| Sn对Nd-Fe-B合金高温(423 K)磁后效和畴壁钉轧的影响 |
| 张正富 左铁镛 |
| 中国工业大学粉末冶金国家重点实验室; 长沙 410083 |
|
引用本文:
张正富; 左铁镛 . Sn对Nd-Fe-B合金高温(423 K)磁后效和畴壁钉轧的影响[J]. 金属学报, 2000, 36(2): 191-195 .
[1] Mylvaganam C K, Gaunt P. Philos Mag, 1981; B44(5): 581 [2] Givord D, Lienard A, Tenaud P. J Magn Magn Mater, 1987;67: L281 [3] Gonzalez J M. IEEE Trans Magn, 1996; 32(5): 1350 [4] Gaunt P. Philos Mag, 1979; B39(4): 313 [5] Gaunt P. Philos Mag, 1983; B48(3): 261 [6] Huang B Y. Trans Nonferrous Met Soc China, 2000; 10(2)(inpress)(黄伯云.中国有色金属学报,2000;10(2)已接收) [7] Schrey P. J Magn Magn Mater, 1991; 101: 417 [8] Raja M M, Narayanasamy A, Ravichandran V. J Magn MagnMater, 1996; 159: 345 [9] Wohlfarth E P. J Phys F: Met Phys, 1984; 14: L155 [10] Brown S D, Street R. J Appl Phys, 1996; 79(5): 2594 [11] Lyberatos A, Chantrell R W. J Phys: Condens Matter, 1997;9: 2623 [12] Taylor D W. J Magn Magn Mater, 1994; 130: 225 [13] Ram U S. J Magn Magn Mater, 1985; 50: 193 [14] Ramesh R, Thomas G. J Appl Phys, 1990; 67: 6968 |
|