| 国外涡轮喷气发动机涡轮盘材料的现状及发展 |
| 郭建亭;朱耀宵;师昌绪 |
|
| No Author |
引用本文:
郭建亭;朱耀宵;师昌绪. 国外涡轮喷气发动机涡轮盘材料的现状及发展[J]. 金属学报, 1974, 10(1): 74-98.
,
,
.
[J]. Acta Metall Sin, 1974, 10(1): 74-98.
[1] McRae,G.M.,Turbojet Disk Life Limits,PWA Paper. [2] Unksov,E.P.et al.,Thermal Stresses and Thermal Fatigue,ed.by D.J.Littler,Butterworths,London,1971,p.501. [3] Timo,D.P.,ibid.,p.453. [4] Hall,G.L.B.,Thermal and High-Strain Fatigue,The Metals and Metallurgy Trust,London,1967,p.28. [5] Manson,S.S.,Metal Fatigue Damage-Mechanisms,Detection,Avoidance and Repair,ed.by S.S.Manson,Amer.Soc.Test.Muter.,Spec.Teeh.Publ.№495,1971,p.254. [6] Landgraf,R.W.,Achievements of High Fatigue Resistance in Metals and Alloys,Amer.Soc.Test.Mater.,Spec.Tech.Publ.№467,1970,p.3. [7] Vinter,A.and Wilbers,L.G.,J.Metals,22(1970) ,№5,46. [8] Clauss,F.J.,Engineer's Guide to High-Temperature Materials,Addison-Wesley,London,1969,p.117. [9] 依田连平,特殊钢,11(1962) ,№2,42. [10] Flinn,P.A.,Strengthening Mechanisms in Solids,ASM,Ohio,1962,p.17. [11] Irvine,K.J.et al.,J.Iron Steel Inst.,199(1961) ,153. [12] Kelly,A.and Nicholson,R.B.,Progress in Materials Science,Vol.10,№3,ed.by B.Chalmers,Pergamon Press,Oxford,1963,p.151. [13] Brown,L.M.and Ham,R.K.,Strengthening Methods in Crystals,ed.by A.Kelly and R.B.Nicholson,Elsevier,Amsterdam,1971,p.9. [14]#12 [15] Seeger,A.,Dislocations and Mechanical Properties of Crystals,ed.by J.C.Fisher,Wiley,New York,1957,p.243. [16] Smallman,R.E.,Modern Physical Metallurgy,Butterworths,London,1962,p.171. [17] Beeston,B.E.P.and France,L.K.,J.Inst.Metals,96(1968) ,105. [18] Waters,W.J.and Freche,J.C.,Metals Eng.Qaurt.,10(1970) ,№2,55. [19] #12 [20]#12 [21] Cottrell,A.H.,Relation of Properties to Microstructure,ASM,Ohio,1954,p.131. [22] Kirman,I.and Warrington,D.H.,J.Inst.Metals,99(1971) ,197. [23] Guard,R.W.and Westbrook,J.H.,Trans.AIME,215(1959) ,807. [24] Copley,S.M.and Kear,B.H.,Trans.AIME,239(1967) ,977. [25] Betteridge,W.,The Nimonic Alloys,Edward Arnold,London,1959,p.128. [26] Hughes,H.,J.Iron Steel Inst.,203(1965) ,1019. [27] Wilson,F.G.and Pickering,F.B.,J.Iron Steel Inst.,204(1966) ,628. [28] #12 [29] Raynor,D.and Silcock,J.M.,Metal Sci.J.,4(1970) ,121. [30] Nordheim,R.and Grant,N,J.,J.Metals,6(1954) ,211. [31] Mihalisin,J.R.and Decker,R.F.,Trans.AIME,218(1960) ,507. [32] Fine,M.E.,The Relation Between the Structure and Mechanical Properties of Metals,Vol.1,HMSO,London,1963,p.300. [33] Gleiter,H.,Z.Metallk.,58(1967) ,306. [34] Decker,R.F.and Mihalisin,J.R.,ASM Trans.Quart.,62(1969) ,481. [35] Maniar,G.N.and James,H.M.,Fifty Years of Progress in Metallographic Techniques,Amer.Soc.Test.Mater.,Spec.Tech.Publ.