| 30吨氧气顶吹转炉吹炼含磷生铁的工艺研究 |
| No Author |
| 北京钢铁学院73届炼钢工人进修班;上海第一钢铁厂第三转炉车间 |
|
| No Author |
引用本文:
No Author. 30吨氧气顶吹转炉吹炼含磷生铁的工艺研究[J]. 金属学报, 1976, 12(1): 23-36.
.
[J]. Acta Metall Sin, 1976, 12(1): 23-36.
[1] Wells, A. A., Brit. Weld. J., 10(1963) , 568, 12(1965) ,2 and 15(1968) , 221. [2] Burdekin, F. M. and Dawes, M. G., Conference on Practical Application of Fracture Mechanics to Pressure-Vessel Technology, 1971, Inst. Mech. Eng., London, p. 28. [3] Burdekin, F. M. and Stone, D. E. W., J.Strain Anal., 1(1966) , 145. [4] Iino, Y., Eng. Fract. Mech., 7(1975) , 205. [5] Andrews, E. H., Fracture, ed. by P. L. Pratt,Chapman and Hall, London,1969,p.881. [6] Weiss, V., Fatigue--An Interdisciplinary Approach, Syracuse Univ. Pr., New York,1964, p.179. [7] Boettner, R. C. et al.,Trans. AIME, 233(1965) , 376. [8] Tomkins, B., Phil. Mag.,18(1968) ,1041. [9] Solomon, H. D., J. Mater., 7(1972) , 299. [10] Morrow, J., Internal Friction, Damping and Cyclic Plasticity, Amer. Soc. Test. Mater., Spec.Tech. Publ. № 378, ASTM, Phil. Pa.,1964, p. 72. [11] Manson, S. S. and Hirshberg, M.H.,Fatigue--An Interdisciplinary Approach, Syracuse Univ. Pr.,New York, 1961, p.133, Discussion by L. F.Coffin, p.173, Authors′Reply, p.176. [12] Calabrese, C. and Laird, C., Met. Trans.,5(1974) , 1785. [13] Van Swam, L. F. et al., Met. Trans., 6A(1975) ,45. [14] Freudenthal, A. F., Eng. Froct. Mech., 6(1974) ,78. [15] Tomkins, B. et al., Fracture, ed. by P.L. Pratt,Chapman and Hall,London,1969,p.712. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|