| Al-Ti-C系中TiC形成的热力学与动力学研究 |
| 张作贵 刘相法 |
| xfliu@dms.sdut.edu.cn |
|
引用本文:
张作贵; 刘相法 . Al-Ti-C系中TiC形成的热力学与动力学研究[J]. 金属学报, 2000, 36(10): 1025-1029 .
[1] Sun X D, Mei B C, Yuan R Z, Liao G S. Acta Metall Sin,1996; 32: 1102孙晓冬,梅炳初,袁润章,廖国胜.金属学报,1996;32:1102) [2] Cibula A. J lust Met, 1949-1950; 76: 321 [3] Baner n A, Reif W. Metall Tetall, 1985; 16A: 2065 [4] Baner n A, Reif W. Metall Metall, 1986; 17A: 2127 [5] Wage N, Frumin N, Levin L, Polak M, Dariel M P. MetallMater Trans, 1998; 29A: 1341 [6] Fine M E, Conley J G. Metall Trans, 1990; 21A: 2609 [7] Tong X C, Fang H S. Metall Mater Trans, 1998; 29A: 875 [8] Rapp R A, Zheng X. Metall Trans, 1991; 22A: 3071 [9] McCartney D G. Int Mater Rev, 1989; 34: 247 [10] Feng Q L, Wang C M. J Tsinghua Unly (Sci Technol ),1994; 34(5): 106(冯庆玲,王昶明清华大学学报(自然科学版),1994;34(5):106) [11] Wang C M, Feng Q L. Chin J Nonferrous Met, 1996; 6(1):130(王昶明,冯庆玲中国有色金属学报,1996;6(1):130) [12] Baner n A, Reif W. Solidification Processing 1987, Vol. 133,London: The institute of Metals, 1988: 145 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|