| 电磁铸造大板坯不平直度形成机制的实验研究 |
| 郑贤淑 李朝霞 |
| 大连理工大学铸工程研究中心; 大连116024 |
|
引用本文:
郑贤淑; 李朝霞 . 电磁铸造大板坯不平直度形成机制的实验研究[J]. 金属学报, 2000, 36(2): 167-170 .
[1] Weaver C H. Light Met, TMS-AIME, Warrendale, PA, 1976:441 [2] Clark W, Larry Y. In: Rooy E L ed, Light Met, The Miner-als, Metals & Materials Societyl 1991: 953 [3] Drezet J M, Rappaz M, Carrupt B, Plata M. Metall Trans,1995; B26: 821 [4] Hallvard G, Fjaer, Asjorn M. Metall Trans, 1990; B21: 1049 [5] Krahebuhl Y, Kaenel R V, Carrupt B,Veber J C. In: Rooy EL ed, Light Met, The Minerals, Metals & Materials Society,1990: 893 [6] Drezet J M, Rappaz M. Metall Trans, 1996; A27: 3214 [7] Hu H Q. Solidification Principle of Metals. Beijing: Machin-ery Industry Press, 1991: 4(胡汉起,金属凝固原理.北京:机械工业出版社,1991:4) [8] Zheng X S, Jin J Z. Acta Metall Sin, 1995; B31(11): 511(郑贤淑,金俊泽.金属学报,1995;B31(11):511)9 |
|