| N80钢CO2腐蚀电极过程交流阻抗分析 |
| 陈长风 路民旭 赵国仙 白真权 严密林 杨延清 |
| 中国石油天然气集团公司管材研究所;西安710065 |
|
引用本文:
陈长风; 路民旭; 赵国仙; 白真权; 严密林; 杨延清 . N80钢CO2腐蚀电极过程交流阻抗分析[J]. 金属学报, 2002, 38(7): 770-774 .
[1] Hong T, Jepson W P, Gopal M, Wang H B, Shi H. Cor-rosion/2000, Paper NO. 44, Houston: NACE, 2000 [2] Moraes F, John R, Shadley, Chen J F, Rybicki E F. Cor-rosion/2000, Paper NO. 30, Houston: NACE, 2000 [3] Jose R V, Rossana A, Intevep S A. Corrosion/1998, PaperNO. 23, Houston: NACE, 1998 [4] Zhang X Y, Yu G, Wang F P, Du Y L. Chem J Chin Univ.1999; 20: 1115(张学元,余刚,王凤平,杜元龙.高等学校化学学报,1999;20:1115) [5] Li J, Lu M X, Yan M L, Zhao G X, Sun D B, Yang D J.J Chin Soc Corros Protect, 1999; 19: 285(李静,路民旭,严密林,赵国仙,孙东柏,杨德.中国腐蚀与学报,1999;19:285) [6] Cao C N. Electrochim Acta, 1990; 35: 831 [7] Cao C N. Electrochim Acta, 1990; 35: 837 [8] Cao C N. J Chin Soc Corros Protect, 1993; 13: 91(曹楚南.中国腐蚀与防护学报,1993;13:91) [9] Dugstad A, Lunde L, Videm K. Corrosion/94, PaperNO.14, Houston: NACE,1994 [10] Chen C F, Zhao G X, Lu M X, Yang Y Q, Li H L. J Chin Soc Corros Protect. In press.(陈长风,赵国仙,路民旭,杨延清,李鹤林.中国腐蚀与防护学报,已接受) [11] Cao C N, Wang J, Lin H C. J Chin Soc Corros Protect.1989; 9: 261(曹楚南,王佳,林海潮.中国腐蚀与防护学报,1989;9:261) [12] Davies D H, Burstein G T. Corrosion. 1980; 36: 416S |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|