| 反向凝固条件下二元合金一维相变传热的研究 |
| 冯妍卉 王新华 |
| 北京科技大学热能工程系;北京 100083 |
|
引用本文:
冯妍卉; 王新华 . 反向凝固条件下二元合金一维相变传热的研究[J]. 金属学报, 2000, 36(4): 383-386 .
[1] Pleschiutschnigg F P, Hagen I V, Gammal T E I. StahlEisen, 1994; 114(2): 47 [2] Bennon W D, Incropera F P. Int J Heat Mass Transfer1987; 30: 2161 [3] Bennon W D, Incropera F P. Numer Heat Transfer 1988;13: 277 [4] Zhang Y Z, Ai L Q. Analytical Resolving and Mumerical Simulation of Ferrous Metallurgical Process, Beijing:Metallurgical Industry Press, 1997: 296(张玉柱,艾立群.钢铁冶金过程的数学解析与模拟.北京:冶金工业出版社,1997:296) [5] University of Science and Technology Beijing, Northeastern University. Report on Fundamental Investigation ofInverse Casting Technique job Producing Thin Steel Strip,Sponsored by National Natural Science Foundation ofChina, No.59634130, Beijing, 1999(北京科技大学,东北大学.国家自然科学基金重点项目“反向凝固法生产薄带技术基础研究”(59634130)1999年度报告,北京,1999)1 |
|