| CuCl-AgCl熔体的蒸气压 |
| 陈自姚;彭瑞伍 |
| 中国科学院冶金研究所;中国科学院冶金研究所 |
|
| VAPOUR PRESSURE OF CuCl-AgCl MELTS |
| CHEN TZU-YAO;PENG HSUI-WU Institute of Metallurgy; Academia Sinica |
引用本文:
陈自姚;彭瑞伍. CuCl-AgCl熔体的蒸气压[J]. 金属学报, 1965, 8(3): 397-400.
,
.
VAPOUR PRESSURE OF CuCl-AgCl MELTS[J]. Acta Metall Sin, 1965, 8(3): 397-400.
[1] #12. [2] Kelley, K. K.: U.S. Bur. Mines Bull., 1934, No. 371. [3] Brewer, L., Lofgren, N. L.: J. Am. Chem. Soc., 1950, 72, 3038. [4] #12. [5] 彭瑞伍、陈自姚、邹元燨:金属学报,1965,8,401. [6] Alock, C. B., Hooper, G. W.: Physical Chemistry of Process Metallurgy, ed. G. R. St. Pierre, (Interscience, 1961) , pt. 1, p. 325. [7] Делимарский,Ю,К,等著,彭瑞伍译:熔盐电化学,(上海科技出版社,1964年),12页。 [8] Rosenstock, H. M., Sites, J. R., Walton, J. R.: J. Chem. Phys., 1955, 23, 2442. [9] Richard, A. W.: Physical Chemistry of Process Metallurgy, ed. G. R. St. Pierre, (Interscience, 196) ,pt. 1, p. 353. |
|