| 熔体超温处理温度对新型镍基单晶高温合金溶质分配行为的影响* |
王海锋,苏海军,张军( ),黄太文,刘林,傅恒志 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| INFLUENCE OF MELT SUPERHEATING TREATMENT TEMPERATURE ON SOLUTE DISTRIBUTION BEHAVIOR OF A NEW Ni-BASED SINGLE CRYSTAL SUPERALLOYS |
Haifeng WANG,Haijun SU,Jun ZHANG( ),Taiwen HUANG,Lin LIU,Hengzhi FU |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China |
引用本文:
王海锋,苏海军,张军,黄太文,刘林,傅恒志. 熔体超温处理温度对新型镍基单晶高温合金溶质分配行为的影响*[J]. 金属学报, 2016, 52(4): 419-425.
Haifeng WANG,
Haijun SU,
Jun ZHANG,
Taiwen HUANG,
Lin LIU,
Hengzhi FU.
INFLUENCE OF MELT SUPERHEATING TREATMENT TEMPERATURE ON SOLUTE DISTRIBUTION BEHAVIOR OF A NEW Ni-BASED SINGLE CRYSTAL SUPERALLOYS[J]. Acta Metall Sin, 2016, 52(4): 419-425.
| [1] | Wollgramm P, Buck H, Neuking K, Parsa A B, Schuwalow S, Rogal J, Drautz R, Eggeler G.Mater Sci Eng, 2015; A628: 382 | | [2] | Wang X G, Liu J L, Jin T, Sun X F, Hu Z Q, Do J H, Choi B G, Kim I S, Jo C Y.Mater Des, 2015; 67: 544 | | [3] | Tian S G, Wang M G, Li T, Qian B J, Xie J.Mater Sci Eng, 2010; A527: 5445 | | [4] | Pollock T M, Murphy W H.Metall Mater Trans, 1996; 27A: 1088 | | [5] | Gui Z L.Aviation Product Eng, 1995; (4): 12 | | [5] | (桂忠楼. 航空制造工程, 1995; (4): 12) | | [6] | Stepanova N N, Roddionov D P, Turkham Y E, Sazonova V A, Khlystov E N.J Phys Met Metallogr, 2003; 95: 605 | | [7] | Tyagunov A G, Baryshev E E, Kostina T K, Semenova I P, Lesnikov V P.Met Sci Heat Treat, 1999; 41: 539 | | [8] | Galenko P K, Reutzel S, Herlach D M, Fries S G, Steinbach I, Apel M.Acta Mater, 2009; 57: 6172 | | [9] | Yin F S, Sun X F, Hou G C, Zheng Q, Guan H R, Hu Z Q.Rare Met Mater Eng, 2004; 33: 659 | | [9] | (殷凤仕, 孙晓峰, 侯贵臣, 郑启, 管恒荣, 胡壮麒. 稀有金属材料与工程, 2004; 33: 659) | | [10] | Zhang J, Li B, Zou M M, Wang C S, Liu L, Fu H Z.J Alloys Compd, 2009; 484: 755 | | [11] | Zou M M, Zhang J, Li B, Liu L, Fu H Z.Int J Mod Phys, 2009; 23B: 1107 | | [12] | Wang Z, Li J G, Zhao N R, Jin T, Zhang J H.Acta Metall Sin, 2002; 38: 922 | | [12] | (王震, 李金国, 赵乃仁, 金涛, 张静华. 金属学报, 2002; 38: 922) | | [13] | Wang C S, Zhang J, Liu L, Fu H Z.J Alloys Compd, 2010; 508: 443 | | [14] | Reed R C, Tao T, Warnken N.Acta Mater, 2009; 57: 5906 | | [15] | Mao X M, Fu H Z, Shi Z X, Liu H M.Acta Metall Sin, 1983; 19: A246 | | [15] | (毛协民, 傅恒志, 史正兴, 刘惠铭. 金属学报, 1983; 19: A246) | | [16] | Liu G, Liu L, Zhang S X, Yang C B, Zhang J, Fu H Z.Acta Metall Sin, 2012; 48: 847 | | [16] | (刘刚, 刘林, 张胜霞, 杨初斌, 张军, 傅恒志. 金属学报, 2012; 48: 847) | | [17] | Liu G, Liu L, Zhao X B, Ge B M, Zhang J, Fu H Z.Metall Mater Trans, 2011; 42A: 2736 | | [18] | Luo Y P, Zhou Y Z, Liu J L.Acta Metall Sin, 2014; 50: 1025 | | [18] | (罗银屏, 周亦胄, 刘金来. 金属学报, 2014; 50: 1025) | | [19] | Mushongera L T, Fleck M, Kundin J, Wang Y, Emmerich H.Acta Mater, 2015; 93: 66 | | [20] | Yu X X, Wang C Y, Zhang X N, Yan P, Zhang Z.J Alloys Compd, 2014; 582: 301 | | [21] | Ganesan M, Dye D, Lee P D.Metall Mater Trans, 2005; 36A: 2202 | | [22] | Frenkel J.Kinetic Theory of Liquids. New York: Dover Publication Inc, 1955: 93 | | [23] | Sidorov V E, Calvo-Dahlborg M, Dahlborg U, Popel P S, Chernoborodova S.J Mater Sci, 2000; 35: 2257 | | [24] | Yin F S, Guan H R, Sun X F, Hu Z Q.Acta Metall Sin, 2005; 41: 1192 | | [24] | (殷凤仕, 管恒荣, 孙晓峰, 胡壮麒. 金属学报, 2005; 41: 1192 ) | | [25] | Kolotukhin E V, Tjagunov G V.J Mater Process Technol, 1995; 53: 223 | | [26] | Brewer L.In: Walter J L, Jackson M R, Sims C T eds., Chemical Bonding Theory Applied to Metals in Alloying, Metals Park, OH: ASM International, 1988: 5 | | [27] | Murakami H, Saito Y, Harada H.In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Superalloys 1996, Champion, PA: TMS, 1996: 249 | | [28] | Ofori A, Rossouw C, Humphreys C.Acta Mater, 2005; 53: 97 | | [29] | Yin F S, Sun X F, Li J G, Guan H R, Hu Z Q.Mater Lett, 2003; 57: 3379 | | [30] | Xin T Z, Tang S, Ji F, Ning L K, Zheng Z.J Alloys Compd, 2015; 641: 229 | | [31] | Cai Y W.PhD Dissertation, Northwestern Polytechnical University, Xi'an, 1996 | | [31] | (蔡英文. 西北工业大学博士学位论文, 西安, 1996) | | [32] | Guo Y G, Li S M, Liu L, Fu H Z.Acta Metall Sin, 2008; 44: 367 | | [32] | (郭勇冠, 李双明, 刘林, 傅恒志. 金属学报, 2008; 44: 367) | | [33] | Stefanescu D M.Science and Engineering of Casting Solidification. 2nd Ed., New York: Springer Science+Business Media, LLC, 2009: 174 |
|
|