| 孕育剂Ti, Zr对2219 Al--Cu合金焊缝组织及性能的影响 |
| 国旭明;杨成刚;钱百年;徐 强;张洪延 |
| 中国科学院金属研究所; 沈阳 110016 |
|
| Effects Of Inoculants Ti And Zr On The Microstructures And Properties Of 2219 Al--Cu Alloy Welds |
| GUO Xuming; YANG Chenggang; QIAN Bainian; XU Qiang; ZHANG Hongyan |
| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
国旭明; 杨成刚; 钱百年; 徐强; 张洪延 . 孕育剂Ti, Zr对2219 Al--Cu合金焊缝组织及性能的影响[J]. 金属学报, 2005, 41(4): 397-400 .
,
,
,
,
.
Effects Of Inoculants Ti And Zr On The Microstructures And Properties Of 2219 Al--Cu Alloy Welds[J]. Acta Metall Sin, 2005, 41(4): 397-400 .
[1]Chinese Welding Society. Welding Handbook (Vol 2). Beijing: China Machine Press, 2001: 520 (中国焊接学会编.焊接手册(第二卷).北京:机械工业出版社, 2001:520) [2]Janaki Ram G D, Mitra T K, Olson D L. Mater Sci Eng, 2000; 276A: 48 [3]Murty B S, Kori S A, Chakraborty M. Int Mater Rev, 2002; 47(1): 3 [4]Ganaha T, Pearce B P, Kerr H W. Metall Trans, 1980; 11A: 1351 [5]Mousavi M G, Cross C E, Grong (?). Sci Technol Weld Join, 1999; 4(6): 381 [6]Yunjia H, Frost R H, Olson D L, Edwards G R. Weld J, 1989; 68(7): 280s [7]Norman A F, Hyde K, Costello F, Thompson S, Birley S, Prangnell P B. Mater Sci Eng, 2003; A354: 188 [8]Guo X M, Yang C G, Qian B N, Chang Y L, Zhang H Y. Trans Chin Welding Inst, 2004; 25(4): 5 (国旭明,杨成刚,钱百年,常云龙,张洪延.焊接学报,2004; 25(4):5) [9]Yunjia H, Dalu G, Zhixiong S. Conference on Proceedings of the Aluminum-Lithium Ⅲ. 1986; 1215 [10]Reddy G M, Gokhale A A, Prasad K S, Prasad Rao K. Sci Technol Weld Join, 1998; 3(4): 208 [11]Kou S, Le Y. Weld J, 1986; 65(12): 305s [12]Dvornak M J, Frost R H, Olson D L. Weld J, 1989; 68(10): 327s |
|