhang M,Zhou Y Q,Wu G H.Solid State Commun,2003;126:323 [19]Liu Z H,Hu H N,Liu G D,Cui Y T,Zhang M,Chen J L and Wu G H.Phys Rev,2004;69 B:134415 [20]Morito H,Fujita A,Fukamichi K,Kainuma R,Ishida K.Appl Phys Lett,2003;83:4993 [21]Oikawa K,Omori T,Kainuma R,Ishida K.J Magn Magn Mater,2004;272-276:2043 [22]Morito H,Oikawa K,Fujita A,Fukamichi K,Kainuma R,Ishida K,Takagi T.J Magn Magn Mater,2005;290-291:850 [23]Webster P J,Ziebeck K R A,Town S L,Peak M S.Philos Mag,1984;49B:295 [24]Wutting M,Liu L,Tsuchiya K,James R D.J Appl Phys,2000;87:4707 [25]Chernenko V A,Pons J,Cesari E,Zasimchuk I K.Scr Mater,2004;50:225 [26]Oikawa K,Imano Y,Chernenko V A,Luo F H,Omori T,Kainuma R,Ishida K.Submitted to Mater Trans JIMq |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|