№430,1966,ASTM,Philadelphia,Pa.p.262. [36] Hammond,C.M.and Ansell,G.S.,ASM Trans.Quart.,57(1964) ,727. [37] Gleiter,H.,Acta Met.,15(1967) ,1223. [38] Copley,S.M.and Kear,B.H.,Trans.AIME,239(1967) ,984. [39] Gleiter,H.and Hornbogen,E.,Phys.Status Solidi,12(1965) ,235. [40] Marcinkowski,M.J.,Electron Microscopy and Strength of Crystals,ed.by G.Thomas and J.Washburn,Interscience,New York,1963,p.333. [41] Guimier,A.and Strudel,J.L.,Proc.Second Intern.Conf.on the Strength of Metals and Alloys,Pacific Grove,Calif.,30 Aug.-4 Sept.,1970,Vol.3,ASM,Ohio,p.1145. [42] Cahn,R.W.,J.Metals,25(1973) ,№2,28. [43] Davies,R.G.and Johnston,T.L.,Ordered Alloys--Structural Application and Physical Metallurgy,Proc.3rd Bolton Landing Conf.,1970,ed.by B.H.Kear,Baton Rouge,La.,1970. [44] Karg,A.V.et al.,J.Inst.Metals,99(1971) ,301. [45] Kriege,O.H.and Baris,J.M.,ASM Trans.Quart.,62(1969) ,195. [46] Cozar,R.and Pineau,A.,Met.Trans.,4(1973) ,47. [47] Quist,W.E.et al.,Met.Trans.,2(1971) ,825. [48] VerSnyder,F.L.and Piearcey,B.J.,SAE J.,74(1966) ,№7,36. [49] Blasko,M.J.,Metal Progr.,103(1973) ,№3,42. [50] Perch,N.J.,J.Iron Steel Inst.,174(1953) ,25. [51] Hall,E.O.,Proc.Phys.Soc.(London),B64(1951) ,747. [52] 依田连平,金属材料,8(1968) ,№1,3. [53] Nordheim,R.and Grant,N.J.,Trans.AIME,200(1954) ,211. [54] Bird,J.E.et al.,Quantltative Relation Between properties and Microstructure,ed.by D.C.Brandon,Israel Univ.Press,Jerusalem,1969,p.255. [55] #12 [56] #12 [57] #12 [58] #12 [59]#12 [60] #12 [61] Symonds,C.H.,J.Aust.Inst.Metals,16(1971) ,№1,1. [62] Collins,H.E.,ASM Trans.Quart.,62(1969) ,82. [63] Betteridge,W.and Franklin,A.W.,J.Inst.Metals,85(1957) ,473. [64] Hagel,W.C.and Beattie,H.J.,Precipitation Processes in Steels,Iron Steel Inst.,London,1959,p.98. [65] Fell,E.A.,Metallurgia,63(1961) ,157. [66] #12 [67]#12 [68] Butteridge,W.,The Nimonic Alloys,Edward Arnold,London,1959,p.99. [69] Gresham,H.E.,Metals Mater.,3(1969) ,433. [70] #12 [71] Brown,J.T.and Bulina,J.,High Temperature Materials,ed.by R.F.Hehemann and G.M.Ault,Wiley,New York,1959,p.38. [72] Ewing,B.A.et al.,J.Mater.,5(1970) ,№3,651. [73] Anon.,Mater.Eng.,74(1971) ,№7,39. [74] Rideout,S.et al.,Trans.AIME,191(1951) ,872. [75] Das,D.K.et al.,Trans.AIME,194(1952) ,1071. [76] Boesch,W.J.and Slaney,J.S.,Metal Progr.,86(1964) ,№1,109. [77] Murphy,H.J.et