| 一种铁镍基合金预裂纹试样的高温持久开裂界限 |
| 孔庆平 |
|
| THE THRESHOLD VALUE K_(Ihcc) OF PRECRACKED SPECIMENS OF AN IRON-NICKEL-BASE ALLOY UNDER CONSTANT LOAD AT HIGH TEMPERATURES |
| Kung Ching-ping |
引用本文:
孔庆平. 一种铁镍基合金预裂纹试样的高温持久开裂界限[J]. 金属学报, 1977, 13(3): 231-234.
.
THE THRESHOLD VALUE K_(Ihcc) OF PRECRACKED SPECIMENS OF AN IRON-NICKEL-BASE ALLOY UNDER CONSTANT LOAD AT HIGH TEMPERATURES[J]. Acta Metall Sin, 1977, 13(3): 231-234.
[1] Brown, W. F. and Scrawloy, J. E., Amer. Soc. Test. Mater., Spec. Tech. Publ. No. 410 (1969) , 12. [2] Gerberich, W. W. and Katz, Y., Eng. Fract. Mech., 1 (1969) , 569. [3] Orange, T. W., Amer. Soc. Test. Mater., Spec. Tech. Publ. No. 513 (1972) , 75.} |
|