| 新一代几何模型(周模型)与对称和非对称模型的应用比较 |
| 甄强 李文超 |
| 北京科技大学理化系; 北京 100083 |
|
引用本文:
甄强; 李文超 . 新一代几何模型(周模型)与对称和非对称模型的应用比较[J]. 金属学报, 1999, 35(7): 748-750 .
[1] Chou K C, Li W C, Li F S, He M H. CALPHAD, 1996 20: 395 [2]Hillert M CALPHAD, 1980 4:1 [3] Hillert M Be, Bunsenges Phys Chem, 1983; 87: 762 [4] Ridlich O, Kister AJ Ind Eng Chem, 1948; 40: 345 [5]Hultgren R, Desal P D, Hawkins D T, Gleiser M, Kelley K K Selected Values of the Thermodynamic Properties of Binary Alloys.Metals Park, Ohio: American Society for Metals, 1973:103 [6]Moser Z, Dutkiewicz J, Gasior W, Salawa J Bull Alloy Phase Diagrams,1985; 6:330 [7] Kamada K.Trans Jpn Inst Met, 1987; 28: 41 [8]Karlhuber S, Komarek K L, Mikula A Z Metallkd. 1994; 85: 307 |
|