| 合金钢中的碳化物 |
| 郭可信 |
| 中国科学院金属研究所 |
|
| RESEARCHES ON CARBIDES IN ALLOY STEELS |
| KEHSIN KUO Institute of Metal Research; Academia Sinica |
引用本文:
郭可信. 合金钢中的碳化物[J]. 金属学报, 1957, 2(3): 305-321.
.
RESEARCHES ON CARBIDES IN ALLOY STEELS[J]. Acta Metall Sin, 1957, 2(3): 305-321.
[1] Kuo, K. (郭可信) & Hagg, G., Nature, 170 (1952) , 245. [2] Kuo, K. (郭可信) & Hultgren, A., Rev. Met., 50 (1953) , 847. [3] Kuo, K. (郭可信), J. Iron and Steel Inst., 173 (1953) , 363. [4] Kuo, K. (郭可信), J. Iron and Steel Inst., 174 (1953) , 223. [5] Kuo, K. (郭可信), Acta Met., 1 (1953) , 301. [6] Kuo, K. (郭可信), Acta Met., 1 (1953) , 611. [7] Kuo, K. (郭可信) & Persson, L. E., J. Iron and Steel Inst., 178 (1954) , 39. [8] Kuo, K. (郭可信), Jernkontorets Annaler, 140 (1956) , 24. [9] Koo, K. (郭可信), Jernkontorets Annaler, 140 (1956) , 854. [10] Kuo, K. (郭可信), J. Iron and Steel Inst., 184 (1956) , 258. [11] Kuo, K. (郭可信), J. Iron and Steel Inst., 185 (1957) , 297. [12] 郭可信,未发表研究报告. [13] Goldechmidt, H. J., J. Iron and Steel Inst., 160 (1948) , 345. [14] Schwartzkopf, P. & Kieffer, R., Refractory Hard Metals, MacMillan Co., New York, 1953. [151 Hagg, G., Z. Physik. Chem., B 12 (1931) , 33. [16] Houdremont, E., Banek, H. & Schrader, H., Trans. Amer. Inst. Min. Met. Engrs., 116 (1935) , 260. [17] Курдюмов, 10 (1940) , 1093. [18] Jack, K. H., J. Iron and Steel Inst.. 169 (1951) , 26. [19] Mahla, E. M. & Nielsen, N. A., Trans. Amer. Soc. Metals, 43 (1951) , 290.
[20] Курдюмов 17 (1947) , 993. [21] 张沛霖,徐萃章,金属学报,1(1956) , 347. [22] Исайчев, 17 (1947) , 835. [23] Багаряцкий, 73 (1950) , 1161. [24] Арбузов, 19 (1949) , 1119. [25] Hyam, E. D. & Nutting J., J. Iron and Steel Inst., 184 (1956) , 148. [26] Owen, W. S., Trans. Amer. Soc. Metals, 46 (1954) , 813. [27] Bain, E. C. & Jeffries, Z., Iron Age, 112 (1923) , 805. [28] Baon, E. C., Alloy Elements in Steels, American Soc. for Metals, Cleveland, 1939. [29] Crafts, W. & Lamont, J. L., Trans. Amer. Inst. Mirs Met. Engrs., 180 (1949) , 471. [30] Wever, F & Koch, W., Stahl und Eisen, 74 (1954) , 989. [31] Bowers, J. E., J. Iron and Steel Inst., 183 (1956) , 268. [32] Бокштейн, 1954. [33] Bowman, F E. & Parke, R. M., Trans. Amer. Soc. Metals, 33 (1944) , 481. [34] Гуляев, 17 (1946) , 14. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|