| FC Mold II电磁制动中磁场匹配对金属液流影响 |
| 贾皓, 张振强, 于湛, 邓康, 雷作胜, 任忠鸣 |
| 上海大学材料学院, 上海 200072 |
|
| INFLUENCE OF MAGNETIC FIELD INTENSITY MATCH OF FC MOLD II ON METAL FLOW |
| JIA Hao, ZHANG Zhenqiang, YU Zhan, DENG Kang, LEI Zuosheng, REN Zhongming |
| School of Materials, Shanghai University, Shanghai 200072 |
引用本文:
贾皓 张振强 于湛 邓康 雷作胜 任忠鸣. FC Mold II电磁制动中磁场匹配对金属液流影响[J]. 金属学报, 2012, 48(9): 1049-1056.
,
,
,
,
,
.
INFLUENCE OF MAGNETIC FIELD INTENSITY MATCH OF FC MOLD II ON METAL FLOW[J]. Acta Metall Sin, 2012, 48(9): 1049-1056.
| [1] Ttimmel K, Eckert S, Gerbeth G. Metall Mater Trans, 2011; 42B: 68[2] Cukierski K, Thomas B G. Metall Mater Trans, 2008; 39B: 94[3] Li B K, Tsukihashi F. ISIJ Int, 2006; 26: 1833[4] Yu Z, Zhang Z Q, Ren ZM, Lei Z S, Deng K. Acta Metall Sin, 2010; 46: 1275(于湛, 张振强, 任忠鸣, 雷作胜, 邓康. 金属学报, 2010; 46: 1275)[5] Harada H, Toh T, Ishii T, Kaneko K, Takeuchi E. ISIJ Int, 2001; 41: 1236[6] Hwang Y S, Cha P R, Nam H S, Moon K H, Yoon J K. ISIJ Int, 1997; 37: 659[7] Mao B. Contin Cast, 1999; 6: 37(毛斌. 连铸, 1999; 6: 37)[8] Thomas B G, Mika L J, Najjar F M. Metall Mater Trans, 1990; 21B: 387[9] Lei H, Xu G J, He J C. Chem Eng Technol, 2007; 30: 1650[10] Garcia–Hernandez S, Morales R D, Torres–Alonso E. Ironmaking Steelmaking, 2010; 37: 360[11] Zhong D Q, Yu L W. ISIJ Int, 2004; 44: 100[12] Choi S L, Ryu K J, Park H S. Met Mater Int, 2002; 8: 527[13] Wang Y F, Zhang L F. Metall Mater Trans, 2011; 42B: 1319[14] Chaudhary R, Thomas B G, Vanka S P. Metall Mater Trans, 2012; 43B: 532[15] Klaus T, Sven E, Gunter G. Metall Mater Trans, 2011; 42B: 68[16] Qian Z D, Wu Y L. ISIJ Int, 2004; 44: 100[17] Yu H Q, Wang B F, Li H Q, Li J C. J Mater Process Technol, 2008; 202: 179[18] Che Z H, Wang E G, Lei H, He J C. Iron Steel, 2008; 43(8): 25(陈芝会, 王恩刚, 雷洪, 赫冀成. 钢铁, 2008; 43(8): 25)[19] Li B K, Okane T, Umeda T. Metall Mater Trans, 2000; 31B: 1491[20] Timmel K, Eckert S, Gerbeth G, Stefani F, Wondrak T.ISIJ Int, 2010; 50: 1134[21] Wang M, Jia H, Zhang Z Q, Deng K. Shanghai Met, 2011; 33(6): 41(王 敏, 贾 皓, 张振强, 邓 康. 上海金属, 2011; 33(6): 41)[22] Jia H, Wang M , Zhang Z Q, Deng K, Lei Z S, Ren Z M. Shanghai Met, 2012; 34: 53(贾 皓, 王 敏, 张振强, 邓 康, 雷作胜, 任忠鸣. 上海金属, 2012; 34: 53)[23] Brito D, Nataf H C, Cardin P, Aubert J, Masson J P. Exp Fluids, 2001; 31: 653[24] Yu Z, Lei Z S, Jia H H, Jin X L, Ren Z M, Deng K, Zhong Y B. Shanghai Met, 2007; 29(2): 54(于湛, 雷作胜, 贾洪海, 金小礼, 任忠鸣, 邓康, 钟云波. 上海金属, 2007; 29(2): 54)[25] Wang Y, Zhang Z Q, Yu Z, Jia H, Deng K, Lei Z S, Ren Z M. Acta Metall Sin, 2011; 47: 1285(王寅, 张振强, 于 湛, 贾 皓, 邓 康, 雷作胜, 任忠鸣. 金属学报, 2011; 47: 1285) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|