al.,J.Metals,20(1968) ,№11,46. [78] Sims,C.T.,J.Metals,18(1966) ,1119. [79] Mihalisin,J.R.et al.,Trans.AIME,242(1968) ,2399. [80] Beattie,H.J.and VerSnyder,F.L.,Nurture,178(1956) ,208. [81] Rizzo,F.J.and Buzzanell,J.D.,J.Metals,21(1969) ,№10,24. [82] Boesch,W.J.and Canada,H.B.,J.Metals,21(1969) ,№10,34. [83] Stroup,J.F.and Heacox,R.A.,J.Metals,21(1969) ,№11,46. [84] Cremisio,R.S.et al.,J.Metals,21(1969) ,№11,55. [85] Schlatter,R.,Blast Furn.Steel Plant,57(1969) ,№1,19. [86] Aufderhaar,W.B.,Metal Progr.,93(1968) ,№6,135. [87] Dyrkacz,W.W.,Metal Progr.,79(1961) ,№5,65. [88] Schlatter,R.,J.Metals,24(1972) ,№5,17. [89] Sperner,von F.,Vak.Tech.,11(1962) ,Nr.7,191. [90] Barraclough,K.C.,J.Iron Steel Inst.,207(1969) ,826. [91] Wood,D.R.and Cook,R.M.,Metallurgia,67(1963) ,109. [92] Johnson,A.R.and Hamaker,J.C.,Mater.Des.Eng.,61(1965) ,№1,86. [93] Cremisio,R.S.,Elec.Furnace Conf.Proc.,29(1971) ,19. [94] Schlatter,R.,Elec.Furnace Conf.Proc.,29(1971) ,2. [95] Bhat,G.K.,A Collection of Technical Papers Presented at the 2nd International Symposium on Electroslag Remelting Technology,Mellon Univ.,Pittsburgh,Pa.,23-25 Sept.1969,part 1. [96] Kelley,T.N.and Klein,H.J.,Metal Progr.,102(1972) ,№3,97. [97] Elliott,C.F.et al.,Metals Eng.Quart.,10(1970) ,№2,46. [98] Oblak,J.M.et al.,Met.Trans.,2(1971) ,1499. [99] Muzyka,D.R.,Metals Eny.Quart.,11(1971) ,№4,12. [100] DeRidder,A.J.and Noel,R.J.,Deformation Processing of Superalloy Gas Turbine Components,SAE Paper №690101,Jan.13-17,1969. [101] Vaccari,J.A.,Mater.Eng.,72(1970) ,№2,28. [102] Rosenhain,W.et at.,J.Inst.Metals,23(1920) ,№1,261. [103] Underwood,E.E.,J.Metals,14(1962) ,914. [104] Johnson,R.H.,Met.Rev.,15(1970) ,№146,115. [105] Avery,D.H.and Backofen,W.A.,ASM Trans.Quart.,58(1965) ,551. [106] Wong,W.A.et al.,J.Inst.Metals,95(1967) ,129. [107] Mukherjee,A.K.,Mater.Sci.Eng.,8(1971) ,№2,83. [108] Stevens,R.N.,Met.Rev.,11(1966) ,№108,129. [109] Morre,J.B.et al.,U.S.Patent №3,519,503,July 7,1970. [110] Staff Report,Metal Progr.,103(1973) ,№3,49. [111] Headley,T.J.et al.,Ultrafine-Grain Metals,ed.by J.J.Burke and V.Weiss,Syracuse Univ.Press,New York,1970,p.325. [112] Kear,B.H.et al.,J.Metals,24(1972) ,№6,25. [113] Giamei,A.F.and Kear,B.H.,Met.Trans.,1(1970) ,2185. [114] Gould,G.C.,Trans.AIME,233(1965) ,1345. [115] Friedman,G.and Kosinski,E.,Metals Eng.Quart.,11(1971) ,№1,48. [116] Anon.,Metal Prog.,101(1972) ,№1,76. [117] Jahnke,L.P.,J.Metals,25(1973) ,№4,15. [118] 田中良平,金属材料,13(1973) ,№4,59. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|