| γ’-Fe4N磁粉的超精细结构及结构转变 |
| 晁月盛 曾繁武 |
| 东北大学理学院; 沈阳110006 |
|
引用本文:
晁月盛; 曾繁武 . γ’-Fe4N磁粉的超精细结构及结构转变[J]. 金属学报, 2000, 36(3): 235-238 .
[1] Li Z R, Meng Q A, Cao Q J, Sun K, Wei Y N. Acta PhysSin, 1996; 45: 314 李子荣,孟庆安,曹琪娟,孙克,魏玉年.物理学报,1996;45:314) [2] Xue D S, Chen Z Y, Li F S. J Lanzhou Univ (Natural Sciences),1996; 32: 49 (薛德胜,陈子瑜,李发伸.兰州大学学报(自然科学版),1996;32:49) [3] Koyano T, Lee C H, Fukunaga T, Mizutani U. Mater SciForum, 1992; 88-90: 809 [4] Lee P Y, Chen T R, Chin T S. J Alloys Comp, 1995; 22: 179 [5] Shirane G, Takei W J, Ruby S L. Phys Rev, 1962; 126: 49 [6] Nozik A J, Wood J C, Haacke G. Sol State Commun, 1969;7: 1677 [7] Kim K J, Sumiyama K, Shibata K, Suzuki K. Mater Sci Eng,1994; A181: 1272 [8] Koyano T, Takizawa T, Fukunaga T, Mizutani U. Jpn J ApplPhys, 1993; 32: 1524 [9] Kim K J, Sumiyama K, Onodera H, Suzuki K. J AlloysComp, 1994; 203: 169) |
|