| Ni基单晶高温合金CMSX-2树枝晶结构错配度变化的测算 |
| 彭志方 任遥遥 梅青松 刘艳 燕平 王延庆 |
| 武汉大学动力与机械工程学院;武汉 430072 |
|
引用本文:
彭志方; 任遥遥; 梅青松; 刘艳; 燕平; 王延庆 . Ni基单晶高温合金CMSX-2树枝晶结构错配度变化的测算[J]. 金属学报, 2001, 37(2): 171-178 .
[1] Peng Z F, Ren Y Y, Met Q S, Fan B Z, Yan P, Zhao J C,Wang Y Q, Sun J H. Acta Metall Sin, 1999; 35: 902(彭志方, 任遥遥, 梅青松, 樊宝珍, 燕平, 赵京晨, 王延庆,孙家华. 金属学报, 1999; 35: 902) [2] Peng Z F, Ren Y Y, Met Q S, Fan B Z, Yan P, Zhao J C,Wang Y Q, Sun J H. Scr Mater 2000; 42: 1959 [3] Glatzel U. Microstrvcture and Internal Strains of Undeformed and Creep Deformed Samples of a Nickel-BaseSoperalloy. Berlin: Verlag Dr Koster, 1994: 10 [4] Bruckner U, Epishin A, Link T, Dressel K. Mater Sci Eng,1998; 23-31: A247 [5] Bruckner U, Epishin A, Link T. Acta Mater 1997; 45:5223 [6] Volkl R, Glatzel U, Feller-Kniepmeier M. Acta Mater1998; 46: 4395 [7] Link T, Epishin A, Bruckner U. Scr Metall, 1998; 39: 1463 [8] Link T. Primate Communication, Dec, 1999 [9] Peng Z F, Glatzel U, Feller-Kniepmeier M. Acta MetallSin, 1995; 31: A531(彭志方, Glatzel U, Feller-Kniepmeier M. 金属学报, 1995;31: A531) [10] Pollock T M, Argon A S. Acta Metall Mater, 1994; 42:1859 [11] Caron P, Khan T. Mater Sci Eng, 1983; 61: 173 [12] Socrate S, Parks D M. Acta Metall Mater 1993; 41: 2185 [13] Lempke H, Wang Y Q, Mukherji D, Chen W Y, Wiedenmann A, Wahi R P. Z Metallkd, 1996; 87: 286 [14] Peng Z F, Ren Y Y, Fan B Z, Yan P, Zhao J C, Wang YQ, Sun J H. Acta Metall Sin, 1999; 35: 265(彭志方, 任遥遥, 樊宝珍, 燕平, 赵京晨, 王延庆 ,孙家华.金属学报, 1999; 35: 265) [15] Dreshfield R L, Wallace J F. Metall Trans, 1974; 5: 71 [16] Compiling Group of Metallographic Altlas for HighTemperature Alloys. Metallographic AHas for High-Temperature Alloys. Beijing: Metallurgical IndustryPress, 1975: 25(高温合金相图谱编写组. 高温合金金相图谱. 北京: 冶金工业出版社, 1975: 25) [17] Woo C S, Kim H T, Chun S S, Choi J. Scr Metall Mater,1993; 29: 1085 [18] Peng Z F, Ren Y Y, Liu Y, Zhang W. Acta Metall Sin,2001; 37, in press(彭志方, 任遥遥, 刘艳, 张伟. 金属学报. 2001; 37, 待发表) [19] Blavette D, Bostel A. Acta Metall, 1984; 32: 811 [20] Pollock T M, Argon A S. Acta Metall, 1992; 40: 1 [21] Watanabe R, Kuno T. J Iron Steel Inst Jpn, 1975; 61:2274(渡力藏, 九重常男. 铁钢, 1975; 61: 2274) [22] Ganghoffer J F, Hazotte A, Denis S, Simon A. Scr MetallMater, 1991; 25: 2491 [23] Fredholm A, Strudel J L. In: Gell M, Kortovich C S, Bricknell R H, Kent W B, Radovich J F eds, Superalloys 1984,AIME, Warrendale, PA, 1984: 211 [24] Nathal M V, Mackay R A, Garlick R G. Mater Sci Eng,1985; 75: 195 [25] Mishima Y, Ochiai S, Suzuki T. Acta Metall, 1985; 33:1161> |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|