| 工艺状态和应力水平对PD3钢轨钢接触疲劳寿命的影响 |
| 盛光敏 范镜泓 |
| 重庆大学材料科学与工程学院;重庆 400044 |
|
引用本文:
盛光敏; 范镜泓 . 工艺状态和应力水平对PD3钢轨钢接触疲劳寿命的影响[J]. 金属学报, 2000, 36(11): 1157-1160 .
[1] Liu Y. Iron Steel, 1986; 21(9): 67(刘怿,钢铁,1986;21(9):67) [2] Dikshit V A, Clayton P. Lubr Eng, 1992; 48: 606 [3] Johnson K L. Key Eng Mater 1989; 33: 17 [4] Clayton P, Hill D N. Wear 1987; 117: 319 [5] Vander Voort G F, Roose A. Metallography, 1984; 17(1):1 [6] Sheng G M, Fan J H, Peng X H. Iron Steel, 1999; 34(11):51(盛光敏,范镜泓,彭向和.钢铁,1999;34(11):51) [7] Sheng G M, Fan J H, Peng X H. Acta Metall Sin, 2000;36: 131(盛光敏,范镜泓,彭向和.金属学报,2000;36:131) [8] Grook A W. Ear Appl Mech, 1965; 12: 187. [9] Bower A F, Johnson K L. Wear, 1991; 144: 1) |
|