| 铁基合金中夹杂物的鉴定 |
| 李静媛;高国忠;吴仲堂 |
|
| IDENTIFICATION OF NON-METALLIC INCLUSIONS IN IRON-BASE ALLOYS |
| LI CHING-YEN; KAO KUO-CHUNG; WU CHUNG-T'ANG |
引用本文:
李静媛;高国忠;吴仲堂. 铁基合金中夹杂物的鉴定[J]. 金属学报, 1965, 8(4): 507-556.
,
,
.
IDENTIFICATION OF NON-METALLIC INCLUSIONS IN IRON-BASE ALLOYS[J]. Acta Metall Sin, 1965, 8(4): 507-556.
[1] Pickering, F. B.:J. Iron Steel Inst. (London), 1955, 181, 147. [2] 李靜媛:金属学报,1963,6,146. [3] Fischer, W. A.:Arch. Eisenhuttenw., 1958, 1,1. [4] Hilty, D. C., Forgenng, W. D., Folkman, R. L.:Trans. AIME, 1955, 203, 252.O |
|