| 定向凝固共晶生长的元胞自动机数值模拟 |
| 石玉峰, 许庆彦, 柳百成 |
| 清华大学机械工程系先进成形制造教育部重点实验室, 北京 100084 |
|
| SIMULATION OF EUTECTIC GROWTH IN DIRECTIONAL SOLIDIFICATION BY CELLULAR AUTOMATON METHOD |
| SHI Yufeng, XU Qingyan, LIU Baicheng |
| Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, Department of Mechanical Engineering, Tsinghua University, Beijing 100084 |
引用本文:
石玉峰 许庆彦 柳百成. 定向凝固共晶生长的元胞自动机数值模拟[J]. 金属学报, 2012, 48(1): 41-48.
,
,
.
SIMULATION OF EUTECTIC GROWTH IN DIRECTIONAL SOLIDIFICATION BY CELLULAR AUTOMATON METHOD[J]. Acta Metall Sin, 2012, 48(1): 41-48.
| [1] Aguiar M R, Caram R. J Cryst Growth, 1996; 166: 398[2] C¸adirli E, Kaya H, G¨und¨uz M. J Alloys Compd, 2007; 431: 171[3] Ginibre M, Akamatsu S, Faivre G. Phys Rev, 1997; 56E: 780[4] Datye V, Langer J S. Phys Rev, 1981; 24B: 4155[5] Meng G H, Lin X, Du L C, HuangWD. Acta Metall Sin, 2007; 43: 459(孟广慧, 林 鑫, 杜立成, 黄卫东. 金属学报, 2007; 43: 459)[6] Li J F, Zhou Y H. Sci China Ser E, 2005; 35: 449(李金富, 周尧和. 中国科学E辑, 2005; 35: 449)[7] Seetharaman V, Trivedi R. Metall Mater Trans, 1988; 19A: 2955[8] Jackson K A, Hunt J D. Trans Metall Soc AIME, 1966; 236: 1129[9] Series R W, Hunt J D, Jackson K. J Cryst Growth, 1977; 40: 221[10] Donaghey L F, Tiller W A. Mater Sci Eng, 1968; 3: 231[11] Magnin P, Trivedi R. Acta Metall Mater, 1991; 39: 453[12] Liu J, Elliott R. Acta Metall Mater, 1995; 43: 3301[13] Steinbach I, Pezzolla F. Physica, 1999; 134D: 385[14] Karma A. Phys Rev, 1994; 49E: 2245[15] Kim S G, Kim W T, Suzuki T, Ode M. J Cryst Growth, 2004; 261: 135[16] Yang Y J, Wang J C, Zhang Y X, Zhu Y C, Li J J, Yang G C. Metall Mater Trans, 2009; 40A: 1670[17] Yang Y J, Yan B. Acta Metall Sin, 2010; 46: 781(杨玉娟, 严彪. 金属学报, 2010; 46: 781)[18] Yang Y J, Yan B. Acta Metall Sin, 2010; 46: 787(杨玉娟, 严彪. 金属学报, 2010; 46: 787)[19] Zhu M F, Hong C P. Phys Rev, 2002; 66B: 155428[20] Wu M W, Xiong S M. Acta Phys Sin, 2011; 60: 058103(吴孟武, 熊守美. 物理学报, 2011; 60: 058103)[21] Akamatsu S, Moulinet S, Faivre G. Metall Mater Trans, 2001; 32A: 2039[22] Zhu Y C, Yang G C, Wang J C, Zhao D W, Fan J F. Chin J Nonferrous Met, 2005; 15: 1026(朱耀产, 杨根仓, 王锦程, 赵达文, 樊建锋. 中国有色金属学报, 2005; 15: 1026)[23] Karma A, Sarkissian A. Metall Mater Trans, 1996; 27A: 635[24] Ginibre M, Akamatsu S, Faivre G. Phys Rev, 1997; 56E: 780[25] Nestler B, Wheeler A A. Physica, 2000; 138D: 114[26] Mathis P. J Cryst Growth, 2007; 303: 49 |
|